Alifanov E.V., Chaykun A.М., Naumov I.S., Еliseev O.A. Elastomeric materials with high heat resistance (review) // Proceedings of VIAM. 2017. No. 2 (50). Ст. 06. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2017-0-2-6-6.

Elastomeric materials with high heat resistance (review)

Alifanov E.V., Chaykun A.М., Naumov I.S., Еliseev O.A.
Abstract

The main types of heat-resisting rubbers and fields of their application are described. Features of selection of elastomers for high-temperature sealants are shown. Thermal stability characteristics of rubbers of different types are given. Comparative characteristics of domestic heat-resistant rubbers of mass application are given. Information on the modern trends and developments in the field of creation of heat-resistant materials is provided.

Keywords
rubber, heat resistance.
Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the develop-ment of materials and technologies of their processing for the period until 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Khimiya v aviatsionnom materialovedenii [Chemistry in aviation materials science] // Rossiyskiy khimicheskiy zhurnal. 2010. T. LIV. №1. S. 3–4.
  3. Kablov E.N. Shestoy tekhnologicheskiy uklad [Sixth technological way] // Nauka i zhizn. 2010. №4. S. 2–7.
  4. Istorija aviacionnogo materialovedenija. VIAM – 80 let: gody i ljudi [History of aviation materials science. VIAM – 80 years: years and people] / pod obshh. red. E.N. Kablova. M.: VIAM, 2012. S. 346–348.
  5. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] // Vse materialy. Entsiklopedicheskiy spravochnik. 2008. №3. S. 2–14.
  6. Fedyukin D.P., Makhles F.A. Tekhnicheskie i tekhnologicheskie svoystva rezin [Engineering and technological properties of rubbers]. M.: Khimiya, 1985. 240 s.
  7. Alifanov E.V., Chaykun A.М., Venediktova M.A., Naumov I.S. Osobennosti receptur rezin na osnove etilenpropilenovyh kauchukov i ih primenenie v izdeliyah specialnogo naznacheniya (obzor) [Specialties of rubber compounds recipes based on ethylene-propylene rubbers and their application in the articles for special purpose (review)] //Aviacionnye materialy i tehnologii. 2015. №2 (35). S. 51–55. DOI: 10.18577/2071-9140-2015-0-2-51-55.
  8. Nudelman Z.N. Ftorkauchuki: osnovy, pererabotka, primenenie [Fluoroelastomers: bases, processing, application]. M.: RIAS, 2007. 383 s.
  9. Koshelev F.F., Kornev A.E., Bukanov A.M. Obshchaya tekhnologiya reziny [General technology of rubber]. M.: Khimiya, 1978. 527 s.
  10. Bolshoy spravochnik rezinshchika v 2 ch [The big reference book for specialist in rubbers in 2 p.]. M.: Tekhinform, 2012. 1385 s.
  11. Chernyavskiy G.G., Emelyanov G.A., Purtseladze V.I., Ugolkov V.L. Ftorpolimernye zashchitnye dezaktiviruemye pokrytiya na osnove nizkomolekulyarnykh funktsional'nykh sopolimerov vinilidenftorida [Ftorpolimernye protective deactivated coverings on the basis of low-molecular functional copolymers of vinylidene fluoride] // Kauchuk i rezina. 2015. №5. S.12–14.
  12. Chapurkin V.V., Medvedev V.P., Chapurkin S.V. Osobennosti strukturirovaniya ftorelastomerov ftorperoksidami [Features of structuring fluoroelastomers ftorperoksidami] // Kauchuk i rezina. 2015. №4. S. 36–37.
  13. Chaykun A.M., Naumov I.S., Eliseev O.A. Ftorsiloksanovye reziny: nekotorye aspekty primeneniya [Ftorsiloksanovye of rubber: some aspects of application] // Aviatsionnye materialy i tekhnologii. 2013. №2. S. 35–36.
  14. Sinteticheskiy kauchuk [Synthetic rubber] / pod red. I.V. Garmonova. L.: Khimiya, 1976. 752 s.
  15. Shveytser F.A. Korroziya plastmass i rezin [Corrosion of plastic and rubbers]. SPb.: Nauchnye osnovy i tekhnologii, 2010. 640 s.
  16. Chaykun A.M., Eliseev O.A., Naumov I.S., Venediktova M.A. Osobennosti postroeniya receptur dlya morozostojkih rezin [Compounding principles in the field of frost resistant rubbers] // Aviacionnye materialy i tehnologii. 2013. №3. S. 53–55.
  17. Eliseev O.A., Krasnov L.L., Zajceva E.I., Savenkova A.V. Razrabotka i modificirovanie elastomernyh materialov dlya primeneniya vo vseklimaticheskih usloviyah [Development and modifying of elastomeric materials for application in all weather conditions] // Aviacionnye materialy i tehnologii. 2012. №S. S. 309–314.
  18. Andrianov K.A., Grudinov I.T., Khananashvili L.M. Destruktsiya siloksanovykh elastomerov [Destruktsiya of siloxane elastomer] // Kauchuk i rezina. 1968. №11. S. 19.
  19. Kopylov V.M., Kovyazin V.A., Kostyleva E.I., Fedorov A.Yu., Kovyazin A.V. Termostabilizatsiya i keramoobrazovanie silikonovykh rezin [Thermostabilization and keramoobrazovaniye of silicone rubbers] // Kauchuk i rezina. 2015. №5. S. 52–57.
  20. Khoroshavina Yu.V., Frantsuzova Yu.V., Nikolaev G.A. Svoystva vulkanizatov na osnove polifenilsilseskvioksanpolidimetilsiloksanovogo blok-sopolimera [Properties of cured stocks on basis polyphenylsilsesquioxanepolydimethylsiloxane block copolymer ] // Kauchuk i rezina. 2015. №1. S. 10–11.
  21. Sposob polucheniya polifenilsilseskvioksanpolidiargonilsiloksanovykh blok-sopolimerov [Way of receiving polyphenylsilseskvioxanpolidiargonilsiloxane block copolymer]: pat. RU 2135529 C1; opubl. 23.08.98.
  22. Naumov I.S., Petrova A.P., Barbotko S.L., Eliseev O.A. Reziny s ponizhennoy goryuchestyu [Rubbers with the lowered combustibility] // Vse materialy. Entsiklopedicheskiy spravochnik. 2016. №4. S. 27–33.