Ryabov D.K., Morozova L.V., Korolev V.A., Ivanova A.O. Alternation of mechanical features of alloy AK9ch manufactured by selective laser melting // Proceedings of VIAM. 2016. No. 9 (45). Ст. 02. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2016-0-9-2-2.

Alternation of mechanical features of alloy AK9ch manufactured by selective laser melting

Ryabov D.K., Morozova L.V., Korolev V.A., Ivanova A.O.
Abstract

Treatment of materials using selective laser melting technology allows obtaining different products from a wide range of metallic materials. Aluminum powders allow also manufacturing construction elements. Achieving required strength of many aluminum alloys depends on applied heat treatment. The article presents investigation results of heat treatment parameters influence on tensile strength characteristics as well as the results of fractographic research. The work is carried out under the realization of integrated research area 10.3. «Technologies of atomization for producing high quality metallic powders for additive manufacturing and powders for brazing» («The strategic directions of development of materials and technologies for their processing for the period till 2030»)

Keywords
AK9ch alloy, SLM, heat treatment, additive manufacturing, strength.
Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  3. Kablov E.N. Rossii nuzhny materialy novogo pokoleniya [Materials of new generation are necessary to Russia ] // Redkie zemli. 2014. №3. S. 8–13.
  4. Sercombe T., Schaffer G. Rapid manufacturing of aluminum components // Science. 2003. Vol. 301 (5637). P. 1225–1227.
  5. Bremen S., Meiners W., Diatlov A. Selective Laser Melting // Laser Technik Journal. 2012. No. 9 (2). P. 33–38.
  6. Vilaro T., Colin C., Bartout J.D. et al. Microstructural and mechanical approaches of the selective laser melting process applied to a nickel-base superalloy // Materials Science and Engineering Structural Materials Properties Microstructure and Processing. 2012. Vol. 534. P. 446–451.
  7. Guan K., Wang Z. M., Gao M. et al. Effects of processing parameters on tensile properties of selective laser melted 304 stainless steel // Materials & Design. 2013. Vol. 50. P. 581–586.
  8. Wang Z.M., Guan K., Gao M. et al. The microstructure and mechanical properties of deposited-IN718 by selective laser melting // Journal of Alloys and Compounds. 2012. Vol. 513. P. 518–523.
  9. Vrancken B., Thijs L., Kruth J.P. et al. Heat treatment of Ti6Al4V produced by Selective Laser Melting: Microstructure and mechanical properties // Journal of Alloys and Compounds. 2012. Vol. 541. P. 177–185.
  10. Evgenov A.G., Rogalev A.M., Nerush S.V., Mazalov I.S. Issledovanie svojstv splava E'P648, poluchennogo metodom selektivnogo lazernogo splavleniya metallicheskikh poroshkov // Trudy VIAM: e'lektron. nauch.-tekhnich. zhurn. 2015. №2. St. 02. URL: http://www.viam-works.ru (data obrashheniya: 19.07.2016). DOI:10.18557/2307-6046-2015-0-2-2-2.
  11. Kablov E.N., Startsev O.V. Fundamentalnye i prikladnye issledovanija korrozii i starenija materialov v klimaticheskih uslovijah (obzor) [The basic and applied research in the field of corrosion and ageing of materials in natural environments (review)] //Aviacionnye materialy i tehnologii. 2015. №4. S. 38–52. DOI: 10.18577/2071-9140-2015-0-4-38-52.
  12. Ryabov D.K., Kolobnev N.I. Izmenenie mehanicheskih svojstv splava 1913 pri dvuhstupenchatom iskusstvennom starenii [Change of mechanical properties of alloy 1913 at two-level artificial aging] // Aviacionnye materialy i tehnologii. 2013. №4. S. 3–7.
  13. Kolobnev N.I., Ber L.B., KHokhlatova L.B., Ryabov D.K. Struktura, svojstva i primenenie splavov sistemy Al–Mg–Si–(Cu) [Structure, properties and application of alloys of Al-Mg-Si-(Cu) system] // Metallovedenie i termicheskaya obrabotka metallov. 2011. №9. S. 40–45.
  14. Antipov V.V. Strategiya razvitiya titanovyh, magnievyh, berillievyh i alyuminievyh splavov [Strategy of development of titanium, magnesium, beryllium and aluminum alloys] //Aviacionnye materialy i tehnologii. 2012. №S. S. 157–167.
  15. Illarionov E.I., Kolobnev N.I., Gorbunov P.Z., Kablov E.N. Alyuminievye splavy v aviakosmicheskoj tekhnike [Aluminum alloys in aerospace equipment]. M.: Nauka, 2001. 192 s.
  16. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] // Vse materialy. Enciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  17. Kempen K., Thijs L., Van Humbeeck J., Kruth J.P. Mechanical Properties of AlSi10Mg Produced by Selective Laser Melting // Phys. Procedia. 2012. Vol. 39. P 439–446.
  18. Olakanmi E.O. Selective laser sintering/melting (SLS/SLM) of pure Al, Al–Mg, and Al–Si powders: Effect of processing conditions and powder properties // J. Mater. Process. Tech. 2013. Vol. 213. P. 1387–1405.
  19. Brandl E., Heckenberger U., Holzinger V. et al. Additive manufactured AlSi10Mg samples using Selective Laser Melting (SLM): Microstructure, high cycle fatigue, and fracture behavior // Materials & Design. Vol. 34. P. 159–169.
  20. Kablov E.N. Shestoj tekhnologicheskij uklad [Sixth technological way] // Nauka i zhizn. 2010. №4. S. 2–7.