Istyagin S.E., Postnov V.I. About increase accuracy of correlation dependence parameters nondestructive control at diagnostics of properties coal plastics // Proceedings of VIAM. 2018. No. 11 (71). Ст. 12. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2018-0-11-101-110.

About increase accuracy of correlation dependence parameters nondestructive control at diagnostics of properties coal plastics

Istyagin S.E., Postnov V.I.
Abstract

Coal plastics reinforced with woven fillers are widely distributed in medium- and strongly loaded details of designs of aircraft. The polymeric composition constructional materials made from coal fillers and used in aircraft construction are appreciated their specific strength characteristics. Measurement and which analysis is possible with applying of the nondestructive control (NC). Contains of additional researches showing importance of application of methods of increase in accuracy of the correlation equations based by NC.

Keywords
polymer composite material, non-destructive testing, informative parameter of control, carbon fiber, dynamic modulus of elasticity, correlation.
Reference list
  1. Kablov E.N. Materialy dlya aviakosmicheskoy tekhniki [Materials for aerospace] // Vse materialy. Entsiklopedicheskiy spravochnik, 2007. №5. S. 7–27.
  2. Murmanskiy B.E. Razrabotka, aprobatsiya i realizatsiya metodov povysheniya nadezhnosti i sovershenstvovaniya sistemy remontov paroturbinnykh ustanovok v usloviyakh ekspluatatsii: dis. dokt. tekhn. nauk [Development, testing and implementation of methods to improve the reliability and improve the repair system of steam turbine units in operation: thesis, Doc. Sc. (Tech.)]. Ekaterinburg, 2015. 457 s.
  3. Mashinostroyeniye: entsiklopediya v 40 t. / pod obshch. red. K.V. Frolova [Engineering: encyclopedia of 40 vol. / gen. ed. By K.V. Frolov]. M.: Mashinostroyeniye, 1998. T. IV-3: Nadezhnost' mashin / pod red. V.V. Klyuyeva. 592 s.
  4. GOST 27.002–2015. Nadezhnost v tekhnike (SSNT). Terminy i opredeleniya [State Standard 27.002–2015. Reliability in technology (SAT). Terms and Definitions]. M: Standartinform, 2016. 28 s.
  5. Kompozitsionnyye materialy / pod red. L. Brautmana, R. Kroka [Composite materials / ed. L. Brautman, R. Krok]. M.: Mashinostroyeniye, 1978. T. 7: Analiz i proyektirovaniye konstruktsiy. CH. 1 / pod red. K. Chamisa. 300 s.
  6. Kablov E.N., Startsev V.O. Sistemnyj analiz vliyaniya klimata na mekhanicheskie svojstva polimernykh kompozitsionnykh materialov po dannym otechestvennykh i zarubezhnykh istochnikov (obzor) [Systematical analysis of the climatics influence on mechanical properties of the polymer composite materials based on domestic and foreign sources (review)] // Aviacionnye materialy i tehnologii. 2018. №2 (51). S. 47–58. DOI: 10.18577/2071-9140-2018-0-2-47-58.
  7. Iosilevich G.B., Lebedev P.A., Strelyayev V.S. Prikladnaya mekhanika: dlya studentov vtuzov [Applied mechanics: for students of technical colleges]. M.: Mashinostroyeniye, 2012. 576 s.
  8. Feodosyev V.I. Soprotivleniye materialov: ucheb. dlya vuzov. 10-ye izd., pererab. i dop. [Resistance materials: textbook for universities. 10th ed., rev. and add.]. M.: Izd-vo MGTU im. N.E. Baumana, 1999. 592 s.
  9. Bochkareva S.A. Otsenka nadezhnosti konstruktsiy iz polimernykh kompozitsionnykh materialov s uchetom razbrosa upravlyayushchikh parametrov: avtoref. dis. … kand. fiz.-mat. nauk [ssessment of the reliability of structures made of polymer composite materials, taking into account the spread of control parameters: authors thesis, Cand. Sc. (Tech.)]. Tomsk, 2006. 21 s.
  10. Murashov V.V., Kosarina E.I., Generalov A.S. Kontrol kachestva aviacionnyh detalej iz polimernyh kompozicionnyh materialov i mnogoslojnyh kleevyh konstrukcij [Quality control of aviation parts made from polymer composite materials and multilayers adhered constructions] // Aviacionnye materialy i tehnologii. 2013. №3. S. 65–70.
  11. Kablov E.N. Materialy i tekhnologii VIAM dlya «Aviadvigatelya» [Materials and technologies of VIAM for Aviadvigatel] // Permskiye aviatsionnyye dvigateli. 2014. №31. S. 43–47.
  12. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  13. Generalov A.S., Murashov V.V., Kosarina E.I., Boychuk A.S. Postroyeniye i analiz korrelyatsionnykh svyazey dlya otsenki prochnostnykh svoystv ugleplastikov reverberatsionno-skvoznym metodom [Plotting of correlation curves and analysis of CFRP strength properties estimated by acoustic-ultrasonic technique] // Aviacionyye materialy i tehnologii. 2014. №1. S. 58–63. DOI: 10.18577/2071-9140-2014-0-1-58-63.
  14. Istyagin S.E., Postnov V.I. K voprosu o korrelyatsionnoy zavisimosti informativnykh parametrov kontrolya pri diagnostike svoystv PKM [On the question of the correlation of informative control parameters in the diagnosis of PCM properties] // Izvestiya Samarskogo nauchnogo tsentra RAN. 2017. T. 19. №4 (2). S. 229–237.
  15. Troitskiy V.A., Karmanov M.N., Troitskaya N.V. Nerazrushayushchiy kontrol kachestva kompozitsionnykh materialov [Non-destructive quality control of composite materials] // Tekhnicheskaya diagnostika i nerazrushayushchiy kontrol. 2016. №1. S. 295–296.
  16. Bolotin V.V., Novichkov Yu.N. Mekhanika mnogosloynykh konstruktsiy [Mechanics of multilayer structures]. M.: Mashinostroyeniye, 1980. 375 s.
  17. Pobedrya B.E. Mekhanika kompozitsionnykh materialov [Mechanics of composite materials]. M.: Izd-vo MGU, 1984. 336 s.
  18. GOST 56682–2015. Kompozity polimernyye i metallicheskiye. Metody opredeleniya obyema matritsy, armiruyushchego napolnitelya i pustot [State Standard 56682–2015. Polymer and metal composites. Methods for determining the volume of the matrix, reinforcing filler and voids]. M.: Standartinform, 2016. 24 s.
  19. GOST 11262–2017. Plastmassy. Metod ispytaniya na rastyazheniye [State Standard 11262–2017. Plastics Tensile test method]. M.: Standartinform, 2018. 24 s.