Bolshakov V.A., Solodilov V.I., Korokhin R.A., Kondrashov S.V., Merkulova Yu.I., Dyachkova T.P. Research of crack resistance of polymeric composite materials fabricatedby infusion using various concentrates on the basis of modified CNT // Proceedings of VIAM. 2017. No. 7 (55). Ст. 09. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2017-0-7-9-9.

Research of crack resistance of polymeric composite materials fabricatedby infusion using various concentrates on the basis of modified CNT

Bolshakov V.A., Solodilov V.I., Korokhin R.A., Kondrashov S.V., Merkulova Yu.I., Dyachkova T.P.
Abstract

In the Russian Federation aircraft component parts and units are usually manufactured by an autoclave solvent polymer impregnation processing technique. However foreign companies used nonsolvent processing technique. Molding without autoclave (for example infusion molding or vacuum and pressure impregnation) sufficiently decreases the FRP production costs. Vacuum impregnation is the matter of the particular interest because there is no need to use sophisticated equipment. For ensuring operability of a material modification by its modified carbon nanotubes is represented especially interesting.

Keywords
carbon plastics, infusional formation, residual durability at compression after blow, functional carbon nanotubes, heat-resistant.
Reference list
  1. Dushin M. I., Hrulkov A.V., Muhametov R.R., Chursova L.V. Osobennosti izgotovleniya izdelij iz PKM metodom propitki pod davleniem [Features of manufacturing of products from PCM impregnation method under pressure] // Aviacionnye materialy i tehnologii. 2012. №1. S. 18–26.
  2. Grigorev M.M., Kogan D.I., Tverdaya O.N., Panina N.N. Osobennosti izgotovleniya PKM metodom RFI [Features of manufacturing of PCM RFI method] // Trudy VIAM: electron. nauch.-tehnich. zhurn. 2013. №4. St. 03. Available at: http://www.viam-works.ru (accessed: September, 22 2016).
  3. Sokolov I.I., Raskutin A.E. Ugleplastiki i stekloplastiki novogo pokoleniya [Coalplastics and fibreglasses of new generation] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №4. St. 09. Available at: http://www.viam-works.ru (accessed: September, 22 2016).
  4. Muhametov R.R., Ahmadieva K.R., Kim M.A., Babin A.N. Rasplavnye svyazujushhie dlya perspektivnyh metodov izgotovleniya PKM novogo pokoleniya [Melt binding for perspective methods of production of PCM of new generation] // Aviacionnye materialy i tehnologii. 2012. №S. S. 260–265.
  5. Gunyaev G.M., Kablov E.N., Aleksashin V.M. Modificirovanie konstrukcionnyh ugleplastikov uglerodnymi nanochasticami [Modifying constructional carbon plastics carbon nanoparticles] // Rossijskij himicheskij zhurnal. 2010. T. 54. №1. S. 3–11.
  6. Kablov E.N., Kondrashov S.V., Yurkov G.Yu. Perspektivy ispolzovaniya uglerodsoderzhashhih nanochastic v svyazuyushhih dlya polimernyh kompozicionnyh materialov [Perspectives of use of carbon-containing nanoparticles in binding for polymeric composite materials] // Rossijskie nanotehnologii. 2013. T. 8. №3–4. S. 24–42.
  7. Aldoshin S.M., Badamshina E.R., Kablov E.N. Polimernye nanokompozity – novoe pokolenie polimernyh materialov s povyshennymi ekspluatacionnymi harakteristikami [Polymeric nanocomposites are the new generation of polymeric materials with the increased utilization properties] // Sb. tez. dokl. I Mezhdunar. foruma po nanotehnologiyam «Rosnanoteh 08». M., 2008. S. 385–387.
  8. Kablov E.N. Konstrukcionnye i funkcionalnye materialy – osnova ekonomicheskogo i nauchno-tehnicheskogo razvitiya Rossii [Constructional and functional materials – basis of economic and scientific and technical development of Russia] // Voprosy materialovedeniya. 2006. №1. S. 64–67.
  9. Kablov E.N. Kompozity: segodnya i zavtra [Composites: today and tomorrow] // Metally Evrazii. 2015. №1. S. 36–39.
  10. Bekyarova E., Thostenson E.T., Yu A. et al. Functionalized single-walled carbon nanotubes for carbon fiber-epoxy composites // J. Phys. Chem. C. 2007. Vol. 111. P. 17865–17871.
  11. Gojny F.H., Wichmann M.H.G., Fiedler B., Bauhofer W., Schulte K. Influence of nano-modification on the mechanical and electrical properties of conventional fiber-reinforced composites // Composites: Part A. 2005. Vol. 36. P. 1525–1535.
  12. Yokozeki T., Iwahori Y., Ishiwata S., Enomoto K. Mechanical properties of CFRP laminates manufactured from unidirectional prepregs using CSCNT-dispersed epoxy // Composites: Part A. 2007. Vol. 38. P. 2121–2130.
  13. Davis D.C., Whelan B.D. An experimental study of interlaminar shear fracture toughness of a nanotube reinforced composite // Composites: Part B. 2011. Vol. 42. P. 105–116.
  14. Almuhammadi K., Alfano M., Yang Y., Lubineau G. Analysis of interlaminar fracture toughness and damage mechanisms in composite laminates reinforced with sprayed multi-walled carbon nanotubes // Materials and Design. 2014. Vol. 53. P. 921–927B.
  15. Guan A.J., Mirjalili V., Zhang Y. et al. Enhancement of mechanical performance of epoxy/carbon fiber laminate composites using single-walled carbon nanotubes // Composites Science and Technology. 2011. Vol. 71. P. 1569–1578.
  16. Mujika F., Vargas G., Ibarretxe J. et al. Influence of the modification with MWCNT on the interlaminar fracture properties of long carbon fiber composites // Composites: Part B. 2012. Vol. 43. P. 1336–1340.
  17. Mirjalili V., Ramachandramoorthy R., Hubert P. Enhancement of fracture toughness of carbon fiber laminated composites using multi wall carbon nanotubes // CARBON. 2014. Vol. 79. P. 413–423.
  18. Fenner J.S., Daniel I.M. Hybrid Nanoreinforced Carbon/Epoxy Composites for Enhanced Damage Tolerance and Fatigue Life // Composites: Part A. 2014. DOI: 10.1016/j.compositesa 2014.05.02315.
  19. Yokozeki T., Iwahori Y., Ishibashi M. et al. Fracture toughness improvement of CFRP laminates by dispersion of cup-stacked carbon nanotubes // Composites Science and Technology. 2009. Vol. 69. P. 2268–2273.
  20. White K.L., Sue H.J. Delamination toughness of fiber-reinforced composites containing a carbon nanotube/polyamide-12 epoxy thin film interlayer // Polymer. 2012. Vol. 53. P. 37–4215.
  21. Zhu Ye, Bakis C.E., Adair J.H. Effects of carbon nanofiller functionalization and distribution on interlaminar fracture toughness of multi-scale reinforced polymer composites // CARBON. 2012. Vol. 50. P. 1316–1331.
  22. Muhametov R.R., Merkulova Yu.I., Chursova L.V. Termoreaktivnye polimernye svyazuyushhie s prognoziruemym urovnem reologicheskih i deformativnyh svojstv [Thermosetting polymeric binding with predicted level of rheological and deformativny properties] // Klei. Germetiki. Tehnologii. 2012. №5. S. 19–24.
  23. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  24. Merkulova Yu.I., Kondrashov S.V., Dyachkova T.P., Marahovskij P.S., Yurkov G.Yu. Vliyanie dispergirovannyh v svyazuyushhem uglerodnyh nanotrubok na svojstva epoksinanokompozita [Influence dispersed in binding carbon nanotubes on properties epoksinanokompozita] // Zhurnal prikladnoj himii. 2015. T. 88. №11. S. 1636–1642.
  25. Babaevskij P.G., Kulik S.G. Treshhinostojkost otverzhdennyh polimernyh kompozicij [Crack firmness of the hardened polymeric compositions]. M.: Himiya, 1991. 336 s.
  26. Marahovskij P.S., Kondrashov S.V., Akatenkov R.V., Aleksashin V.M., Anoshkin I.V., Mansurova I.A. O modifikacii teplostojkih epoksidnyh svyazuyushhih uglerodnymi nanotrubkami [About updating heatresistant epoxy binding carbon nanotubes] // Vestnik Moskovskogo gosudarstvennogo tehnicheskogo universiteta im. N.E. Baumana. Ser.: Mashinostroenie. 2015. №2 (101). S. 118–127.
  27. Akatenkov R.V., Aleksashin V.N., Anoshkin I.V., Babin A.N., Bogatov V.A., Grachev V.P., Kondrashov S.V., Minakov V.T., Rakov E.G. Vliyanie malyh kolichestv funkcionalizirovannyh nanotrubok na fiziko-mehanicheskie svojstva i strukturu epoksidnyh kompozicij [Influence of trace amounts of functional nanotubes on physicomechanical properties and structure of epoxy compositions] // Deformaciya i razrushenie materialov. 2011. №11. S. 35–39.
  28. Solodilov V.I., Korohin R.A., Gorbatkina Yu.A., Kuperman A.M. Sravnenie energij razrusheniya epoksisulfonovyh matric i odnonapravlennyh namotochnyh kompozitov na ih osnove [Comparison of energy of destruction of epoksisulfonovy matrixes and unidirectional winding composites on their basis] // Mehanika kompozitnyh materialov. 2015. T. 51. №2. S. 253–272.