Bryk Ya. А., Smirnov D.N. Research of frost resistance of aeronautical sealants // Proceedings of VIAM. 2018. No. 1 (61). Ст. 09. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2018-0-1-9-9.

Research of frost resistance of aeronautical sealants

Bryk Ya. А., Smirnov D.N.
Abstract

The principles of creating frost-resistant sealing materials are considered. The influence of components (fillers, plasticizers and crosslinking agents) on the frost resistance of sealants was investigated. Two methods for evaluating the frost resistance of sealants have been studied: the determination of the strength and elongation of the material at a negative temperature, the determination of the dynamic shear modulus G and the tangent of the mechanical loss angle tgδ in the negative temperature region. The article presents data on glass transition temperatures of sealing materials, as well as temperature dependences of the dynamic mechanical characteristics of sealants, depending on their polymer base. It is shown that the frost resistance of sealants is an ambiguous concept, since the operability of the material in a structure depends not only on its properties, but also on the characteristics of hermetic joints and the conditions of their operation.

Keywords
frost resistance, polar and nonpolar rubbers, sealing materials, glass transition temperature, shear modulus, elongation.
Reference list
  1. Kablov E.N. Iz chego sdelat budushhee? Materialy novogo pokoleniya, tehnologii ih sozdaniya i pererabotki – osnova innovacij [Of what to make the future? Materials of new generation, technology of their creation and processing – basis of innovations] // Krylya Rodiny. 2016. №5. S. 8–18.
  2. Kablov E.N. Materialy novogo pokoleniya [Materials of new generation] // Zashhita i bezopasnost. 2014. №4. S. 28–29.
  3. Kablov E.N. Himiya v aviacionnom materialovedenii Chemistry in aviation materials science] // Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  4. Kablov E.N. Shestoj tehnologicheskij uklad [Sixth technological way] // Nauka i zhizn. 2010. №4. S. 2–7.
  5. Kablov E.N. Materialy dlya aviakosmicheskoj tehniki [Materials for aerospace equipment] // Vse materialy. Enciklopedicheskij spravochnik. 2007. №5. S. 7–27.
  6. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] // Vse materialy. Enciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  7. Grashhenkov D.V., Chursova L.V. Strategiya razvitiya kompozicionnyh i funkcionalnyh materialov [Strategy of development of composite and functional materials] // Aviacionnye materialy i tehnologii. 2012. №S. S. 231–242.
  8. Zajceva E.I., Donskoj A.A. Germetiki na osnove polisul'fidnyh elastomerov [Hermetics on the basis of polysulphide elastomer] // Klei. Germetiki. Tehnologii. 2008. №6–7. S. 15–25.
  9. Minkin V.S., Hakimullin Yu.N., Deberdeev T.R., Berlin Al. Al. Vliyanie ionov Fe (III) v sostave MnO2 na kinetiku vulkanizacii zhidkih tiokolov [Influence of ions of Fe (III) as a part of MnO2 on kinetics of curing of the liquid it is thiokol] // Klei. Germetiki. Tehnologii. 2009. №4. S. 28–30.
  10. Mudrov O.A., Savchenko I.M., Shitov V.S. Spravochnik po elastomernym pokrytiyam i germetikam v sudostroenii [The directory on elastomeric coverings and hermetics in ship-building]. L.: Sudostroenie, 1982. S. 112.
  11. Zajceva E.I., Donskoj A.A. Novye polisulfidnye germetiki dlya aviacionnoj promyshlennosti [New polysulphide hermetics for the aviation industry] // Klei. Germetiki. Tehnologii. 2009. №3. S. 18–23.
  12. Zaitseva Е.I., Donskoi А.А. Sealants Based on Polysulfide Elastomers // Polymer Science. Ser. С. 2008. Vol. 1. P. 15–25.
  13. Zajceva E.I., Chursova L.V. Issledovanie mikrobiologicheskoj stojkosti polisulfidnogo germetika s novymi antisepticheskimi dobavkami [Research of microbiological firmness of polysulphide hermetic with new antiseptic additives] // Klei. Germetiki. Tehnologii. 2012. №1. S. 16–20.
  14. Eliseev O.A., Bryk Ya.A., Smirnov D.N. Modifikaciya polisulfidnyh germetikov ingibitorami korrozii [Polysulfide sealants modification by corrosion inhibitors] // Aviacionnye materialy i tehnologii. 2016. №S2 (44). S. 15–21. DOI: 10.18577/2071-9140-2016-0-S2-15-21.
  15. Averenko-Antanovich L.A., Kirpichnikov P.A., Smyslova R.A. Polisulfidnye oligomery i germetiki na ih osnove [Polysulphide oligomers and hermetics on their basis]. L.: Himiya, 1983. 128 s.
  16. Zajceva E.I., Chursova L.V., Smirnov D.N. Perspektivy snizheniya plotnosti polisulfidnyh germetikov [Perspectives of decrease in density of polysulphide hermetics] // Klei. Germetiki. Tehnologii. 2012. №5. S. 10–14.
  17. Bryk Ya.A., Eliseev O.A., Smirnov D.N. Zashhita ot korrozii magnievyh splavov polisulfidnymi germetikami [Corrosion protection of magnesium alloys polysulphide sealants] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2017. №10. St. 10. Available at: http://www.viam-works.ru (accessed: Desember 08, 2017). DOI: 10.18577/2307-6046-2017-0-10-10-10.
  18. Petrova A.P., Donskoj A.A. Kleyashhie materialy, germetiki: spravochnik [Gluing materials, hermetics: directory]. SPb.: Professional, 2008. S. 503–567.
  19. Eliseev O.A., Krasnov L.L., Zajceva E.I., Savenkova A.V. Razrabotka i modificirovanie elastomernyh materialov dlya primeneniya vo vseklimaticheskih usloviyah [Development and modifying of elastomeric materials for application in all weather conditions] // Aviacionnye materialy i tehnologii. 2012. №S. S. 309–314