Nikolaev E.V., Barbotko S.L., Andreeva N.P., Pavlov M.R., Grachshencov D.V. Comprehensive research of the influence of climatic and operational factors on new generation epoxy binding and polymeric composite materials on its basis. Part 3. Calculation of activation energy and thermal resource of polymeric composite materials on the basis of epoxy matrix // Proceedings of VIAM. 2016. No. 5 (41). Ст. 11. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2016-0-5-11-11.

Comprehensive research of the influence of climatic and operational factors on new generation epoxy binding and polymeric composite materials on its basis

Part 3. Calculation of activation energy and thermal resource of polymeric composite materials on the basis of epoxy matrix
Nikolaev E.V., Barbotko S.L., Andreeva N.P., Pavlov M.R., Grachshencov D.V.
Abstract

Stability of strength characteristics of polymeric composite materials ( carbon fiber and fibreglass based on epoxy binder)in the process of thermal aging has been evaluated. Calculation of energy of activation during the process of thermal aging for polymeric composite materials has been carried out. An influence of freeze-traw cycles on mechanical characteristics of materials is shown. The level of stability of strength characteristics for long-term operation has been determined. Work is executed within implementation of the complex scientific direction 18.3. «Modeling and forecasting of climatic resistance» («The strategic directions of development of materials and technologies of their processing for the period till 2030»)

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Kablov E.N., Gunyaev G.M. Tumanov A.T. – iniciator sozdaniya kompozitov [A.T Tumanov – initiator of creation of composites] // Kompozicionnye materialy v aviakosmicheskom materialovedenii: sb. tez. dokl. mezhotrasl. nauch.-tehnich. konf. M.: VIAM, 2009. S. 6–9.
  3. Kablov E.N., Startsev O.V., Krotov A.S., Kirillov V.N. Klimaticheskoe starenie kompozicionnyh materialov aviacionnogo naznacheniya. III. Znachimye faktory stareniya [Climatic aging of composite materials of aviation assignment. III. Significant factors of aging] // Deformaciya i razrushenie materialov. 2011. №1. S. 34–40.
  4. Muhametov R.R., Ahmadieva K.R., Chursova L.V., Kogan D.I. Novye polimernye svyazujushhie dlya perspektivnyh metodov izgotovleniya konstrukcionnyh voloknistyh PKM [New polymeric binding for perspective methods of manufacturing of constructional fibrous PCM] // Aviacionnye materialy i tehnologii. 2011. №2. S. 38–42.
  5. Donetskij K.I., Hrulkov A.V., Kogan D.I., Belinis P.G., Lukyanenko Yu.V. Primenenie obemno-armiruyushhih preform pri izgotovlenii izdelij iz PKM [Use of three-dimensional reinforcing preforms during the production of polymer composite products] // Aviacionnye materialy i tehnologii. 2013. №1. S. 35–39.
  6. Kirillov V.N., Vapirov Yu.M., Drozd E.A. Issledovanie atmosfernoj stojkosti polimernyh kompozicionnyh materialov v usloviyah atmosfery teplogo vlazhnogo i umerenno teplogo klimata [Research of atmospheric firmness of polymeric composite materials in the conditions of the atmosphere of warm wet and moderately warm climate] // Aviacionnye materialy i tehnologii. 2012. №4. S. 31–38.
  7. Mishra G., Mohapatra S.R., Behera P.R., Dash B., Mohanty U.K., Ray B.C. Environmental stability of GFRP laminated composites: an emphasis on mechanical behaviour // Aircraft Eng. and Aerosp. technol. 2010. V. 82. №4. P. 258–266.
  8. 88ABW-2012-0190. Firefighting and emergency responsestudy of advanced composites aircraft // Objective 2: Firefighting Effectiveness of Technologies and Agents on Composite Aircraft Fires: distribution A. Approved for public release 10.01.2012. P. 3.
  9. Sugita Y., Winkelmann C., La Saponara V. Environmental and chemical degradation of carbon/epoxy lap joints for aerospace applications, and effects on their mechanical performance // Compos. Sci. and Technol. 2010. V. 70. №5. P. 829–839.
  10. Kirillov V.N., Efimov V.A. Problemy issledovaniya klimaticheskoj stojkosti aviacionnyh nemetallicheskih materialov [Problems of research of climatic firmness of aviation non-metallic materials] // 75 let. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2007: yubilejnyj nauch.-tehnich. sb. M.: VIAM, 2007. S. 379–388.
  11. Mikols W.J., Seferis J.C., Apicella A., Nicolais L. Evaluation of structural changes in epoxy systems by moisture sorption-desorption and dynamic mechanical studies // Polym. Compos. 1982.
  12. V. 3. №3. P. 118–124.
  13. Nikolaev E.V., Kirillov V.N., Skirta A.A., Grashhenkov D.V. Issledovanie zakonomernostej vlagoperenosa i razrabotka standarta po opredeleniyu koefficienta diffuzii i predelnogo vlagosoderzhaniya dlya ocenki mehanicheskih svojstv ugleplastikov [Study of moisture transport rules and development of a standard on measurement of the diffusion coefficient and moisture content limit to evaluate mechanical properties of carbon fiber reinforced plastics] // Aviacionnye materialy i tehnologii. 2013. №3. S. 44–48.
  14. Kablov E.N., Startsev O.V., Krotov A.S., Kirillov V.N. Klimaticheskoe starenie kompozicionnyh materialov aviacionnogo naznacheniya. I. Mehanizmy stareniya [Climatic aging of composite materials of aviation assignment. I. Aging mechanisms] // Deformaciya i razrushenie materialov. 2010. №11. S. 19–27.
  15. Kirillov V.N., Startsev O.V., Efimov V.A. Klimaticheskaya stojkost i povrezhdaemost polimernyh kompozicionnyh materialov, problemy i puti resheniya [Climatic firmness and damageability of polymeric composite materials, problems and solutions] // Aviacionnye materialy i tehnologii. 2012. №S. S. 412–423.
  16. Efimov V.A., Shvedkova A.K., Korenkova T.G., Kirillov V.N. Issledovanie polimernyh konstrukcionnyh materialov pri vozdejstvii klimaticheskih faktorov i nagruzok v laboratornyh i naturnyh usloviyah [Research of polymeric constructional materials at influence of climatic factors and loadings in laboratory and natural conditions] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №1. St. 05. Available at: http://www.viam-works.ru (accessed: December 01, 2015).
  17. Kablov E.N., Startsev O.V., Krotov A.S., Kirillov V.N. Klimaticheskoe starenie kompozicionnyh materialov aviacionnogo naznacheniya. II. Relaksaciya ishodnoj strukturnoj neravnovesnosti i gradient svojstv po tolshhine [Climatic aging of composite materials of aviation assignment. II. Relaxation of initial structural non-equilibrium and gradient of properties on thickness] // Deformaciya i razrushenie materialov. 2012. №6. S. 17–19.
  18. Van Krevelen D.V. Svojstva i himicheskoe stroenie polimerov [Properties and chemical structure of polymers]. M.: Himiya, 1976. 416 s.
  19. Nikolaev E.V., Barbotko S.L., Andreeva N.P., Pavlov M.R. Kompleksnoe issledovanie vozdejstviya klimaticheskih i jekspluatacionnyh faktorov na novoe pokolenie jepoksidnogo svyazuyushhego i polimernyh kompozicionnyh materialov na ego osnove. Chast 1. Issledovanie vliyaniya sorbirovannoj vlagi na jepoksidnuyu matricu i ugleplastik na ee osnove [Comprehensive research of the influence of climatic and operational factors on new generation epoxy binding and polymeric composite materials on its basis. Part 1. Research of the influence of sorbate moisture on epoxy matrix and layered carbon fiber on its basis] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №12. St. 11. Available at: http://www.viam-works.ru (accessed: January 25, 2015). DOI: 10.18577/2307-6046-2015-0-12-11-11.
  20. Nikolaev E.V., Barbotko S.L., Andreeva N.P., Pavlov M.R. Kompleksnoe issledovanie vozdejstviya klimaticheskih i jekspluatacionnyh faktorov na novoe pokolenie jepoksidnogo svyazuyushhego i polimernyh kompozicionnyh materialov na ego osnove. Chast 2. Obosnovanie vybora rezhimov i provedenie teplovogo stareniya polimernyh kompozicionnyh materialov na osnove jepoksidnoj matricy [Comprehensive research of the influence of climatic and operational factors on new generation epoxy binding and polymeric composite materials on its basis. Part 2. Substantiation of the choice of modes and conducting heat aging of polymeric composite materials based on epoxy matrix] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №1. St. 10. Available at: http://www.viam-works.ru (accessed: February 15, 2016). DOI: 10.18577/2307-6046-2016-0-1-10-10.
  21. Janz G.J., Estimation of thermodynamic properties of organic compounds. New York: Academic press, 1958. 224 p.
  22. Parks G.S., Huffman H.M. The free energies of some organic compounds. New York: Chem. Cat. Co.,1932. 60 p.
  23. Rossini F.D. Chemical termodinamics. New York: Wiley, 1950. 514 p.
  24. Karpuhin O.N. Opredelenie sroka sluzhby polimernogo materiala kak fiziko-himicheskaya problema [Definition of service life of polymeric material as physical and chemical problem] // Uspehi himii. 1980. T. 49. Vyp. 8. S. 1523–1553.