Nochovnaya N.A., Shiryaev A.A., Dzunovich D.А., Panin P.V. Study of chemical composition of large-dimensioned experimental-industrial ingot from a new high-alloyed metastable β-titanium alloy VT47 // Proceedings of VIAM. 2018. No. 1 (61). Ст. 06. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2018-0-1-6-6.

Study of chemical composition of large-dimensioned experimental-industrial ingot from a new high-alloyed metastable β-titanium alloy VT47

Nochovnaya N.A., Shiryaev A.A., Dzunovich D.А., Panin P.V.
Abstract

Chemical composition studies have been carried out for a large-dimensioned experimental-industrial 1,5 tons ingot from high-alloyed high-strength metastable β-titanium alloy VT47, the ingot having been obtained by threefold vacuum-arc remelting in PSC «VSMPO-AVISMA Corporation». A comparative analysis has been completed for the results of 30 kg laboratory ingots investigation (obtained by VIAM experimental production) and those for the large-dimensioned ingot in order to evaluate the scale factor influence on quality characteristics of VT47 ingots. The possible ways of further metallurgical quality increase have been proposed for large-dimensioned industrial ingots from VT47 alloy.

Keywords
VT47 alloy, large-dimensioned ingots, industrial production, chemical composition, vacuum-arc melting.
Reference list
  1. Boyer R.R., Briggs R.D. The Use of β Titanium Alloys in the Aerospace Industry // Journal of Materials Engineering and Performance. 2005. Vol. 14 (6). P. 681–685.
  2. Moiseev V.N. Beta-titanovye splavy i perspektivy ih razvitiya [Beta titanium alloys and perspectives of their development] // MiTOM. 1998. №12. S. 11–14.
  3. Shiryaev A.A., Nochovnaya N.A. Issledovanie struktury i himicheskogo sostava slitkov opytnogo vysokolegirovannogo titanovogo splava [Study of structure and chemical com-position of pilot high-alloyed titanium alloy ingots] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №9. St. 06. Available at: http://www.viam-works.ru (accessed: November 30, 2017). DOI: 10.18577/2307-6046-2015-0-9-6-6
  4. Kablov D.E., Panin P.V., Shiryaev A.A., Nochovnaya N.A. Opyt ispolzovaniya vakuumno-dugovoj pechi ALD VAR L200 dlya vyplavki slitkov zharoprochnyh splavov na osnove aljuminidov titana [The use of ADL VAR L200 vacuum-arc furnace for ingots fabrication of high-temperature titanium aluminides base alloys] //Aviacionnye materialy i tehnologii. 2014. №2. S. 27–33. DOI: 10.18577/2071-9140-2014-0-2-27-33.
  5. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  6. Kablov E.N. Materialy novogo pokoleniya [Materials of new generation] // Zashhita i bezopasnost. 2014. №4. S. 28–29.
  7. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemelnye elementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare-earth elements are materials for modern and future high technologies] // Aviacionnye materialy i tehnologii. 2013. №S2. S. 3–10.
  8. Vysokoprochnyj splav na osnove titana i izdelie, vypolnennoe iz vysokoprochnogo splava na osnove titana: pat. 2569285 Ros. Federaciya. №2014153690/02 [High-strength alloy on the basis of titanium and the product executed from high-strength alloy on the basis of titanium: pat. 2569285 Rus. Federation. No. 2014153690/02]; zayavl. 29.12.14; opubl. 20.11.15, Byul. №32.
  9. Zhijun Yang, Hongchao Kou, Fengshou Zhang, Xiangyi Xue, Jinshan Li, Lian Zhou. The Effect of VAR Process Parameters on Beta Flecks Formation in Ti–10V–2Fe–3Al // Pro-ceedings of the 12th World Conference on «Titanium Ti-2011 Science and Technology». Beijing, 2012. Vol. 1. P. 601–604.
  10. Andreev A.L., Anoshkin N.F. i dr. Titanovye splavy. Plavka i lite titanovyh splavov [Titanium alloys. Melting and molding of titanium alloys]. M.: Metallurgiya, 1978. 384 s.
  11. Savickij E.M., Livanov V.A., Nuss P.A. i dr. Splavy titana s redkozemelnymi metallami [Titanium alloys with rare earth metals] // Titan v promyshlennosti. M.: Oborongiz, 1961. S. 85–89.
  12. Khorev A.I. Alloying titanium alloys with rare-earth metals // Russian Engineering Research. 2011. Vol. 31. No. 11. P. 1087–1094.
  13. Yu-Yong Chen, Yu-Feng Si, Fan-Tao Kong et al. Effects of yttrium on microstructures and properties of Ti–17Al–27Nb alloy // Transactions of Nonferrous Metals Society of China. 2006. Vol. 16. No. 2. P. 316–320.
  14. Skupov A.A., Panteleev M.D., Ioda E.N., Movenko D.A. Effektivnost primeneniya redkozemelnyh metallov dlya legirovaniya prisadochnyh materialov [The efficiency of rare earth metals for filler materials alloying] // Aviacionnye materialy i tehnologii. 2017. №3 (48). S. 14–19. DOI: 10.18577/2071-9140-2017-0-3-14-19.
  15. Horev A.I., Muhina L.G., Zhegina I.P. Vliyanie redkozemelnyh elementov na svojstva titanovyh splavov [Influence of rare earth elements on properties of titanium alloys] // Legirovanie i termicheskaya obrabotka titanovyh splavov. M.: VIAM, 1977. S. 106–113.
  16. Kyosuke Ueda, Shinichiro Nakaoka, Takayuki Narushima. β-Grain Refinement of α+β-Type Ti–4,5Al–6Nb–2Fe–2Mo Alloy by Using Rare-Earth-Oxide Precipitates // Materials Transactions. 2013. Vol. 54 (2). P. 161–168.