Babin A.N., Guseva M.A. The use of rheological methods for study of the solubility of components in polymeric binder // Proceedings of VIAM. 2016. No. 6 (42). Ст. 05. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2016-0-6-5-5.

The use of rheological methods for study of the solubility of components in polymeric binder

Babin A.N., Guseva M.A.
Abstract

In this work a compatibility of the components of polymer composition «polysulfone–epoxy oligomer» has been studied by rheological method. The processes and factors influencing the solubility of polysulfone in epoxides of different molecular structure have been established. Samples have been studied both in rotation and oscillation conditions. Work is executed within implementation of the complex scientific direction 13.1. «Binding for polymeric and composite materials of structural and special purposes» («The strategic directions of development of materials and technologies of their processing for the period till 2030»)

Keywords
rheology of polymeric binder, rotational viscometry, polysulfone, epoxy olygomers.
Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Babin A.N., Petrova A.P. Metody ispytanij i issledovanij osnovnyh svojstv polimernyh svyazuyushhih dlya konstrukcionnyh PKM [Test methods and researches of the main properties polymeric binding for constructional PСM] // Vse materialy. Kommentarii k standartam, TU, sertifikatam. 2016. №3. S. 2.
  3. Kablov E.N. Rossii nuzhny materialy novogo pokoleniya [Materials of new generation are necessary to Russia] // Redkie zemli. 2014. №3. S. 813.
  4. Kablov E.N. Tendencii i orientiry innovacionnogo razvitiya Rossii. 3-e izd. [Tendencies and reference points of innovative development of Russia. 3rd ed.]. M.: VIAM, 2015. 720 s.
  5. Petrovа A.P., Dementyevа L.A., Lukina N.F., Chursova L.V. [Adhesive binders for polymer composite materials based on carbon- and glass fillers] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №9. St. 11. Available at: http://www.viam-works.ru (accessed: November 02, 2015). DOI: 10.18577/2307-6046-2015-0-9-11-11.
  6. Alentev A.Yu., Yablokova M.Yu. Svyazuyushhie dlya polimernyh kompozicionnyh materialov: ucheb. posobie [Binding for polymeric composite materials: studies. grant.]. M.: Izd-vo MGU im. M.V. Lomonosova, 2010. 69 s.
  7. Kablov E.N., Bejder E.Ya., Petrova G.N., Stolyankov Yu.V., Rumyanceva T.V. Penopoliimidy // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №4. St. 09. Available at: http://www.viam-works.ru (accessed: November 02, 2015). DOI: 10.18577/2307-6046-2015-0-4-9-9.
  8. Yakovlev N.O. Issledovanie i opisanie relaksacionnogo povedeniya polimernyh materialov (obzor) [Study and description of relaxation behavior of polymers (review)] // Aviacionnye materialy i tehnologii. 2014. №S4. S. 50–54.
  9. Muranov A.N., Malysheva G.V., Nelyub V.A. i dr. Issledovanie svojstv polimernyh kompozicionnyh materialov na osnove geterogennoj matricy [Research of properties of polymeric composite materials on the basis of heterogeneous matrix] // Vse materialy. Enciklopedicheskij spravochnik. 2012. №4. S. 2–6.
  10. Guseva M.A. Cianovye efiry – perspektivnye termoreaktivnye svyazujushhie (obzor) [Cyanic esters are prospective thermosetting binders (review)] // Aviacionnye materialy i tehnologii. 2015. №2 (35). S. 45–50.
  11. Merkulova Yu.I., Muhametov R.R. Nizkovyazkoe epoksidnoe svyazuyushhee dlya pererabotki metodom vakuumnoj infuzii [Development of a low-viscosity epoxy binder for processing by vacuum infusion] // Aviacionnye materialy i tehnologii. 2014. №1. S. 39–41.
  12. Bejder E.Ya., Petrova G.N. Termoplastichnye svyazuyushhie dlya polimernyh kompozicionnyh materialov [The thermoplastic binder for polymeric composite materials] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №11. St. 05. Available at: http://viam-works.ru. (accessed: December 07, 2015). DOI: 10.18577/2307-6046-2015-0-11-5-5.
  13. Gryaznov V.I., Petrova G.N., Yurkov G.Yu., Buznik V.M. Smesevye termojelastoplasty so specialnymi svojstvami [Thermoplastic mixtures with special properties] // Aviacionnye materialy i tehnologii. 2014. №1. S. 25–29.
  14. Brantseva T.V., Gorbatkina Yu.A., Dutschek V., Kerber M.L. et al. Modification of epoxy resin by polysulfone to improve the interfacial and mechanical properties in glass fibre composites. I. Study of processes during matrix/glass fibre interface formation // J. Adhesion Sci. Technol. 2003. V. 17. №15. P. 2047–2063.
  15. Mezhikovskij S.M., Arinshtejn A.E., Deberdeev R.Ya. Oligomernoe sostoyanie veshhestva [Oligomerous condition of substance]. M.: Nauka, 2005. 252 s.
  16. Novakov I.A., Sidorenko N.V., Vaniev M.A. i dr. Fazovaya stabil'nost' i reologicheskie harakteristiki sistem termoplast–polimerizacionnosposobnoe soedinenie v usloviyah prilozheniya mehanicheskogo polya [Phase stability and rheological characteristics of systems thermoplastic – capable connection to polymerization in the conditions of the appendix of mechanical field] // Vestnik Bashkirskogo universiteta. 2008. T.13. №4. S. 911–915.