Volkova E.F., Akinina M.V., Mostyaev I.V. The ways of rising of wrought magnesium alloys main mechanical characteristics // Proceedings of VIAM. 2017. No. 10 (58). Ст. 02. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2017-0-10-2-2.

The ways of rising of wrought magnesium alloys main mechanical characteristics

Volkova E.F., Akinina M.V., Mostyaev I.V.
Abstract

The paper presents the investigation results of the influence of non-standard deformation technology with the using of superplastic deformation upon the microstructure, phase composition and properties of commercial MA14 alloy. It was suggested the solution of the problem connected with anisotropy of strengthening properties of MA14 alloy and increasing the material utilization coefficient using the technology of volumetric deformation under isothermal conditions. It was showed the effect of rising of alloy mechanical properties according to the changes in microstructure and in phase composition, that took place with alloying the basic Mg–Zn–Zr system alloy with RE elements.

Keywords
wrought magnesium alloys, technology, microstructure, phase composition, rare earth elements.
Reference list
  1. Mashinostroenie: enciklopediya v 40 t. [Mechanical engineering: the encyclopedia in 40 vol.] M.: Mashinostroenie, 2001. Tom II-3. Cvetnye metally i splavy. Kompozicionnye metallicheskie materialy / Volkova E.F., Fridlyander I.N., Senatorova O.G., Kablov E.N., Kolobnev N.I. S. 365–382.
  2. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  3. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] // Vse materialy. Enciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  4. Kornysheva I.S., Volkova E.F., Goncharenko E.S., Muhina I.Yu. Perspektivy primeneniya magnievyh i litejnyh alyuminievyh splavov [Perspectives of application of magnesium and cast aluminum alloys] // Aviacionnye materialy i tehnologii. 2012. №S. S. 212–222.
  5. Volkova E.F., Duyunova V.A. O sovremennyh tendenciyah razvitiya magnievyh splavov [About current trends of development of magnesium alloys] // Tehnologiya legkih splavov. 2016. №3. S. 94–105.
  6. Antipov V.V. Strategiya razvitiya titanovyh, magnievyh, berillievyh i alyuminievyh splavov [Strategy of development of titanium, magnesium, beryllium and aluminum alloys] // Aviacionnye materialy i tehnologii. 2012. №S. S. 157–167.
  7. Kablov E.N. Nauka kak otrasl ekonomiki [Science as economy industry] // Nauka i zhizn. 2009. №10. S. 7–8.
  8. Volkova E.F., Duyunova V.A. Effekt primeneniya nestandartnoj tehnologii deformacii k nekotorym serijnym magnievym splavam [Effect of unconventional deformation technology applicable to some commercial magnesium–based alloys] // Aviacionnye materialy i tehnologii. 2016. №3. S. 17–23. DOI: 10.18577/2071-9140-2016-03-17-23.
  9. Lashko N.F., Zaslavskaya L.V., Kozlova M.N. i dr. Fiziko-himicheskij fazovyj analiz stalej i splavov [Physical and chemical phase analysis staly and alloys]. M.: Metallurgiya, 1978. 336 s.
  10. Volkova E.F., Antipov V.V., Morozova G.I. Osobennosti formirovaniya struktury i fazovogo sostava deformirovannyh polufabrikatov iz serijnogo splava MA14 // Aviacionnye materialy i tehnologii. 2011. №3. S. 8–15.
  11. Volkova E.F., Ishodzhanova I.V., Tarasenko L.V. Strukturnye izmeneniya v magnievom splave MA14 pod vozdejstviem tehnologicheskih faktorov [Structural changes in MA14 magnesium alloy under the influence of technology factors] // Metallovedenie i termicheskaya obrabotka metallov. 2010. №12. S. 19–23.
  12. Volkova E.F., Moiseev N.V., Akinina M.V. Razvitie effekta sverhplastichnosti v serijnyh splavah sistem Mg–Al–Zn–Mn i Mg–Zn–Zr [Development of effect of superplasticity in serial alloys of Mg-Al-Zn-Mn and Mg-Zn-Zr systems] // Tehnologiya legkih splavov. 2014. №4. S. 52–57.
  13. Emli E.F. Osnovy tehnologii proizvodstva i obrabotki magnievyh splavov [Bases of the production technology and processing of magnesium alloys]. M.: Metallurgiya, 1972. 488 s.
  14. Kajbyshev R.O., Galiev A.M. Ispolzovanie yavleniya sverhplastichnosti dlya sozdaniya tehnologii izgotovleniya izdelij iz magnievyh splavov [Use of the phenomenon of superplasticity for creation of manufacturing techniques of products from magnesium alloys] // Metallovedenie i termicheskaya obrabotka metallov. 2006. №11. S. 23–25.
  15. Volkova E.F., Rohlin L.L., Becofen S.Ya., Akinina M.V. Issledovanie vliyaniya RZE ittrievoj i cerievoj podgrupp na svojstva magnievyh splavov [Research of influence of REE of yttric and ceric subgroups on properties of magnesium alloys] // Tehnologiya legkih splavov. 2014. №2. S. 42–48.
  16. Kablov E.N., Volkova E.F., Filonova E.V. Issledovanie vliyaniya RZE na fazovyj sostav i svojstva novogo zharoprochnogo magnievogo splava sistemy Mg–Zn–Zr–RZE [Research of influence of REE on phase structure and properties of new heat resisting magnesium alloy of Mg–Zn–Zr–REE system] // Metallovedenie i termicheskaya obrabotka metallov. 2017. №7. S. 19–26.