Definition of the amount of water in honeycomb structures by the acoustic free vibration method
Abstract
The scope, ways of implementation of acoustic free vibration method, areas of its application and feature of control multilayer glued structures with honeycomb core are covered. Possibility of definition of amount of water in honeycomb structures is shown.
Keywords
glued structure, honeycomb core, water in honeycombs, non-destructive testing, acoustic methods, free vibration method.
Reference list
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] // Vse materialy. Enciklopedicheskij spravochnik. 2008. №3. S. 2–14.
- Petrova A.P., Lukina N.F. Klei dlya mnogorazovoj kosmicheskoj sistemy [Glues for reusable space system] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №4. St. 04. Available at: http://www.viam-works.ru (accessed: November 22, 2016).
- Kablov E.N. Kontrol kachestva materialov – garantiya bezopasnosti ekspluatacii aviacionnoj tehniki [Quality control of materials – security accreditation of operation of aviation engineering] // Aviacionnye materialy i tehnologii. M.: VIAM, 2001. Vyp.: Metody ispytanij i kontrolya kachestva metallicheskih i nemetallicheskih materialov. S. 3–8.
- Murashov V.V. Kontrol i diagnostika mnogoslojnyh konstrukcij iz polimernyh kompozicionnyh materialov akusticheskimi metodami [Control and diagnostics of multi-layer designs from polymeric composite materials acoustic methods]. M.: Spektr, 2016. 244 s.
- Murashov V.V. Ocenka stepeni nakopleniya mikropovrezhdenij struktury PKM v detalyah i konstrukciyah nerazrushayushhimi metodami [Assessment of accumulation degree of microdamages of PCM structure in structures determined by nondestructive methods] // Aviacionnye materialy i tehnologii. 2016. №3 (42). S. 73–81. DOI: 10.18577/2071-9140-2016-0-3-73-81.
- Murashov V.V., Rumyancev A.F. Diagnostika sostava i svojstv polimernyh kompozitov v detalyah i konstrukciyah [Diagnostics of structure and properties of polymeric composites in details and designs] // Kontrol. Diagnostika. 2008. №8. S. 13–17.
- Kablov E., Murashov V., Rumyantsev A. Diagnostics of Polymer Composites by Acoustic Methods // Ultragarsas. Kaunas: Tecnologija. 2006. No. 2. Р. 7–10.
- Karabutov A.A., Murashov V.V., Podymova N.B., Oraevsky A.A. Nondestructive Characterisation of Layered Composite Materials with a Laser Optoacoustic Sensor // Nondestructive Evaluation of Materials and Composites II (San Antonio, Texas, march–april 1998). San Antonio: Published by SPIE – The International Society for Optical Engineering. 1998. Vol. 3396. P. 103–111.
- Sposob opredeleniya fiziko-mehanicheskih harakteristik polimernyh kompozicionnyh materialov i ustrojstvo dlya ego osushhestvleniya: pat. 2214590 Ros. Federaciya. №2001135020/28 [Way of definition of physicomechanical characteristics of polymeric composite materials and the device for its implementation: pat. 2214590 Rus. Federation. №2001135020/28]; zayavl. 26.12.01; opubl. 20.10.03, Byul. №29.
- Sposob opredeleniya fiziko-mehanicheskih harakteristik i sostava polimernyh kompozicionnyh materialov v konstrukciyah ultrazvukovym metodom: pat. 2196982 Ros. Federaciya. №2001100302/28 [Way of definition of physicomechanical characteristics and composition of polymeric composite materials in designs ultrasonic method: pat. 2196982 Rus. Federation. №2001100302/28]; zayavl. 09.01.01; opubl. 20.01.03, Byul. №2.
- Murashov V.V. Kontrol kleenyh konstrukcij [Control of glued designs] // Klei. Germetiki. Tehnologii. 2005. №1. S. 21–27.
- Murashov V.V., Generalov A.S. Kontrol mnogoslojnyh kleenyh konstrukcij nizkochastotnymi akusticheskimi metodami [Control of multilayer adhesive structures operating in severe climatic condition] // Aviacionnye materialy i tehnologii. 2014. №2. S. 59–67. DOI: 10.18577/2071-9140-2014-0-2-59-67.
- Murashov V.V., Aleksashin V.M. Kontrol prochnosti zony soedineniya elementov integralnyh konstrukcij iz polimernyh kompozitov ultrazvukovym metodom [Control of durability of zone of connection of elements of integral designs from polymeric composites ultrasonic method] // Klei. Germetiki. Tehnologii. 2014. №7. S. 15–19.
- Murashov V.V. Opredelenie prochnostnyh harakteristik ugleplastikov v monolitnyh i integralnyh konstrukciyah lazerno-akusticheskim sposobom ultrazvukovogo kontrolya [Definition of strength characteristics carbon plastics in monolithic and integral designs in the laser and acoustic way of ultrasonic control] // Materialovedenie. 2016. №11. S. 9–16.
- Murashov V.V. Kontrol kachestva izdelij iz polimernyh kompozicionnyh materialov akusticheskimi metodami [Quality control of products from polymeric composite materials acoustic methods] // Kontrol. Diagnostika. 2016. №12. S. 16–29.
- Murashov V.V., Trifonova S.I. Kontrol kleevyh soedinenij v konstrukciyah i izdeliyah iz PKM ultrazvukovym tenevym metodom [Control of glued joints in designs and products from PKM ultrasonic shadow method] // Klei. Germetiki. Tehnologii. 2015. №5. S. 15–23.
- Murashov V.V. Control of Glued Structures Made of Dissimilar Materials by Ultrasound Reverberation // Polymer Science. Series D. 2016. Vol. 9. No. 3. P. 303–306.
- Murashov V.V. Kontrol mnogoslojnyh kleenyh konstrukcij akustiko-teplovym metodom [Control of multi-layer glued designs by acoustic-thermal method] // Klei. Germetiki. Tehnologii. 2014. №9. S. 36–40.
- Murashov V.V. Attestation of Glued Articles by Acoustic Impedance Method // Polymer Science. Series D: Glues and Sealing Materials. 2010. Vol. 3. No. 4. Р. 267–273.
- Murashov V.V. Vyyavlenie zon otsutstviya adgezionnogo soedineniya sloev v mnogoslojnyh konstrukciyah [Identification of zones of lack of adhesive connection of layers in multi-layer designs] // Klei. Germetiki. Tehnologii. 2013. №3. S. 29–31.
- Murashov V.V. Identification of Areas of Absence of Adhesive Bonding between Layers in Multilayer Structures // Polymer Science. Series D: Glues and Sealing Materials. 2014. Vol. 7. No. 1. Р. 46–48.
- Murashov V.V. Control of Multilayer Constructions by Spectral Acoustic-Impedance Defectoscopy // Polymer Science. Series D: Glues and Sealing Materials. 2014. Vol. 7. No. 2. Р. 133–135.
- Murashov V.V. Control of Glued Structures by the Electromagnetic Acoustic Variant of the Impedance Method // Ibid. Р. 136–139.
- Murashov V.V., Slyusarev M.V., Evdokimov A.A. Kontrol' kachestva obolochek arochnyh elementov nadzemnyh chastej opor bystrovozvodimyh mostovyh sooruzhenij iz PKM [Quality control of covers of arch elements of elevated parts of support of fast-erected bridge constructions from PСM] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №7. St. 10. Available at: http://www.viam-works.ru (accessed: November 22. 2016). DOI: 10.18577/2307-6046-2016-0-7-10-10.
- Murashov V.V., Slyusarev M.V. Vyyavlenie zon ponizhennoj prochnosti soedineniya obshivki s sotovym zapolnitelem v kleenyh sotovyh agregatah [Identification of zones of the lowered durability of connection of covering with cellular filler in glued cellular units] // Klei. Germetiki. Tehnologii. 2016. №12. S. 27–32.
- Murashov V.V. Control of Multilayer Glued Constructions of Polymeric Composite Materials // Polymer Science. Series D: Glues and Sealing Materials. 2012. Vol. 5. No. 2. Р. 109–115.
- Murashov V.V. Kontrol kleenyh konstrukcij akustiko-topograficheskim metodom [Control of kleeny designs acoustics topographical method] // Klei. Germetiki. Tehnologii. 2016. №3. S. 21–27.
- Murashov V.V. Control of Laminated Structures by the Acoustic Free Vibration Method // Polymer Science. Series D: Glues and Sealing Materials. 2012. Vol. 5. No. 4. Р. 341–345.
- Bakunov A.S., Murashov V.V., Sysoev A.M. Kontrol lopastej vozdushnogo vinta sredstvami nizkochastotnoj akustiki [Control of blades of air screw by means of low-frequency acoustics] // Kontrol. Diagnostika. 2012. №6. S. 72–74.
- Lange Yu.V. Akusticheskij spektralnyj metod nerazrushayushhego kontrolya [Acoustic spectral method of non-destructive testing] // Defektoskopiya. 1978. №3. S. 7–14.
- Murashov V.V., Toktueva V.N. Spektralnyj sostav impulsov udarnogo vozbuzhdeniya [Spectral content of impulses of shock excitation] // Aviacionnye materialy. M.: VIAM, 1979. Vyp. 6. S. 21–26.
- Nerazrushayushhij kontrol: spravochnik / pod obshh. red. V.V. Klyueva [Non-destructive testing: directory / gen. ed. by E.N. Kablov]. M.: Mashinostroenie, 2006. T. 3: Ultrazvukovoj kontrol / pod red. I.N. Ermolova, Yu.V. Lange. 864 s.
- Kosarina E.I., Stepanov A.V. Radiograficheskij kontrol sotovyh konstrukcij s celyu obnaruzheniya tehnologicheskih i ekspluatacionnyh defektov [Radiographic control of cellular designs for the purpose of detection of technological and operational defects] // V mire nerazrushayushhego kontrolya. 2003. №3. S. 2–5.
- Stepanov A.V. Metody kontrolya sotovyh konstrukcij aviacionnoj tehniki v usloviyah ekspluatacii [Control methods of cellular designs of aviation engineering under operating conditions] // Aviacionnye materialy i tehnologii. 2004. M.: VIAM. S. 81–86.
- Skuchik E. Prostye i slozhnye kolebatelnye sistemy [Simple and complex vibrating systems]. M.: Mir, 1971. 557 s.
- Lange Yu.V. Akusticheskie nizkochastotnye metody i sredstva nerazrushayushhego kontrolya mnogoslojnyh konstrukcij [Acoustic low-frequency methods and means of non-destructive testing of multi-layer designs]. M.: Mashinostroenie, 1991. 272 s.