Eliseev E.A., Tonysheva О.А., Yakusheva N.A. Materials and development of the technologies providing the resource trunks of artillery, tank and shooting systems of arms (review) // Proceedings of VIAM. 2017. No. 9 (57). Ст. 03. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2017-0-9-3-3.

Materials and development of the technologies providing the resource trunks of artillery, tank and shooting systems of arms (review)

Eliseev E.A., Tonysheva О.А., Yakusheva N.A.
Abstract

Barrel of different guns and small arms are training in different atmospheric and weather conditions by the contingent of different degree of readiness. Different materials and various technologies of their processing are used for barrels manufacturing. There are identical and specific requirements to barrels which are differ from each other depending on fighting assignment of tools, installation on vehicle and caliber. A trunk is most loaded detail of the weapon and its resource is considerably smaller than all other nodes and details of a weapon. The factors influencing weapon trunks, materials for manufacturing of trunks and ways of their processing are considered in the article.

Keywords
barrel, piece of artillery, tank gun, gun barrel, materials for trunks, manufacturing techniques of barrels, autofrettage.
Reference list
  1. Kablov E.N. Konstrukcionnye i funkcionalnye materialy – osnova ekonomicheskogo i nauchno-tehnicheskogo razvitiya Rossii [Constructional and functional materials are the base of economic and scientific and technical development of Russia] // Voprosy materialovedeniya. 2006. №1. S. 64–67.
  2. Ospennikova O.G. Strategiya razvitiya zharoprochnyh splavov i stalej specialnogo naznacheniya, zashhitnyh i teplozashhitnyh pokrytij [Strategy of development of hot strength alloys and steels special purpose, protective and heat-protective coverings] // Aviacionnye materialy i tehnologii. 2012. №S. S. 19–36.
  3. Tukanov A.G. Tehnologiya proizvodstva strelkovo-pushechnogo i artillerijskogo oruzhiya [Production technology of shooting and gun and gun weapon]. M.: Mashinostroenie, 2010. 238 s.
  4. Hasenbein R.G. Wear and Erosion in Large Caliber Gun Barrels: RTO-MP-AVT-109. U.S. Army Armament Research, Development & Engineering Center. P. 16-1–16-14.
  5. Nowotny S., Spatzier J., Kubisch F. et al. Repair of Erosion Defects in Gun Barrels by Direct Laser Deposition // Journal of Thermal Spray Technology. 2012. Vol. 21. Issue 6. P. 1173–1183.
  6. Kablov E.N. Materialy i himicheskie tehnologii dlya aviacionnoj tehniki [Materials and chemical technologies for aviation engineering] // Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
  7. Emerson R., Kaste R., Carter R. et al. Approaches for the Design of Ceramic Gun Barrels. U.S. Army Research Laboratory Weapons & Materials Research Directorate. P. 1–7.
  8. Kreknin L.T. Proizvodstvo avtomaticheskogo oruzhiya: Ch. 1 [Production of automatic arms: P.1]. Izhevsk: Izhevskij gos. tehnich. un-t, 2012. 236 s.
  9. Tonysheva O.A., Voznesenskajya N.M., Shalkevich A.B., Petrakov A.F. Issledovanie vliyaniya vysokotemperaturnoj termomehanicheskoj obrabotki na strukturu, tehnologicheskie, mehanicheskie i korrozionnye svojstva vysokoprochnoj korrozionnostojkoj stali perehodnogo klassa s povyshennym soderzhaniem azota [Research of influence of high-temperature thermomechanical processing on structure, technological, mechanical and corrosion properties of high-strength corrosion-resistant steel of transitional class with the raised content of nitrogen] // Aviacionnye materialy i tehnologii. 2012. №3. S. 31–36.
  10. Voznesenskaya N.M., Eliseev E.A., Kapitanenko D.V., Tonysheva O.A. Optimizaciya tehnologicheskih rezhimov polucheniya tonkih listov i lenty iz korrozionnostojkoj stali VNS-9-Sh [Optimization of technological modes of receiving thin sheets and tape from the corrosion-resistant steel VNS-9-Sh] // Metally. 2014. №1. S. 46–51.
  11. Orlov M.R., Ospennikova O.G., Gromov V.I. Razvitie mehanizmov vodorodnoj i bejnitnoj hrupkosti konstrukcionnoj stali v processe ekspluatacii krupnogabaritnyh konstrukcij [Development of mechanisms of hydrogen and bainitic embrittlement of structural steel in use large-size designs] // Aviacionnye materialy i tehnologii. 2012. №S. S. 88–93.
  12. De Rosset W.S., Montgomery J.S. Cobalt-Base Alloy Gun Barrel Study. Army Research Laboratory. July, 2014. P. 119–123.
  13. Orlov B.V., Larman E.K., Malikov V.G. Ustrojstvo i proektirovanie stvolov artillerijskih orudij [Device and design of trunks of artillery pieces]. M.: Mashinostroenie, 1976. 432 s.
  14. Zhuk A.B. Strelkovoe oruzhie [Small arms]. M.: Voenizdat, 1992. 735 s.
  15. Alferov V.V. Konstrukciya i raschet avtomaticheskogo oruzhiya [Design and calculation of automatic arms]. M.: Mashinostroenie, 1977. 248 s.
  16. Fedoseev S.V. Oruzhie sovremennoj pehoty [Weapon of modern infantry]. M.: Astrel, 2001. T. 1. 351 s.
  17. Polnaya enciklopediya boevyh tankov i samohodnyh orudij / pod. red. O.V. Doroshkevicha, V.S. Likso, K.L. Arhipova [The full encyclopedia of fighting tanks and self propelled guns / ed. byO. V. Doroshkevich, V. S. Likso, K.L. Arhipov]. M.: AST; Minsk: Harvest, 2008. 384 s.
  18. Sposob izgotovleniya stvola artillerijskogo orudiya: pat. 2419757 Ros. Federaciya [Way of manufacturing of trunk of artillery piece: pat. 2419757 Rus. Federation]; zayavl. 31.05.10; opubl. 27.05.11, Byul. №15. 11 s.
  19. De Rosset W.S., Gray D. Processing of Niobium-Lined M240 Machine Gun Barrels. Army Research Laboratory. November, 2014. P. 1–20.
  20. Salahova R.K. Korrozionnaja stojkost stali 30HGSA s «trehvalentnym» hromovym pokrytiem v estestvennyh i iskusstvennyh sredah [Corrosion resistance of steel 30ХГСА with «trivalent» chrome plating in natural and artificial environments] // Aviacionnye materialy i tehnologii. 2012. №2. S. 59–66.
  21. Audino M.J. Use of Electroplated Chromium in Gun Barrels. US Army RDECOM-ARDEC-Benet Laboratories. DoD Metal Finishing Workshop. Washington, DC. May, 2006. P. 22–23.
  22. Kopejko S. Oruzhie vojskovogo snajpera [Weapon of the army sniper] // Kalashnikov. Oruzhie, boepripasy, snaryazhenie. 2012. №1. S. 46–52.
  23. Kuzmin Yu.A. Sostoyanie i napravleniya razvitiya bronetankovoj tehniki v zarubezhnyh stranah [Condition and the directions of development of armoured equipment in foreign countries] // Zarubezhnoe voennoe obozrenie. 2015. №3. S. 55–59.
  24. Golubcov S.G., Kasha O.B. Osnovnye obrazcy bronetankovoj tehniki FRG [Main samples of armoured equipment of Germany] // Zarubezhnoe voennoe obozrenie. 2014. №10. S. 49–54.
  25. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.