Nochovnaya N.A., Panin P.V. Phase composition and structure formation in VT5, VT20, and VT6 titanium alloys upon thermo-hydrogen treatment and plastic deformation // Proceedings of VIAM. 2017. No. 9 (57). Ст. 01. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2017-0-9-1-1.

Phase composition and structure formation in VT5, VT20, and VT6 titanium alloys upon thermo-hydrogen treatment and plastic deformation

Nochovnaya N.A., Panin P.V.
Abstract

A complex approach to structure and properties transformation of titanium alloys has been in focus, the approach including thermo-hydrogen treatment and plastic deformation combination. It has been shown that thermo-hydrogen treatment together with plastic deformation allow to obtain a multiphase structure in 2 mm sheet semi-finished products of VT5 (Ti–5,8Al), VT20 (Ti–6,2Al–1,2V–1Mo–2Zr), and VT6 (Ti–5,7Al–4,3V) titanium alloys (wt.%). The obtained structure contain α-phase in two structural constituents: primary αI-phase enriched by aluminum up to Ti3Al-based α2-phase, and secondary αdeg-phase depleted by aluminum.

Keywords
titanium alloys, thermo-hydrogen treatment, plastic deformation, phase composition, structure.
Reference list
  1. Kablov E.N. Iz chego sdelat budushhee? Materialy novogo pokolenija, tehnologii ih sozdanija i pererabotki – osnova innovacij [Of what to make the future? Materials of new generation, technology of their creation and processing – basis of innovations] // Krylja Rodiny. 2016. №5. S. 8–18.
  2. Kablov E.N. Materialy dlya aviakosmicheskoy tekhniki [Materials for aerospace equipment] // Vse materialy. Entsiklopedicheskiy spravochnik. 2007. №5. S. 7–27.
  3. Nochovnaja N.A. Perspektivy i problemy primenenija titanovyh splavov [Perspectives and problems of application of titanium alloys] // Sb. dokl. «Perspektivy razvitija i primenenija titanovyh splavov dlja samoletov, raket, dvigatelej i sudov». M.: VIAM, 2007. S. 4–8.
  4. Balabuev P.V. Titanovye splavy v izdelijah ANTK im. O.K. Antonova [Titanium alloys in products of ASTC of O.K. Antonov] // Titan. 1998. №1 (10). S. 15–19.
  5. Bratuhin A.G., Kolachev B.A., Sadkov V.V. i dr. Tehnologija proizvodstva titanovyh samo-letnyh konstrukcij [Production technology of titanic aircraft designs]. M.: Mashinostroenie, 1995. 448 s.
  6. Skvorcova S.V., Ilin A.A., Becofen S.Ja., Filatov A.A., Dzunovich D.A., Panin P.V. Ani-zotropija mehanicheskih svojstv i tekstura listovyh polufabrikatov iz titanovyh splavov [Anisotropy of mechanical properties and structure of sheet semi-finished products from titanium alloys] // Tehnologija legkih splavov. 2006. №1–2. S. 81–87.
  7. Ilin A.A., Kolachev B.A., Polkin I.S. Titanovye splavy. Sostav, struktura, svojstva: spravoch-nik [Titanium alloys. Structure, structure, properties: directory]. M.: VILS–MATI, 2009. 520 s.
  8. Kajbyshev O.A., Utjashev F.Z. Sverhplastichnost, izmelchenie struktury i obrabotka trudnodeformiruemyh splavov [Over plasticity, crushing of structure and processing of difficult deformable alloys]. M.: Nauka, 2002. 438 s.
  9. Panin P.V., Manohin S.S., Dzunovich D.A. Poluchenie i issledovanie submikrokristallicheskoj struktury v titanovyh splavah pri obratimom legirovanii vodorodom i plasticheskoj deformacii [Receiving and research of submicrocrystal structure in titanium alloys at reversible alloying hydrogen and plastic strain] // Voprosy materialovedenija. 2016. №4 (88). S. 7–17.
  10. Ilin A.A., Skvorcova S.V., Panin P.V., Shalin A.V. Vlijanie termovodorodnoj obrabotki i plasticheskoj deformacii na strukturoobrazovanie v titanovyh splavah raznyh klassov [Influence of thermohydrogen treating and plastic strain on structurization in titanium alloys of different classes] // Aviacionnaja promyshlennost. 2009. №4. S. 31–36.
  11. Panin P.V. Zakonomernosti formirovanija fazovogo sostava i struktury v titanovyh splavah pri termovodorodnoj obrabotke i plasticheskoj deformacii: avtoref. dis. … kand. tehn. Nauk [Patterns of forming of phase structure and structure in titanium alloys at thermohydrogen treating and plastic strain: thesis cand. Sc. (Tech.)] M.: MATI, 2009. 24 s.
  12. Ilin A.A., Kolachev B.A., Nosov V.K., Mamonov A.M. Vodorodnaja tehnologija titanovyh splavov [Hydrogen technology of titanium alloys]. M.: MISiS, 2002. 392 s.
  13. Kolachev B.A., Ilin A.A., Nosov V.K., Mamonov A.M. Dostizhenija vodorodnoj tehnologii titanovyh splavov [Achievements of hydrogen technology of titanium alloys] // Tehnologija legkih splavov. 2007. №3. S. 10–26.
  14. Ovchinnikov A.V., Nosov V.K., Afonin V.E., Panin P.V. Osnovnye zakonomernosti deformacii splavov titan-vodorod [Main patterns of deformation of alloys titanium-hydrogen] // Tehnologija legkih splavov. 2007. №3. S. 96–99.
  15. Ilin A.A., Skvorcova S.V., Mamonov A.M., Kollerov M.Ju. Fazovye i strukturnye prevrashhenija v titanovyh splavah raznyh klassov pod dejstviem vodoroda [Phase and structural transformations in titanium alloys of different classes under the influence of hydrogen] // Titan. 2007. №1 (20). S. 32–37.
  16. Skvorcova S.V., Popova Ju.A., Panin P.V., Grushin I.A., Kuryshev E.A. Vlijanie termicheskoj obrabotki na strukturu i svojstva svarnyh soedinenij iz titanovogo splava VT23 [Influence of thermal processing on structure and property of welded connections from BT23 titanium alloy] // Titan. 2011. №2 (32). S. 16–21.
  17. Skvorcova S.V., Panin P.V., Nochovnaja N.A., Grushin I.A., Mitropolskaja N.G. Vlijanie vodoroda na fazovye i strukturnye prevrashhenija v titanovom splave VT6 [Influence of hydrogen on phase and structural transformations in BT6 titanium alloy] // Tehnologija legkih splavov. 2011. №4. S. 35–40.
  18. Panin P.V., Dzunovich D.A., Zasypkin V.V. Sozdanie dvuhfaznoj kompozitnoj struktury v alfa-splave Ti–6Al s pomoshhju termovodorodnoj obrabotki [Creation of diphasic composite structure in Ti–6Al alpha alloy by means of thermohydrogen treating] // Nauchnye trudy (Vestnik MATI). 2012. №19 (91). S. 33–37.
  19. Panin P.V., Grushin I.A., Mitropol'skaja N.G. Issledovanie zakonomernostej izmenenija strukturno-fazovogo sostojanija titanovogo splava VT6 pri dopolnitelnom legirovanii vodorodom [Research of patterns of change of structural and phase condition of BT6 titanium alloy at additional alloying hydrogen] // Nauchnye trudy (Vestnik MATI). 2013. №20 (92). S. 31–34.
  20. Panin P.V., Shirjaev A.A., Dzunovich D.A. Postroenie temperaturno-koncentracionnoj diagrammy fazovogo sostava titanovogo splava VT6, dopolnitel'no legirovannogo vodorodom [Creation of the temperature and concentration chart of phase composition of the BT6 titanium alloy which has been in addition alloyed by hydrogen] // Tehnologija mashinostroenija. 2014. №3 (141). S. 5–9.
  21. Panin P.V., Dzunovich D.A., Alekseev E.B. Sposoby opisaniya fazovogo sostava titanovyh splavov, dopolnitelno legirovannyh vodorodom (obzor) [Ways of phase areas representation in titanium alloys additionally doped with hydrogen (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №3. St. 03. Available at: http://www.viam-works.ru (accessed: August 07, 2017). DOI: 10.18577/2307-6046-2015-0-3-3-3.
  22. Panin P.V., Dzunovich D.A., Alekseev E.B. Fazovyj sostav i struktura titanovogo splava VT6, dopolnitelno legirovannogo vodorodom, posle vakuumnogo otzhiga [Phase composition and structure of hydrogenated titanium alloy VT6 after vacuum annealing] // Trudy VIAM: jelektron. nauch.-tehnich. zhurn. 2016. №2 (38). St. 05. Available at: http://www.viam-works.ru (accessed: August 07, 2017). DOI: 10.18577/2307-6046-2016-0-2-5-5.
  23. Panin P.V., Dzunovich D.A., Shiryaev A.A. Issledovanie termicheskoj stabilnosti struktury titanovogo splava VT6 posle termovodorodnoj obrabotki [Research on thermal stability of VT6 titanium alloy structure after thermohydrogen treatment] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №3. St. 06. Available at: http://www.viam-works.ru (accessed: August 07, 2017). DOI: 10.18577/2307-6046-2016-0-3-6-6.
  24. Dzunovich D.A., Shalin A.V., Panin P.V. Struktura, tekstura i mehanicheskie svojstva de-formirovannyh polufabrikatov iz splava VT6, poluchennyh po promyshlennym i opytnym tehnologijam [Structure, structure and mechanical properties of the deformed semi-finished products from alloy of BT6 received on industrial and pilot technologies] // Deformacija i razrushenie materialov. 2017. №6. S. 19–27.
  25. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the develop-ment of materials and technologies of their processing for the period until 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  26. Nochovnaja N.A., Panin P.V., Kochetkov A.S. Problemy poluchenija himicheski i strukturno odnorodnyh slitkov iz zharoprochnyh splavov na osnove gamma-aljuminida titana [Receiving problems chemically and structurally uniform ingots from hot strength alloys on the basis of titanium gamma aluminide] // Materialy konf. «Problemy proizvodstva slitkov i polufabrikatov iz slozhnolegirovannyh i intermetallidnyh titanovyh splavov» (30 okt. 2015 g.). M.: VIAM, 2015. St. 03. 1 jelektr. optich. disk (CD).
  27. Kablov D.E., Panin P.V., Shiryaev A.A., Nochovnaya N.A. Opyt ispolzovaniya vakuumno-dugovoj pechi ALD VAR L200 dlya vyplavki slitkov zharoprochnyh splavov na osnove alju-minidov titana [The use of ADL VAR L200 vacuum-arc furnace for ingots fabrication of high-temperature titanium aluminides base alloys] //Aviacionnye materialy i tehnologii. 2014. №2 (31). S. 27–33. DOI: 10.18577/2071-9140-2014-0-2-27-33.
  28. Ilin A.A. Mehanizm i kinetika fazovyh i strukturnyh prevrashhenij v titanovyh splavah [The mechanism and kinetics of phase and structural transformations in titanium alloys]. M.: Nauka, 1994. 304 s.