Alekseev A.V., Rastegayeva G.Yu., Pahomkina T.N. Experience of the determination of carbon, sulfur, oxygen and nitrogen in alloys based on niobium on the gas-analyzers of the LECO firm // Proceedings of VIAM. 2018. No. 1 (61). Ст. 03. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2018-0-1-3-3.

Experience of the determination of carbon, sulfur, oxygen and nitrogen in alloys based on niobium on the gas-analyzers of the LECO firm

Alekseev A.V., Rastegayeva G.Yu., Pahomkina T.N.
Abstract

A study was made of the possibility of determining the mass fraction of carbon and sulfur in an alloy based on Nb by burning in an induction furnace a gas analyzer CS-444 from Leco, followed by detection in an infrared cell of a spectrometer. A catalyst is selected, with a specially selected composition, which allows full recovery of carbon and sulfur from the analyzed material. Determination of the content of the oxygen and nitrogen mass fraction in the Nb-based alloy was carried out by reductive melting in a stream of an inert carrier gas, followed by detection of oxygen in an infrared cell and nitrogen in a conductometric cell of a TC-600 from Leco gas analyzer. The catalysts required for the complete extraction of these elements from an Nb-based alloy were selected

Keywords
alloys based on Nb, determination of carbon, determination of sulfur, determination of oxygen, determination of nitrogen, method of infrared absorption spectroscopy, melting method in a current of an inert carrier gas.
Reference list
  1. Kablov E.N. Materialy novogo pokoleniya [Materials of new generation] // Zashhita i bezopasnost. 2014. №4. S. 28–29.
  2. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokoleniya [Nickel foundry heat resisting alloys of new generation] // Aviacionnye materialy i tehnologii. 2012. №S. C. 36–52.
  3. Kablov E.N., Bondarenko Yu.A., Echin A.B., Surova V.A. Razvitie processa napravlennoj kristallizacii lopatok GTD iz zharoprochnyh splavov s monokristallicheskoj i kompozicionnoj strukturoj [Development of process of the directed crystallization of blades of GTE from hot strength alloys with single-crystal and composition structure] // Aviacionnye materialy i tehnologii. 2012. №1. S. 3–8.
  4. Kablov E.N., Sidorov V.V., Kablov D.E., Rigin V.E., Goryunov A.V. Sovremennye tehnologii polucheniya prutkovyh zagotovok iz litejnyh zharoprochnyh splavov novogo pokoleniya [Modern technologies of receiving the bar stock preparations from foundry heat resisting alloys of new generation] // Aviacionnye materialy i tehnologii. 2012. №S. S. 97–105.
  5. Kablov E.N., Svetlov I.L., Efimochkin I.Yu. Vysokotemperaturnye Nb–Si-kompozity [High-temperature Nb-Si-composites] // Vestnik MGTU im. N.E. Baumana. Ser.: Mashinostroenie. 2011. №SP2. S. 164–173.
  6. Min P.G., Sidorov V.V. Opyt pererabotki litejnyh othodov splava ZhS32-VI na nauchno-proizvodstvennom komplekse VIAM po izgotovleniyu lityh prutkovyh (shihtovyh) zagotovok [The experience of GS32-VI alloy scrap recycling at the VIAM scientific and production complex for cast bars production] // Aviacionnye materialy i tehnologii. 2013. №4. S. 20–25.
  7. Sidorov V.V., Timofeeva O.B., Kalitsev V.A., Goryunov A.V. Vliyanie mikrolegirovanija RZM na svojstva i strukturno-fazovye prevrashheniya v intermetallidnom splave VKNA-25-VI [Influence of microalloying of RZM on properties and structural phase changes in intermetallidny alloy VKNA-25-VI] // Aviacionnye materialy i tehnologii. 2012. №4. S. 8–13.
  8. Svetlov I.L., Abuzin Yu.A., Babich B.N. i dr. Vysokotemperaturnye Nb–Si kompozity, uprochnennye silicidami niobiya [High-temperature Nb–Si the composites strengthened by silicides of niobium] // Zhurnal funkcionalnyh materialov. 2007. T. 1. №2. S. 48–52.
  9. Bewlay B.P., Jackon M.R., Zhao H.C. et al. Ultrahigh-Temperature Nb-Silicide-Based Composites // Mrs. Bulletin. Spt., 2003. P. 646–653.
  10. High Temperature Niobium alloy: pat. 7632455 US; publ. 15.12.09.
  11. Lomberg B.S., Ovsepyan S.V., Bakradze M.M., Mazalov I.S. Vysokotemperaturnye zharo-prochnye nikelevye splavy dlya detalej gazoturbinnyh dvigatelej [High-temperature heat resisting nickel alloys for details of gas turbine engines] // Aviacionnye materialy i tehnologii. 2012. №S. S. 52–57.
  12. Lomberg B.S., Ovsepjan S.V., Bakradze M.M. Osobennosti legirovaniya i termicheskoj obrabotki zharoprochnyh nikelevyh splavov dlja diskov gazoturbinnyh dvigatelej novogo pokolenija [Features of alloying and thermal processing of heat resisting nickel alloys for disks of gas turbine engines of new generation] //Aviacionnye materialy i tehnologii. 2010. №2. S. 3–8.
  13. Alekseev A.V., Yakimovich P.V., Min P.G. Opredelenie primesej v splave na osnove Nb metodom ISP-MS. Chast I [Determination of impurities in Nb-based alloy by ICP-MS method. Part I] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №6. St. 04. Available at: http://www.viam-works.ru (accessed: December 08, 2017). DOI: 10.18557/2307-6046-2015-0-6-4-4.
  14. Alekseev A.V., Yakimovich P.V., Min P.G. Opredelenie primesej v splave na osnove niobiya metodom ISP-MS. Chast II [Determination of impurity in alloy based on Nb by ICP-MS. Part II] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №7. St. 03. Available at: http://www.viam-works.ru (accessed: December 08, 2017). DOI: 10.18557/2307-6046-2015-0-7-3-3.
  15. ASTME E1019-08. Standard Test Methods for Determination of Carbon, Sulfur, Nitrogen, and Oxygen in Steel, Iron, Nickel, and Cobalt Alloys by Various Combustion and Fusion Techniques. 2008. 21 p.