Dermel I.V., Shashkeev K.A. Peculiarities of magnetron sputtering of metals in the presence of reactive gases // Proceedings of VIAM. 2017. No. 11 (59). Ст. 11. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2017-0-11-11-11.

Peculiarities of magnetron sputtering of metals in the presence of reactive gases

Dermel I.V., Shashkeev K.A.
Abstract

In this article, peculiarities of magnetron sputtering of metals and semiconductors in the presence of reactive gases are discussed. Aluminum, titanium, and silicon targets were used. Oxygen and atmospheric air dissolved in argon were used as reactive gases. An influence of oxygen and atmospheric fractions in the gas mixture on the discharge voltage and oxides’ deposition rate during sputtering was investigated.

Keywords
magnetron sputtering, reactive gases, metal, semiconductor, oxide, magnetron.
Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Konstrukcionnye i funkcionalnye materialy – osnova ekonomicheskogo i nauchno-tehnicheskogo razvitiya Rossii [Constructional and functional materials – basis of economic and scientific and technical development of Russia] // Voprosy materialovedeniya. 2006. №1. S. 64.
  3. Kablov E.N., Kondrashov S.V., Yurkov G.Y. Prospects of using carbonaceous nanoparticles in binders for polymer composites // Nanotechnologies in Russia. 2013. Vol. 8. No. 3–4. Р. 163–185.
  4. Khokhlov Yu.A., Bogatov V.A, Krynin A.G. Vliyanie raspredeleniya magnitnogo polya na svojstva ITO pokrytiya, poluchaemogo na polimernoj plenke metodom reaktivnogo magnetronnogo osazhdeniya [An influence of the magnetic field distribution on properties of ITO coating deposited on a polymer film by reactive magnetron sputtering method] // Trudy VIAM : electron. nauch.-tenhich. zhurn. 2014. №12. St. 11. Available at: http://viam-works.ru (accessed: October 09, 2017). DOI: 10.18577/2307-6046-2014-0-12-11-11.
  5. Bogatov V.A., Kondrashov S.V., Hohlov Yu.A. Mnogofunkcionalnye opticheskie pokrytiya i materialy [Multifunction optical coatings and materials] // Aviacionnye materialy i tehnologii. 2012. №S. S. 343–348.
  6. Krynin A.G., Hohlov Yu.A., Bogatov V.A., Kislyakov P.P. Prozrachnye interferencionnye pokrytiya dlya funkcionalnyh materialov ostekleniya [Transparent interferential coatings for functional materials of glazing] // Trudy VIAM : elektron. nauch.-tenhich. zhurn. 2013. №11. St. 05. Available at: http://viam-works.ru (accessed at: October 09, 2017).
  7. Bogatov V.A., Hohlov Yu.A. Mnogofunkcionalnye opticheskie pokrytiya, poluchaemye metodami plazmennoj tehnologii, i sposoby kontrolya ih optiko-fizicheskih harakteristik [The multifunction optical coatings received by methods of plasma technology, and ways of control of their optic and physical characteristics] // Aviacionnye materialy i tehnologii. 2001. №1. S. 93–99.
  8. Kelly P.J., Arnell R.D. Magnetron sputtering: a review of recent developments and application // Vacuum. 2000. Vol. 56. P. 159–172.
  9. Rossnagel S.M. Sputter Deposition // Opportunities for Innovation: Advanced Surface Engineering. Switzerland: Technomic Publishing Co., 1995. 186 с.
  10. Danilin B.S., Syrchin V.K. Magnetronnye raspylitelnye sistemy [Magnetronnye spraying systems]. M.: Radio i svyaz, 1982. 72 s.
  11. Bassett G.A. Continuous observation of the growth of vacuum evaporated metal films // Proceeding of the European Regional Conference on Electron Microscopy. 1960. Vol. 1. P. 270–275.
  12. Berlin E.V., Sejdman L.A. Poluchenie tonkih plenok reaktivnym magnetronnym napyleniem [Receiving thin films by reactive magnetron dusting]. M.: Tehnosfera, 2014. 256 s.
  13. Odynec L.L., Orlov V.M. Anodnye oksidnye plenki [Anode oxide films]. L.: Nauka, 1990. 200 s.
  14. Bollman W. The Experimental Foundations of Particle Physics // Physical review. 1956. Vol. 103. P. 1588–1594.
  15. Silicox J., Whelan M.J. Structure and Properties of Thin Films. John Willey and Sons, London. 1959. 183 p.
  16. Gusev E.P., Popov A.P. Nachalnaya stadiya okisleniya metallov v modeli reshetochnogo gaza [Initial stage of oxidation of metals in model of the lattice gas] // Poverhnost. 1991. №2. S. 33–46.
  17. Kubashevskij O.V., Gopkins B.A. Okislenie metallov i splavov [Oxidation of metals and alloys]. M.: Metallurgiya, 1968.
  18. S. 370–428.
  19. Kulikov I.S. Termodinamika oksidov [Thermodynamics of oxides]. M.: Metallurgiya, 1986. 358 s.