Popova S.V., Dobrynin D.A., Muboyadzhyan S.A., Budinovskiy S.A. Removal of heat resisting condensation and diffusion coatings from the surface of GTE blades before and after the operating time // Proceedings of VIAM. 2017. No. 1 (49). Ст. 04. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2017-0-1-4-4.

Removal of heat resisting condensation and diffusion coatings from the surface of GTE blades before and after the operating time

Popova S.V., Dobrynin D.A., Muboyadzhyan S.A., Budinovskiy S.A.
Abstract

The significant part of the blade repair technology is removing used coatings from the surface of complex geometry blade. A method has been developed for removal of heat resisting condensation and diffusion coatings in electrolytic plasma by directional jet of electrolyte. This method allows uniform layer-by-layer removing heat resistant coatings from heat-resistant nickel alloys. The peculiarity of the process is a universality of usable electrolytes not requiring component correction in dependence on heat-resistant coating and alloy composition. The work is executed within the implementation of the complex scientific direction 10.11. «Power-efficient, resource-saving progressive technologies of machining of metal and non-metallic materials» («The strategic directions of development of materials and technologies of their processing for the period till 2030»)

Keywords
electrolytic-plasma treating, stripping, heat-resistant coating, blade, heat-resistant nickel alloy, condensation-diffusion coating, surface.
Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N., Orlov M.R., Ospennikova O.G. Mehanizmy obrazovaniya poristosti v monokristallicheskih lopatkah turbiny i kinetika ee ustraneniya pri goryachem izostaticheskom pressovanii [Mechanisms of formation of porosity in single crystals turbine blades and kinetics of its elimination at hot isostatic pressing ] // Aviacionnye materialy i tehnologii. 2012. №S. S. 117–129.
  3. Svetlov I.L., Khvatskiy K.K., Gorbovets M.A., Belyaev M.S. Vliyanie goryachego izostaticheskogo pressovaniya na mehanicheskie svojstva litejnyh nikelevyh zharoprochnyh splavov [An effect of Hot Isostatic Pressing (HIP) on mechanical properties of casting Ni-based superalloys] // Aviacionnye materialy i tehnologii. 2015. №3 (36). S. 10–14. DOI: 10.18577/2071-9140-2015-0-3-10-14.
  4. Bybin A.A., Nevyanceva R.R., Smol'nikova O.G. Zakonomernosti udaleniya vneshnej i vnutrennej zon zharostojkogo alyuminidnogo pokrytiya s dlitelnoj narabotkoj pri remonte lopatok TVD [Patterns of removal of external and internal zones of heat resisting alyuminide covering with long operating time at repair of blades of TVD] // Vestnik UGATU. 2008. T. 10. №1 (26). S. 127–130.
  5. Lesnikov V.P., Kuznecov V.P., Korotkih A.V. Tehnologiya vosstanovitelnogo remonta turbinnyh lopatok GTD [Technology of restoring repair of turbine blades of GTD] // Aviacionno-kosmicheskaya tehnika i tehnologiya. 2004. №7 (15). S. 236–239.
  6. Kablov E.N., Muboyadzhyan S.A. Zharostojkie i teplozashhitnye pokrytiya dlya lopatok turbiny vysokogo davleniya perspektivnyh GTD [Heat resisting and heat-protective coverings for turbine blades of high pressure of perspective GTE] // Aviacionnye materialy i tehnologii. 2012. №S. S. 60–70.
  7. Kablov E.N., Muboyadzhyan S.A., Budinovskij S.A., Lucenko A.N. Ionno-plazmennye zashhitnye pokrytiya dlya lopatok gazoturbinnyh dvigatelej [Ion-plasma protecting covers for blades of gas turbine engines] // Metally. 2007. №5. S. 23–34.
  8. Muboyadzhyan S.A., Budinovskij S.A., Gayamov A.M., Smirnov A.A. Poluchenie keramicheskih teplozashhitnyh pokrytij dlya rabochih lopatok turbin aviacionnyh GTD magnetronnym metodom [Receiving ceramic heat-protective coatings for working blades of turbines of aviation GTD magnetronny method] // Aviacionnye materialy i tehnologii. 2012. №4. S. 3–8.
  9. Popova S.V., Muboyadzhyan S.A., Budinovskij S.A. Elektrolitno-plazmennaya finishnaya obrabotka metallov i splavov [Electrolyte-plasma finishing processing of metals and alloys] // Pisma o materialah. 2015. T. 5. №1. S. 39–42.
  10. Budinovskij S.A., Muboyadzhyan S.A., Gayamov A.M., Kosmin A.A. Udalenie zharostojkih pokrytij s poverhnosti pera lopatok turbin v vodnyh malokoncentrirovannyh rastvorah [Removal of heat resisting coverings from surface of feather of blades of turbines in the aqueous low-concentrated solutions] // Tehnologiya metallov. 2006. №11. S. 15–24.
  11. Kulikov I.S. i dr. Elektrolitno-plazmennaya obrabotka materialov [Electrolyte-plasma processing of materials]. Minsk: Belarus. Navuka, 2010. 232 s.
  12. Galoyan A.G., Muboyadzhyan S.A., Kashin D.S. Formirovanie termodiffuzionnyh barernyh sloev na poverhnosti bezuglerodistyh zharoprochnyh renij- i renij-rutenijsoderzhashhih splavov metodom gazovoj cementacii [Termodiffusion barrier formation under vacuum cementation process on rhenium and rhenium-ruthenium comprising nickel based superalloys] //Aviacionnye materialy i tehnologii. 2015. №3 (36). S. 38–43. DOI: 10.18577/2071-9140-2015-0-3-27-37.
  13. Matveev P.V., Budinovskij S.A., Chubarov D.A. Tehnologiya polucheniya ionno-plazmennyh zharostojkih podsloev s povyshennym soderzhaniem alyuminiya dlya perspektivnyh TZP [Technology for production of ion-plasma heat-resistant bonding sub-layers with increased aluminum content for advanced TBCs] // Aviacionnye materialy i tehnologii. 2014. №S5. S. 56–60. DOI: 10.18577/2071-9140-2014-0-s5-56-60.
  14. Lazarenko B.R., Duradzhi V.N., Bryancev I.V. O strukture i soprotivlenii prielektrodnoj zony pri nagreve metallov v elektrolitnoj plazme [About structure and resistance of near electrode zone when heating metals in electrolyte plasma] // Elektronnaya obrabotka materialov. 1980. №2. S. 50–55.
  15. Pogrebnyak A.D., Kulmeneva O.P. i dr. Processy massoperenosa i legirovaniya pri elektrolitno-plazmennoj obrabotke chuguna [Processes the transfer of mass and alloying at electrolyte-plasma processing of cast iron] // Pisma v ZhTF. 2003. T. 29. Vyp. 8. S. 8.