Petrova A.P., Mukhametov R.R., Shishimirov M.V., Pavlyuk B.Ph., Starostina I.V. Test methods and researches thermosetting binding for polymeric composite materials (review) // Proceedings of VIAM. 2018. No. 12 (72). Ст. 07. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2018-0-12-62-70.

Test methods and researches thermosetting binding for polymeric composite materials (review)

Petrova A.P., Mukhametov R.R., Shishimirov M.V., Pavlyuk B.Ph., Starostina I.V.
Abstract

By production of PKM use binding and the fibrous filler, thus the binding carries out number of functions: will define way of receiving composite material and its such properties, as durability, chemical resistance, warm and moisture resistance, climatic firmness, technological conditions of processing, etc.

In this regard it is important to know properties binding and to provide stability in the course of receiving. Therefore it is necessary to carry out control of the main properties  binding both at receiving stage, and in the course of processing in PKM to provide implementation of the guaranteed requirements for their properties.

In article properties binding which are control for carrying out target and incoming inspection thermosetting polymeric binding, and also at stage of tests binding with reference to technology of their processing and receiving PKM on their basis are considered.

At the first stage – receiving binding – important parameters are appearance, the maintenance of flying products, viability, viscosity, gelation time, density. As a rule, these parameters are used at carrying out target and incoming inspection.

At stage of receiving PKM important parameters binding are rheological properties and the curing mode which observance provides obtaining necessary physicomechanical characteristics otverzhdenny binding, thermal effects of transients.

As a part of  PKM important parameters otverzhdenny binding are glass transition temperature, tensile strength, compression, bend, relative lengthening, impact strength, adhesion binding to fibrous filler.

For definition of the resource characteristics necessary for establishment

Keywords
thermosetting binder, test methods, viscosity, processing in PCM, cure, rheology, manufacturability, input control, DSC, TMA, IRS.
Reference list
  1. Grelmann V., Zaydler S. Ispytaniya plastmass [Tests of plastic]. SPb.: Professiya, 2010. 720 s.
  2. Barbotko S.L. Razvitie metodov ocenki pozharobezopasnosti materialov aviacionnogo naznacheniya [Development of the fire safety test methods for aviation materials] // Avi-acionnye materialy i tehnologii. 2017. №S. S. 516–526. DOI: 10.18577/2071-9140-2017-0-S-516-526.
  3. Nikolayev E.V., Lutsenko A.N., Barbotko S.L., Pavlov M.R., Abramov D.V. Kompleksnyy metodicheskiy podkhod k opredeleniyu sokhranyaemosti svoystv polimernogo svyazuyushchego i polimernykh kompozitsionnykh materialov na ego osnove pri vozdeystvii klimaticheskikh i ekspluatatsionnykh faktorov [Comprehensive methodical approach to determining the persistence properties of polymer binder and polymer composite materials based on it under the influence of climatic and operational factors] // Sb. tez. dokl. konf. «Fundamentalnye issledovaniya i poslednie dostizheniya v oblasti zashchity ot korrozii, stareniya i biopovrezhdeniy materialov i slozhnykh tekhnicheskikh sistem v razlichnykh klimaticheskikh usloviyakh». M.: VIAM, 2016. St. 13.
  4. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innova-tive developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  5. Kablov E.N. Materialy novogo pokoleniya [New generation materials] // Zashchita i be-zopasnost. 2014. №4. S. 28–29.
  6. Kablov E.N. Iz chego sdelat budushchee? Materialy novogo pokoleniya, tekhnologii ikh soz-daniya i pererabotki – osnova innovatsiy [What to make the future from? Materials of the new generation, technologies of their creation and processing - the basis of innovation] // Krylya Rodiny. 2016. №5. S. 8–18.
  7. Babin A.N. Svyazujushhie dlya polimernyh kompozicionnyh materialov novogo pokoleniya [Binding for polymeric composite materials of new generation] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №4. St. 11. Available at: http://www.viam-works.ru (accessed: November 14, 2018).
  8. Babin A.N., Petrova A.P. Metody ispytaniy i issledovaniy osnovnykh svoystv polimernykh svyazuyushchikh dlya konstruktsionnykh PKM [Test methods and studies of the basic properties of polymeric binders for structural PCM] // Vse materialy. Entsiklopedicheskiy spravochnik. 2016. №3. S. 52–59.
  9. Petrova A.P., Lukina N.F., Melnikov D.A., Besednov K.L., Pavlyuk B.F. Issledovanie svojstv ot-verzhdennyh kleevyh svyazuyushchikh [Research of properties of cured adhesive binders] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2017. №10 (58). St. 06. Available at: http//www.viam-works.ru (accessed: November 14, 2018). DOI: 10.18577/2307-6046-2017-0-10-6-6.
  10. Kirienko T.F., Lukina N.F., Kutsevich K.E., Petrova A.P. A Study of the reological proper-ties of Adhesive binders // Polymer Science. Ser.: D. 2016. T. 9. No. 3. P. 295–297.
  11. Grashchenkov D.V., Chursova L.V. Strategiya razvitiya kompozicionnyh i funkcionalnyh materialov [Strategy of development of composite and functional materials] // Aviacionnye materialy i tehnologii. 2012. №S. S. 231–242.
  12. Petrovа A.P., Dementyevа L.A., Lukina N.F., Chursova L.V. Kleevye svjazujushhie dlja po-limernyh kompozicionnyh materialov na ugle- i steklonapolniteljah [Adhesive binders for polymer composite materials based on carbon- and glass fillers] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №9. St. 11. Available at: http://www.viam-works.ru (accessed: November 20, 2018). DOI: 10.18577/2307-6046-2015-0-9-11-11.
  13. Antyufeeva N.V., Aleksashin V.M., Zhelezina G.F., Stolyankov Yu.V. Metodicheskie pod-khody termoanatomicheskikh issledovaniy dlya otsenki svoystv prepregov i ugleplastikov [Methodical approaches of thermoanatomical studies for the evaluation of the properties of prepregs and carbon plastics // Vse materialy. Entsiklopedicheskiy spravochnik. Kommentarii k standartam, TU, sertifikatam. 2012. №4. S. 18–22.
  14. Antyufeeva N.V., Komarova O.A., Pavlovskij K.A., Aleksashin V.M. Opyt primeneniya kalorimetricheskogo kontrolya reakcionnoj sposobnosti preprega KMU-11tr [Practice of the calorimetric control reactionary ability prepreg KMU-11tr] // Trudy VIAM. 2014. №2. St. 06. Available at: http://viam-works.ru (accessed: November 15, 2018). DOI: 10.18577/2307-6046-2014-0-2-6-6.
  15. Deyev I.S., Kobets L.P. Issledovanie mikrostruktury i osobennostey razrusheniya epoksidnykh matrits [Study of the microstructure and features of the destruction of epoxy matrices] // Klei. Germetiki. Tekhnologii. 2013. №5. S. 19–27.
  16. Kobets L.P., Deyev I.S. Strukturoobrazovanie v termoreaktivnykh svyazuyushchikh i matrit-sakh kompozitsionnykh materialov na ikh osnove [Structure formation in thermosetting binders and matrices of composite materials based on them] // Rossiyskiy khimicheskiy zhurnal. 2010. LIV. №1. S. 67–78.