Abstract

The methods and techniques of machining technology for polymer composite materials (PCM) are considered. The features of PCM processing, tool selection, modes and methods of PCM processing as well as problems arising in the manufacture of the holes in the PCM structures are described. The major objectives of composites implementation in developing aircraft constructions currently are: – development and implementation of new materials and processes aimed at reducing technological cycles in structures manufacturing, quality improvement by improving the PCM processing technology, increasing tools life for machining technology and cutting modes, implementing universal methods of non-destructive quality control of the finished product; – reducing prices for feedstock and technology; – minimizing the harmful effects on nature, development of green technologies, reducing processing temperature, time of manufacture, development of technologies to exclude further processing in assembly oper

Keywords
polymer composite materials, mechanical processing, technological processes, processing of details, operational reliability.
Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Sovremennye materialy – osnova innovatsionnoy modernizatsii Rossii [Modern materials – basis of innovative modernization of Russia] // Metally Evrazii. 2012. №3. S. 10–15.
  3. Zhelezina G.F. Konstrukcionnye i funkcionalnye organoplastiki novogo pokoleniya [Constructional and functional organoplastics of new generation] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №4. St. 06. Available at: http://www.viam-works.ru (accessed: February 01, 2016).
  4. Kablov E.N. Materialy i tekhnologii VIAM dlya «Aviadvigatelya» [Materials and VIAM technologies for «Aircraft engine»] // Permskie aviatsionnye dvigateli: inform. byul. 2014. №S. S. 43–47.
  5. Kablov E.N. O nastoyashchem i budushchem VIAM i otechestvennogo materialovedeniya: intervyu [About the real and future VIAM and domestic materials science: interview] // Rossiyskaya akademiya nauk. 2015. 19 yanvarya.
  6. Kablov E.N. Kompozity: segodnya i zavtra [Composites: today and tomorrow] // Metally Evrazii. 2015. №1. S. 36–39.
  7. Kablov E.N. Materialy i khimicheskie tekhnologii dlya aviatsionnoy tekhniki [Materials and chemical technologies for aviation engineering] // Vestnik Rossiyskoy akademii nauk. 2012. T. 82. №6. S. 520–530.
  8. Kogan D.I., Chursova L.V., Petrova A.P. Tekhnologiya izgotovleniya PKM sposobom propitki plenochnym svyazuyushchim [PCM manufacturing techniques in the way of impregnation by the film binding] // Klei. Germetiki. Tekhnologii. №6. 2011. S. 25–29.
  9. Kogan D.I., Chursova L.V., Petrova A.P. Polimernye kompozitsionnye materialy, poluchennye putem propitki plenochnym svyazuyushchim [The polymeric composite materials received by impregnation by the film binding] // Vse materialy. Entsiklopedicheskiy spravochnik. 2011. №11. S. 2–6.
  10. Chursova L.V., Dushin M.I., Khrulkov A.V., Mukhametov R.R. Osobennosti tekhnologii izgotovleniya detaley iz kompozitsionnykh materialov metodom propitki pod davleniem [Features of manufacturing techniques of details from composite materials impregnation method under pressure] // Kompozitsionnye materialy v aviakosmicheskom materialovedenii: sb. tez. dokl. mezhotraslevoy nauch.-tekhnich. konf. M.: VIAM, 2009. S. 17.
  11. Hrulkov A.V., Dushin M.I., Popov Yu.O., Kogan D.I. Issledovaniya i razrabotka avtoklavnyh i bezavtoklavnyh tehnologij formovaniya PKM [Researches and development autoclave and out-of-autoclave technologies of formation of PCM] //Aviacionnye materialy i tehnologii. 2012. №S. S. 292–301.
  12. Timoshkov P.N., Kogan D.I. Sovremennye tehnologii proizvodstva polimernyh kompozicionnyh materialov novogo pokoleniya [Modern production technologies of polymeric composite materials of new generation] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №4. St. 07. Available at: http://www.viam-works.ru (accessed: February 01, 2016).
  13. Muhametov R.R., Ahmadieva K.R., Kim M.A., Babin A.N. Rasplavnye svyazujushhie dlya perspektivnyh metodov izgotovleniya PKM novogo pokoleniya [Melt binding for perspective methods of production of PCM of new generation] // Aviacionnye materialy i tehnologii. 2012. №S. S. 260–265.
  14. Muhametov R.R., Ahmadieva K.R., Chursova L.V., Kogan D.I. Novye polimernye svyazujushhie dlya perspektivnyh metodov izgotovleniya konstrukcionnyh voloknistyh PKM [New polymeric binding for perspective methods of manufacturing of constructional fibrous PCM] // Aviacionnye materialy i tehnologii. 2011. №2. S. 38–42.
  15. Babin A. N. Svyazujushhie dlya polimernyh kompozicionnyh materialov novogo pokoleniya [Binding for polymeric composite materials of new generation] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №4. St. 11. Available at: http://www.viam-works.ru (accessed: February 01, 2016).
  16. Grashhenkov D.V., Chursova L.V. Strategiya razvitiya kompozicionnyh i funkcionalnyh materialov [Strategy of development of composite and functional materials] // Aviacionnye materialy i tehnologii. 2012. №S. S. 231–242.