Titov V.I., Dvoretskov R.M. Determination of calcium as a dopant in the casting of magnesium alloys of the Mg–Al–Zn–Mn and spectrophotometric atomic emission techniques // Proceedings of VIAM. 2017. No. 4 (52). Ст. 10. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2017-0-4-10-10.

Determination of calcium as a dopant in the casting of magnesium alloys of the Mg–Al–Zn–Mn and spectrophotometric atomic emission techniques

Titov V.I., Dvoretskov R.M.
Abstract

The result of this work it is shown that the photometric determination of calcium main alloying elements (Al, Zn, Mn), present in the casting of magnesium alloys of the Mg–Al–Zn–Mn, no effect on the magnitude of optical density for determining the content of calcium in the alloy. To obtain reproducible results, the experiment should be carried out in a quartz dish.

Determination of calcium in magnesium alloys by atomic-emission spectrometry with inductively coupled plasma and simultaneously allows to define other alloying elements comprising the alloy. It was found that they do not adversely affect the quantitative determination of calcium. For the studied calcium concentration range selected the most sensitive and the least susceptible to interference of analytic line Ca.

To control the correctness and reliability of the determination by analyzing the results of calcium magnesium alloys used in model solutions. The content items are within tolerances.

Procedures for photometric and atomic-emission determination of calcium in casting magnesium alloys of the Mg–Al–Zn–Mn.

The work is executed within the implementation of the complex scientific direction 2.1. «Fundamental Oriented Research» («The strategic directions of development of materials and technologies of their processing for the period till 2030»)

Keywords
magnesium alloys of Mg–Al–Zn–Mn, calcium, spectrophotometry, atomic emission spectrometry with inductively coupled plasma.
Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Materialy dlya izdeliya «Buran» – innovacionnye resheniya formirovaniya shestogo tehnologicheskogo uklada [Materials for «Buran» spaceship – innovative solutions of formation of the sixth technological mode] //Aviacionnye materialy i tehnologii. 2013. №S1. S. 3–9.
  3. Kablov E.N. Iz chego sdelat budushhee? Materialy novogo pokoleniya, tehnologii ih sozdaniya i pererabotki – osnova innovacij [What the future to make of? Materials of new generation, technology of their creation and processing – basis of innovations] // Krylya Rodiny. 2016. №5. S. 8–18.
  4. Kablov E.N. Kontrol kachestva materialov – garantiya bezopasnosti ekspluatacii aviacionnoj tehniki [Quality control of materials – security accreditation of operation of aviation engineering] // Aviacionnye materialy i tehnologii. 2001. №1. S. 3–8.
  5. Kablov E.N. Aviacionnoe materialovedenie v XXI veke. Perspektivy i zadachi [Aviation materials science in the XXI century. Perspectives and tasks] // Aviacionnye materialy. Izbrannye trudy VIAM 1932–2002. M.: MISIS–VIAM, 2002. S. 23–47.
  6. Kornysheva I.S., Volkova E.F., Goncharenko E.S., Muhina I.Yu. Perspektivy primeneniya magnievyh i litejnyh alyuminievyh splavov [Perspectives of application of magnesium and cast aluminum alloys] // Aviacionnye materialy i tehnologii. 2012. №S. S. 212–222.
  7. Antipov V.V. Strategiya razvitiya titanovyh, magnievyh, berillievyh i alyuminievyh splavov [Strategy of development of titanium, magnesium, beryllium and aluminum alloys] // Aviacionnye materialy i tehnologii. 2012. №S. S. 157–167.
  8. Muhina I.Yu., Duyunova V.A., Uridiya Z.P. Perspektivnye litejnye magnievye splavy [] // Novosti materialovedeniya. Nauka i tehnika: elektron. nauch.-tehnich. zhurn. 2013. №6. St. 05. Available at: http://www.materialsnews.ru (accessed: December 12, 2016).
  9. Koltygin A.V., Pliseckaya I.V. Perspektivy razvitiya magnievyh litejnyh splavov, svyazannye s primeneniem kal'ciya v kachestve legiruyushhej dobavki [Perspectives of development of the magnesium cast alloys, connected using calcium as alloying additive] // Litejshhik Rossii. 2012. №1. S. 38–41.
  10. Koltygin A.V., Pliseckaya I.V. O povedenii kalciya v litejnyh magnievyh splavah sistemy Mg–Al–Zn–Mn [About behavior of calcium in cast magnesium alloys of Mg-Al-Zn-Mn system] // Litejnoe proizvodstvo. 2010. №8. S. 2–6.
  11. Belov V.D., Koltygin A.V., Belov N.A., Pliseckaya I.V. Innovacii v oblasti litejnyh magnievyh splavov [Innovations in the field of cast magnesium alloys] // Metallurg. 2010. №5. S. 67–70.
  12. Koltygin A.V., Bazlova T.A., Pliseckaya I.V. Vliyanie kalciya na process polucheniya i strukturu magniya, vyplavlennogo v usloviyah besflyusovoj plavki [Influence of calcium on process of receiving and structure of the magnesium melted in the conditions of fluxless melting] // Metallovedenie i termicheskaya obrabotka metallov. 2012. №10 (688). S. 50–54.
  13. Koltygin A.V., Pliseckaya I.V. Uluchshenie svojstv magnievyh splavov tipa ML5 s pomoshhyu dobavok kalciya [Improvement of properties of magnesium alloys of the ML5 type by means of calcium additives] // Sb. mater. konf. «Progressivnye litejnye tehnologii». M.: MISiS, 2011. S. 38–40.
  14. Koltygin A.V., Pliseckaya I.V. Osobennosti plavki magnievyh splavov, legirovannyh kalciem v zashhitnoj gazovoj srede, soderzhashhej elegaz [Features of melting of the magnesium alloys alloyed by calcium in the protective gas environment, containing elegas] // Ibid. S. 40–42.
  15. Karpov Yu.A., Baranovskaya V.B. Rol i vozmozhnosti analiticheskogo kontrolya v metallurgii [Role and possibilities of analytical control in metallurgy] // Tsvetnye metally. 2016. №8 (884). S. 63–67. DOI:10.17580/tsm.2016.08.09.
  16. Karpov Yu.A., Baranovskaya V.B. Vozmozhnosti i problemy sovremennoj analiticheskoj himii neorganicheskih materialov [Opportunities and problems of modern analytical chemistry of inorganic materials] // Izvestiya Akademii nauk. Ser.: Himicheskaya. 2015. №8. S. 1989.
  17. Tormysheva E.A., Smirnova E.V., Ermolaeva T.N. Opredeleniya oksidov zheleza, kal'ciya i alyuminiya v magnezialnyh ogneuporah metodom AES s ISP v usloviyah mikrovolnovogo razlozheniya proby [Definitions of iron oxides, calcium and aluminum in magnezialny refractory materials nuclear power plant method with ISP in the conditions of microwave decomposition of test] // Vestnik Voronezhskogo Gosudarstvennogo universiteta. Ser.: Himiya. Biologiya. Farmaciya. 2010. №1. S. 51–55.
  18. Pupyshev A.A., Danilova D.A. Ispolzovanie atomno-emissionnoj spektrometrii s induktivno-svyazannoj plazmoj dlya analiza materialov i produktov chernoj metallurgii [Use of nuclear and emission spectrometry with the inductive and connected plasma for the analysis of materials and products of ferrous metallurgy] // Analitika i kontrol. 2007. T. 11. №2–3. S. 131–181.
  19. Zagvozdkina T.N., Karachevtsev F.N., Dvoretskov R.M. Primenenie modelnyh rastvorov v atomno-absorbcionnom analize [Application of model solutions for ICP-AES procedures] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №3. St. 10. Available at: http://www.viam-works.ru (accessed: December 12, 2016). DOI: 10.18577/2307-6046-2015-0-3-10-10.