Choice of technological modes of drying fibrous foam materials

Beljaev А.А., Bespalova E.E.
Abstract

Development of technical progress in aerospace, transport, power and other industries is inseparably linked with creation of new and improvement traditional materials [1–4]. Broad application of radio engineering and electrotechnical means defines need for development of radio absorbing materials (RAM) with the set technical characteristics. In this article results of working off of technological modes of drying fibrous foam materials, broadband radio absorbing materials applied to manufacturing are provided. Influence of modes of heat treatment for receiving stable and uniform fibrous materials is shown. Work is executed within implementation of the complex scientific direction 15.3. «Materials and coverings for protection against EMR, shock, vibrating, acoustic and electric influences» («The strategic directions of development of materials and technologies of their processing for the period till 2030»)

Keywords
radio absorbing material, foam material, inorganic fibers, electromagnetic wave, electromagnetic radiation.
Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] // Vse materialy. Enciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  3. Kablov E.N. Materialy i himicheskie tehnologii dlya aviacionnoj tehniki [Materials and chemical technologies for aviation engineering] // Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
  4. Dospehi dlya «Burana». Materialy i tehnologii VIAM dlya MKS «Energiya–Buran» / pod obshh. red. E.N. Kablova [Armor for «Buran». Materials and VIAM technologies for ISS of «Energiya–Buran»]. M.: Nauka i zhizn, 2013. 128 s.
  5. Bibikov S.B., Prokofev M.V., Kulikovskij K.E., Zhuravlev V.A. Razrabotka materialov i pokrytij, ispolzuemyh dlya provedeniya radiotehnicheskih ispytanij i obespecheniya elektromagnitnoj sovmestimosti [Development of materials and the coverings used for carrying out radio engineering tests and ensuring of electromagnetic compatibility] // Voprosy oboronnoj tehniki. Ser.: Tehnicheskie sredstva protivodejstviya terrorizmu. 2013. №5–6. S. 56–64.
  6. Bibikov S.B., Titov A.N., Cherepanov A.K. Sintez materiala s zadannym koefficientom otrazheniya v shirokom diapazone chastot i uglov padeniya [Material synthesis with the set reflection coefficient with the broad range of frequencies and incidence angles] // Sb. trudov XV Mezhdunar. nauch.-tehnich. konf. «Radiolokaciya, navigaciya, svyaz'». Voronezh, 2009. S. 1578–1584.
  7. Mihajlin Yu.A. Specialnye polimernye kompozicionnye materialy [Special polymeric composite materials]. SPb.: Nauchnye osnovy i tehnologii, 2014. 664 s.
  8. Latypova A.F., Kalinin Yu.E. Analiz perspektivnyh radiopogloshhayushhih materialov [The analysis of perspective radio absorbing materials] // Vestnik Voronezhskogo gos. teh. un-ta. 2012. T. 8. №6. S. 70–76.
  9. Belyaev A.A., Kondrashov S.V., Lepeshkin V.V., Romanov A.M. Radiopogloshhayushhie materialy [Radio absorbing materials] // Aviacionnye materialy i tehnologii. 2012. №S. S. 348–352.
  10. Belyaev A.A., Bespalova E.E., Romanov A.M. Pozharobezopasnye radiopogloshhayushhie materialy dlya bezehovyh kamer [Fireproof radio absorbing materials for anechoic cameras] // Aviacionnye materialy i tehnologii. 2013. №1. S. 53–55.
  11. Lushina M.V., Parshin S.G., Rzhevskij A.A. Sovremennye ekraniruyushhie i radiopogloshhayushhie materialy [Modern shielding and radio absorbing materials] // Sistemy upravleniya i obrabotka informacii. 2011. №22. S. 208–223.
  12. Nikolskij V.V., Nikolskaya T.I. Elektrodinamika i rasprostranenie radiovoln [Electrodynamics and radio propagation]. M.: URSS, 2012. S. 163–164.
  13. Shirokov V.V., Romanov A.M. Issledovanie dielektricheskih harakteristik steklosotoplasta volnovodnym metodom [Waveguide method research of honeycomb glass fibre plastics dielectric characteristics] // Aviacionnye materialy i tehnologii. 2013. №4. S. 62–68.
  14. Belyaev A.A., Agafonova A.S., Antipova E.A., Botanogova E.D. Konstrukcionnyj radiopogloshhayushhij material trehslojnoj struktury s soglasuyushhim sloem [Constructional radio absorbing material of three-layered structure with approval layer] // Trudy VIAM: elektron. nauch. tehnich. zhurn. 2013. №7. St. 02. Available at: http://www.viam-works.ru (accessed: May 15, 2017).
  15. Agafonova A.S., Belyaev A.A., Kondrashov E.K., Romanov A.M. Osobennosti formirovaniya monolitnyh konstrukcionnyh radiopogloshhayushhih materialov na osnove kompozitov, napolnennyh rezistivnym voloknom [Features of the formation of monolithic structural radio absorbing materials based on composites filled with resistive fibers] // Aviacionnye materialy i tehnologii. 2013. №3. S. 56–59.
  16. Bespalova E.E., Kondrashov E.K. Osobennosti korrektirovki receptury pozharobezopasnogo materiala dlya bezehovyh kamer pri izmenenii parametrov radiopogloshhayushhego napolnitelya [Features of updating of a composition of a fireproof material for anechoic chambers when changed of parameters radio absorbing filler] // Aviacionnye materialy i tehnologii. 2014. №2. S. 48–52. DOI: 10.18577/2071-9140-2014-0-2-48-52.
  17. Romanov A.M., Belyaev A.A., Shirokov V.V. Osobennosti optimizacii rezonansnyh radiopogloshhayushhih materialov nemagnitnogo tipa [Peculiar features of optimization of resonant radar-absorbing materials of nonmagnetic type] // Trudy VIAM: elektron. nauch. tehnich. zhurn. 2014. №11. St. 05. Available at: http://www.viam-works.ru (accessed: May 15, 2017). DOI: 10.18577/2307-6046-2014-0-11-5-5.
  18. Bibikov S.B., Zasovin E.A., Cherepanov A.K., Hmelnik G.I. Matematicheskoe modelirovanie parametrov mnogoslojnyh radiopogloshhayushhih pokrytij [Mathematical modeling of parameters of multi layer radio absorbing coatings] // Sb. trudov XV Mezhdunar. nauch.-tehnich. konf. «Radiolokaciya, navigaciya, svyaz'». Voronezh, 2009. S. 1585–1595.
  19. Volkov V.P., Zeleneckij A.N. i dr. Poluchenie radiozashhitnyh polimernyh materialov ponizhennoj goryuchesti [Receiving radio protective polymeric materials of the lowered combustibility] // Plasticheskie massy. 2008. №6. S. 42–46.
  20. D'yachenko P.B., Rybalko V.P., Nikityuk A.I., Pisarenko E.I., Kireev V.V. Pozharobezopasnye termostojkie polimernye kompozicionnye materialy s ponizhennoj plotnostyu [Fireproof heat-resistant polymeric composite materials with lowered density] // Uspehi v himii i himicheskoj tehnologii. T. XXV. 2011. №2 (118). S. 94–99.
  21. Grashchenkov D.V., Shchetanov B.V., Tinyakova E.V., Shcheglova T.M. O vozmozhnosti ispolzovaniya kvartsevogo volokna v kachestve svyazuyushchego pri poluchenii legkovesnogo teplozashchitnogo materiala na osnove volokon Al2O3 [About possibility of use of quartz fiber as lightweight heat-protective material binding at receiving on the basis of Al2O3 fibers] // Aviacionnye materialy i tehnologii. 2011. №4. S. 8‒14.
  22. Micmaher M.Yu., Torgovanov V.A. Bezehovye kamery SVCh. [Microwave ovens anechoic cameras]. M.: Radio i svyaz, 1982. 129 s.
  23. Maslov M.Yu., Semakov L.M., Skachkov D.V. Ispytatelnaya bezehovaya kamera diapazona 1200 MGc [Test anechoic chamber of the range of 1200 MHz] // Telekommunikacii i transport. 2009. Spec. vyp.: Tehnologii informacionnogo obshhestva. S. 123–125.
  24. Radiopogloshhayushhij material: pat. 2417491 Ros. Federaciya [Radio absorbing material: pat. 2417491 Rus. Federation]; opubl. 27.04.11.