Bytsenko O.A., Filonova E.V., Markov A.B., Belova N.A. Influence of radiation by high-current pulse electronbeams on surface layers of modern heat-resisting nickel alloys with ion-plasma coatings of different composition // Proceedings of VIAM. 2016. No. 6 (42). Ст. 10. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2016-0-6-10-10.
Influence of radiation by high-current pulse electronbeams on surface layers of modern heat-resisting nickel alloys with ion-plasma coatings of different composition
Abstract
With use of complex of metallophysical methods the research of physical-chemical, structural and phase conditions of the surface layer before and after modifying is carried out by means of radiation by high-current electron beams of samples with heat-resisting condensed ion-plasma coatings of three different compositions on 5 chosen modes at variation of values of electron energy and pulse number. Work is executed within implementation of the complex scientific direction 2.1. «Fundamental-oriented researches» («The strategic directions of development of materials and technologies of their processing for the period till 2030»)
Keywords
radiation by the high-current electron beams, condensed ion-plasma coatings, structural and phase conditions, microstructure research.
Reference list
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
- Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials – basis of innovative modernization of Russia] // Metally Evrazii. 2012. №3. S. 10–15.
- Kablov E.N., Ospennikova O.G., Lomberg B.S. Strategicheskie napravleniya razvitiya kon-strukcionnyh materialov i tehnologij ih pererabotki dlya aviacionnyh dvigatelej nastoyashhego i budushhego [The strategic directions of development of constructional materials and technologies of their processing for aircraft engines of the present and the future] // Avtomaticheskaya svarka. 2013. № 10. S. 23–32.
- Kablov E.N., Muboyadzhyan S.A. Zharostojkie i teplozashhitnye pokrytiya dlya lopatok turbiny vysokogo davleniya perspektivnyh GTD [Heat resisting and heat-protective coverings for turbine blades of high pressure of perspective GTE] //Aviacionnye materialy i tehnologii. 2012. №S. S. 60–70.
- Muboyadzhyan S.A., Aleksandrov D.A., Gorlov D.S., Egorova L.P., Bulavinceva E.E. Zashhitnye i uprochnyayushhie ionno-plazmennye pokrytiya dlya lopatok i drugih otvetstvennyh detalej kompressora GTD [Protective and strengthening ion-plasma coverings for blades and other responsible details of the GTE compressor] //Aviacionnye materialy i tehnologii. 2012. №S. S. 71–81.
- Budinovskij S.A., Smirnov A.A., Matveev P.V., Chubarov D.A. Razrabotka teplozashhitnyh pokrytij dlja rabochih i soplovyh lopatok turbiny iz zharoprochnyh i intermetallidnyh splavov [Development of thermal barrier coatings for rotor and nozzle turbine blades made of nickel-base super- and intermetallic alloys] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №4. St. 05. Available at: http://www.viam-works.ru (accessed: February 18, 2015). DOI: 10.18577/2307-6046-2015-0-4-5-5.
- Litye lopatki gazoturbinnyh dvigatelej: splavy, tehnologii, pokrytiya. 2-e izd. / pod obshh. red. E.N. Kablova [Cast blades of gas turbine engines: alloys, technologies, coverings. 2nd ed. / gen. ed. by E.N.Kablov]. M.: Nauka, 2006. 632 s.
- Shulov V.A., Engelko V.I., Gromov A.N., Teryaev D.A., Bycenko O.A. Primenenie silnotochnyh impul'snyh jelektronnyh puchkov dlya modificirovaniya poverhnosti lopatok gazoturbinnogo dvigatelya s perforacionnymi otverstiyami [Application of high-current pulse electronic bunches for modifying of surface of blades of the gas turbine engine with perforation openings] // Uprochnyayushhie tehnologii i pokrytiya. 2013. № 10 (106). S. 23–25.
- Pajkin A.G., L'vov A.F., Shulov V.A. i dr. Ispolzovanie silnotochnyh impulsnyh jelektronnyh puchkov dlya modifikacii svojstv lopatok GTD [Use of high-current pulse electronic bunches for updating of properties of blades of GTE] // Problemy mashinostroeniya i avtomatizacii. 2003. №3. S. 41–49.
- Novikov A.S., Pajkin A.G., Lvov A.F., Shulov V.A. Perspektivnye tehnologii poverhnostnoj obrabotki pri izgotovlenii i remonte lopatok GTD [Perspective technologies of surface processing during the manufacturing and repair of blades of GTE] // Dvigatel. 2004. №2 (32). S. 18–19.
- Pajkin A.G., Shulov V.A., Petuhov A.N., L'vov A.F. Perspektivy primeneniya silnotochnyh impul'snyh elektronnyh puchkov dlya modifikacii poverhnosti pri izgotovlenii i remonte lopatok GTD [Perspectives of application of high-current pulse electronic bunches for surface updating during the manufacturing and repair of blades of GTE] // Voprosy aviacionnoj nauki i tehniki: sb. tr. TsIAM. Ser.: Aviacionnoe dvigatelestroenie. 2006. №4 (1327). S. 5–32.
- Chabina E.B., Alekseev A.A., Filonova E.V., Lukina E.A. Primenenie metodov analiticheskoj mikroskopii i rentgenostrukturnogo analiza dlya issledovaniya strukturno-fazovogo sostoyaniya materialov [Application of methods of analytical microscopy and X-ray of the structural analysis for research of structural and phase condition of materials] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №5. St. 06. Available at: http://www.viam-works.ru (accessed: February 18, 2015).
- Pajkin A.G., Krajnikov A.V., Shulov V.A., Bytsenko O.A., Engelko V.I., Tkachenko K.I., Chikiryaka A.V. Tehnologicheskie osnovy modificirovaniya poverhnosti detalej iz zharoprochnyh nikelevyh splavov s zharostojkim NiCrAlY pokrytiem s primeneniem silnotochnyh impulsnyh jelektronnyh puchkov [Technological bases of modifying of surface of details from heat resisting nickel alloys with heat resisting NiCrAlY covering using high-current pulse electronic bunches] // Fizika i himiya obrabotki materialov. 2008. №3. S. 56–60.
- Shulov V.A., Pajkin A.G., Bytsenko O.A., Teryaev D.A., Engelko V.I., Tkachenko K.I. Razrabotka elektronno-luchevogo tehnologicheskogo processa vosstanovleniya svojstv lopatok turbiny GTD iz splava ZhS26NK s zharostojkim pokrytiem NiCrAlY [Development of electron beam technological process of recovery of properties of turbine blades of GTD from alloy ZhS26NK with heat resisting covering of NiCrAlY] // Uprochnyayushhie tehnologii i pokrytiya. 2010. №3. S. 34–38.
- Shulov V.A., Pajkin A.G., Teryaev D.A., Bycenko O.A., Engelko V.I., Tkachenko K.I. Strukturno-fazovye izmeneniya v poverhnostnyh sloyah detalej iz titanovogo splava VT6 pri obluchenii sil'notochnym impul'snym jelektronnym puchkom [Структурно-фазовые изменения в поверхностных слоях деталей из титанового сплава ВТ6 при облучении сильноточным импульсным электронным пучком] // Fizika i himiya obrabotki materialov. 2012. № 3. S. 5–9.