Semenychev V.V., Smirnova T.B. The evaluation of corrosion resistance of protective and functional coatings using corrosion-ratemeter // Proceedings of VIAM. 2016. No. 6 (42). Ст. 12. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2016-0-6-12-12.

The evaluation of corrosion resistance of protective and functional coatings using corrosion-ratemeter

Semenychev V.V., Smirnova T.B.
Abstract

Using device R5035 the corrosion rate, expressed as current units (A/sm2), of different protective and functional coatings, deposited on steel 12H18N9T was assessed. Samples with galvanic nickel, nickel-cobalt, tin and zinc coatings were investigated. Measurements of polarization resistance were carried out in a 3% aqueous solution of NaCl with the addition of 1 ml of HCl per 100 ml of solution. Polarization resistance of pairs of samples with similar coatings was defined for forward and reverse polarization current, amounting to 800 Ω for nickel, 700 Ω for nickel-cobalt, 96 Ω for tin, 6 Ω for zinc and550 Ω for steel without coating. From the values of polarization resistance the corrosion rate of coatings in the current units was calculated and the comparison of obtained values with the sample mass loss per surface unit was given. Using «Olympus» microscope the depth of the pits formed on the surface of coatings was assessed. Work is executed within implementation of the comp

Keywords
corrosion rate, polarization resistance, protective and functional coatings, depth of pits, nano particles.
Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Dospehi dlya «Burana». Materialy i tehnologii VIAM dlya MKS «Energiya–Buran» / pod obshh. red. E.N. Kablova [Armor for «Buran». VIAM’s materials and technologies for ISS of «Energiya-Buran» / gen. ed. by E.N. Kablov]. M.: Nauka i zhizn, 2013. S. 10–27.
  3. Kablov E.N. Himiya v aviacionnom materialovedenii [Chemistry in aviation materials science] // Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  4. Dolmatov V.Yu., Fudzhimura T., Burkat G.K., Orlova E.A. Poluchenie iznosostojkih hromovyh pokrytij s primeneniem nanoalmazov razlichnoj prirody [Receiving anti wear chrome platings using nanodiamonds of the different nature] // Sverhtverdye materialy. 2002. №6. S. 16–21.
  5. Vinokurov E.G., Arsenkin A.M., Grigorovich K.V., Bondar V.V. Elektroosazhdenie modificirovannyh dispersnymi chasticami hromovyh pokrytij i ih fiziko-mehanicheskie svojstva [Electrosedimentation of the chrome platings modified by dispersion particles and their physicomechanical properties] // Zashhita metallov. 2006. T. 42. №3. S. 312–316.
  6. Tyurikov E.V. Svojstva hromovyh pokrytij, poluchennyh v jelektrolitah, soderzhashhih nanoporoshok oksida alyuminiya [Properties of the chrome platings received in electrolits, containing aluminum oxide nanopowder] // Korroziya: materialy, zashhita. 2007. №11. S. 33–37.
  7. Muboyadzhyan S.A., Budinovskij S.A., Gayamov A.M., Matveev P.V. Vysokotemperaturnye zharostojkie pokrytiya i zharostojkie sloi dlya teplozashhitnyh pokrytij [High-temperature heat resisting coverings and heat resisting layers for heat-protective coverings] // Aviacionnye materialy i tehnologii. 2013. №1. S. 17–20.
  8. Azarovskij E.N., Muboyadzhyan S.A. Modificirovanie poverhnosti detalej iz konstrukcionnyh stalej v vakuumno-dugovoj plazme titana [Modifying of surface of details from constructional staly in vacuum and arc plasma of titanium] // Aviacionnye materialy i tehnologii. 2013. №3. S. 20–25.
  9. Shapnik M.S. Galvanicheskie pokrytiya splavami [Galvanic coverings alloys] // Sorosovskij obrazovatelnyj zhurnal. 2001. Tom 7. №6. S. 42–47.
  10. Nagaeva L.V., Nagaev V.V., Semenychev V.V. Galvanicheskie pokrytiya na osnove cinka, poluchennye iz elektrolitov, soderzhashhih soli nikelya ili kobalta i nanoporoshki oksidov i karbidov [Galvanic coverings on the basis of the zinc, received from the electrolits containing salts of nickel or cobalt and nanopowders of oxides and carbides] // Aviacionnye materialy i tehnologii. 2009. №1. S. 3–6.
  11. Spiridonov B.A., Falicheva A.I., Shalimov Yu.N. Elektroosazhdenie splava hrom-kobalt v sernokislom jelektrolite [Alloy electrosedimentation chrome-cobalt in sulphuric acid electrolit] // Zashhita metallov. 1982. T. 18. №5. S. 782–784.
  12. Spiridonov B.A. Elektroosazhdenie pokrytij splavom hrom-kobalt iz sulfatnyh rastvorov [Electrosedimentation of coverings by alloy chrome-cobalt from sulphatic solutions] // Zashhita metallov. 2005. T. 41. №3. S. 273–277.
  13. Shluger M.A., Pozdeeva Yu.V., Tok L.D. Zashhitnye svojstva elektroliticheskih hromomolibdenovyh pokrytij [Protective properties of electrolytic chrome molybdenum coverings] // Zashhita metallov. 1981. T. 22. №4. S. 468–470.
  14. Nagaeva L.V. Primenenie nanoporoshkov v elektrolitah nikelirovaniya kak sposob polucheniya nikelevyh pokrytij, po svojstvam ne ustupayushhim hromovym pokrytiyam [Application of nanopowders in nickel plating electrolits as way of receiving nickel coverings, on properties to not conceding chrome platings] // Korroziya: materialy, zashhita. 2007. №9. S. 32–36.
  15. Salahova R.K., Semenychev V.V., Tyurikov E.V., Tihoobrazov A.B. Issledovanie vnutrennih (ostatochnyh) napryazhenij v kompozicionno-klasternyh hromovyh i nikelevyh pokrytiyah [Investigation of internal (residual) stresses in composite-cluster chrome and nickel coatings] // Aviacionnye materialy i tehnologii. 2014. №S3. S. 42–46.
  16. Semenychev V.V., Nagaev V.V. Gal'vanicheskie pokrytiya na osnove cinka, poluchennye iz elektrolitov, soderzhashhih soli nikelya ili kobalta i nanoporoshki oksidov i karbidov [Galvanic coverings on the basis of the zinc, received from the electrolits containing salts of nickel or cobalt and nanopowders of oxides and carbides] // Izvestiya Samarskogo nauchnogo centra RAN. Specializirovannyj vypusk. 2008. T. 1. S. 29–32.
  17. Semenychev V.V., Salahova R.K., Tyurikov E.V., Ilin V.A. Zashhitnye i funkcionalnye galvanicheskie pokrytiya, poluchaemye s primeneniem nanorazmernyh chastic [The protective and functional galvanic coverings received using nanodimensional particles] // Aviacionnye materialy i tehnologii. 2012. №S. S. 335–342.
  18. Kablov E.N., Starcev O.V., Medvedev I.M., Panin S.V. Korrozionnaya agressivnost' primorskoj atmosfery. Ch. 1. Faktory vliyaniya (obzor) [Corrosion aggression of the seaside atmosphere. P.1. Factors of influence (overview)] // Korroziya: materialy, zashhita. 2013. №12. S. 6–18.
  19. Kablov E.N., Startsev O.V., Medvedev I.M. Obzor zarubezhnogo opyta issledovanij korrozii i sredstv zashhity ot korrozii [Review of international experience on corrosion and corrosion protection] //Aviacionnye materialy i tehnologii. 2015. №2 (35). S. 76–87.
  20. Semenychev V.V., Salahova R.K., Smirnova T.B. Ocenka tokov korrozii razlichnyh par materialov metodom pryamogo izmereniya [Assessment of currents of corrosion of different couples of materials method of direct measurement] // Praktika protivokorrozionnoj zashhity. 2015. №2 (76). S. 44–50.
  21. Semenychev V.V., Smirnova T.B. O vozmozhnosti ocenki poristosti pokrytij potenciostaticheskimi metodami [About possibility of assessment of porosity of coverings potentsiostatichesky methods] // Aviacionnye materialy i tehnologii. 2009. №2. S. 7–10.
  22. Vulf B.K., Romadin K.P. Aviacionnoe materialovedenie [Aviation materials science]. M.: Mashinostroenie, 1967. 391 s.
  23. Rozenfeld I.L. Korroziya i zashhita metallov [Corrosion and protection of metals]. M.: Metallurgiya, 1969. 448 s.
  24. Elektrolit nikelirovaniya: pat. 2293803 Ros. Federaciya [Nickel plating electrolit: pat. 2293803 Rus. Federation]; zayavl. 01.08.05; opubl. 20.02.07. Byul. №5.
  25. Elektrolit nikelirovaniya: pat. 2449063 Ros. Federaciya [Nickel plating electrolit: pat. 2449063 Rus. Federation]; zayavl. 05.04.11; opubl. 27.04.12. Byul. №12.
  26. Elektrolit hromirovaniya: pat. 2409707 Ros. Federaciya [Chromizing electrolit: pat. 2409707 Rus. Federation]; zayavl. 28.10.09; opubl. 20.01.11. Byul. №2.