Analysis of the temperature-time parameters mode curing PCM with specified characteristics

Satdinov R.A., Istyagin S.E., Veshkin E.A
Abstract

In addition to the general of requirements for polymeric composite materials such as tensile, compression, flexural modulus of elasticity and so on. There are further defined construction assignment. Known that for bearing structures materials these characteristics are strength and cyclic alternating load and specific mechanical properties, the materials in the interior given special attention fire properties for details entering into direct contact with the aggressive or the environment - chemical resistance, etc. As the design of new materials and in adaptation to already existing material projected new constructs, as well as modifications in material through the various additives require comprehensive analysis of the actual properties.

The application of thermokinetic analysis for prediction solidification mode and fiberglass prepreg based on phenol-formaldehyde binder ВСФ-16М. Revealed three step polymerization reaction of a phenol-formaldehyde binder ВСФ-16М. Based on the analysis of physical and chemical properties of the chosen mode is the optimal curing it at a temperature of 140±5°C. Comparisons are carried with experimental design parameters.

The work in the implementation comprehensive scientific direction 17.2. «The development on the basis of fiberglass fabric with low surface density and fast hardening combustible binder WSF-16M» («The strategic directions of development of materials and technologies of their processing for the period till 2030») 

Keywords
polymer composite materials, thermo-kinetic analysis, physical and chemical properties, of phenol-formaldehyde binder, prepreg, plastic.
Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Veshkin E.A., Postnov V.I., Abramov P.A. Puti povysheniya kachestva detalej iz PKM pri vakuumnom formovanii [Ways of improvement of quality of details from PCM at vacuum formation] // Izvestiya Samarskogo nauchnogo centra RAN. 2012. №4 (3). S. 834–839.
  3. Veshkin E.A., Abramov P.A., Postnov V.P., Strelnikov S.V. Vliyanie tehnologii podgotovki preprega na svojstva PKM [Influence of technology of preparation of prepreg on PCM properties] // Vse materialy. Enciklopedicheskij spravochnik. 2013. №9. S. 8–14.
  4. Postnov V.P., Veshkin E.A., Abramov P.A. Osobennosti podgotovki polimernogo svyazuyushhego dlya snizheniya poristosti stekloplastikov, poluchaemyh metodom vakuumnogo formovaniya [Features of preparation polymeric binding for decrease in porosity of the fibreglasses received by method of vacuum formation] // Izvestiya Samarskogo nauchnogo centra RAN. 2011. T. 13. №4 (2). S. 462–468.
  5. Dushin M.I., Hrulkov A.V., Muhametov R.R. Vybor tehnologicheskih parametrov avtoklavnogo formovaniya detalej iz polimernyh kompozicionnyh materialov [A choice of technological parameters of autoclave formation of details from polymeric composite materials] // Aviacionnye materialy i tehnologii. 2011. №3. S. 20–26.
  6. Kablov E.N. Kontrol kachestva materialov – garantiya bezopasnosti ekspluatacii aviacionnoj tehniki [Quality control of materials – security accreditation of operation of aviation engineering] // Aviacionnye materialy i tehnologii. M.: VIAM, 2001. №1. S. 3–8.
  7. Sokolov I.I., Raskutin A.E. Ugleplastiki i stekloplastiki novogo pokoleniya [Carbon plastics and fibreglasses of new generation] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №4. St. 09. Available at: http://www.viam-works.ru (accessed: July 12, 2016).
  8. Kogan D.I., Dushin M.I., Borshhev A.N., Veshkin E.A., Abramov P.A., Makrushin K.V. Svojstva konstrukcionnyh ugleplastikov, izgotovlennyh propitkoj pod vakuumom [Properties constructional carbon plastics made by impregnation under vacuum] // Izvestiya Samarskogo nauchnogo centra RAN. 2012. T. 14. №4 (2). S. 762–766.
  9. Panina N.N., Kim M.A., Gurevich Ya.M. i dr. Svyazuyushhie dlya formovaniya izdelij iz polimernyh kompozicionnyh materialov [Binding for formation of products from polymeric composite materials] // Klei. Germetiki. Tehnologii. 2013. №10. S. 27–35.
  10. Pavlovskij K.A., Yamshhikova G.A., Gunyaeva A.G., Ulkin M.Yu. Razrabotka svyazuyushhego, ne podderzhivayushhego gorenie ugleplastika, dlya izgotovleniya tolstostennyh izdelij iz PKM metodom pressovogo formovaniya [Development of binding, not sustaining combustion of CFRP, for manufacturing of thick-walled products from polymeric composite materials by method of press formation] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №4. St. 08. Available at: http://www.viam-works.ru (accessed: July 21, 2016). DOI: 10.18577/2307-6046-2016-0-4-8-8.
  11. Kablov E.N. Himiya v aviacionnom materialovedenii [Chemistry in aviation materials science] // Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  12. Antyufeeva N.V., Komarova O.A., Pavlovskij K.A., Aleksashin V.M. Opyt primeneniya kalorimetricheskogo kontrolya reakcionnoj sposobnosti preprega KMU-11tr [Practice of the calorimetric control reactionary ability prepreg KMU-11tr] //Trudy VIAM. 2014. №2. St. 06. Available at: http://viam-works.ru (accessed: July, 24 2016). DOI: 10.18577/2307-6046-2014-0-2-6-6.
  13. Antyufeeva N.V., Aleksashin V.M., Zhelezina G.F., Stolyankov Yu.V. Metodicheskie podhody termoanaliticheskih issledovanij dlya ocenki svojstv prepregov i ugleplastikov [Methodical approaches of thermoanalytical researches for assessment of properties of prepregs and carbon plastics] // Vse materialy. Enciklopedicheskij spravochnik. 2012. №4. S. 18–27.
  14. Malysheva G.V., Ahmetova E.Sh., Shimina Yu.Yu. Ocenka temperatur fazovyh perehodov polimernyh svyazuyushhih metodom differencial'no-skaniruyushhej kalorimetrii [Assessment of temperatures of phase transitions polymeric binding method differential scanning calorimetry] // Klei. Germetiki. Tehnologii. 2014. №6. S. 29–33.
  15. Dushin M.I., Kogan D.I., Hrulkov A.V., Gusev Yu.A. Prichiny obrazovaniya poristosti v izdeliyah iz polimernyh kompozicionnyh materialov (obzor) [The reasons of formation of porosity in products from polymeric composite materials (review)] // Kompozity i nanostruktury. 2013. №3. S. 60–68.