Fracture toughness of laminated polymer composites (review)
Abstract
The current situation in the field of estimation methods of interlaminar fracture toughness of polymer composite materials is analyzed. Experimental data on the interlayer fracture toughness GIс and GIIс of laminated polymeric composite materials based on carbon (HTS40, T-800HB, UТ-900, Porher 4510, 3692, 14535) and glass (Т-10(VMP)-14, Porher 7781) reinforcement and polymer matrix – VSE-1212, VST-1208, VST-1210, BMI-3, VSN-31, EDT-69N are given. Special fractographic features of damages of fiberglasses VPS-47/7781 and VPS-48/7781 are described. Work is executed within implementation of the complex scientific direction 2.2 «Qualification and researches of materials» («The strategic directions of development of materials and technologies of their processing for the period till 2030»)
Reference list
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
- Kablov E.N. Materialy i himicheskie tehnologii dlya aviacionnoj tehniki [Materials and chemical technologies for aviation engineering] // Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6.
- S. 520–530.
- Erasov V.S., Yakovlev N.O., Nuzhnyj G.A. Kvalifikatsionnye ispytaniya i issledovaniya prochnosti aviatsionnyh materialov [Qualification tests and researches of durability of aviation materials] //Aviacionnye materialy i tehnologii. 2012. №S. S. 440–448.
- Dimitrienko Yu.I., Gubareva E.A., Sborshhikov S.V., Erasov V.S., Yakovlev N.O. Chislennoe modelirovanie i jeksperimentalnoe issledovanie deformirovaniya uprugoplasticheskih plastin pri smyatii [Numerical modeling and pilot study of deformation of elasto-plastic plates when crushing] // Matematicheskoe modelirovanie i chislennye metody. 2015. №1 (5). S. 67–82.
- Yakovlev N.O., Erasov V.S., Popov Yu.O., Kolokoltseva T.V. Razdir po mode III tonkolistovyh polimernyh kompozicionnyh materialov dlya izdelij aviacionnoj tehniki [Tearing on mode of the III tonkolistovy polymeric composite materials for products of aviation engineering] // Novosti materialovedeniya. Nauka i tehnika: elektron. nauch.-tehnich. zhurn. 2014. №1. St. 08. Available at: http://www.materialsnews.ru (accessed: September, 03 2015).
- Kablov E.N., Grashhenkov D.V., Erasov V.S., Anchevskij I.Je., Ilin V.V., Valter R.S. Stend dlya ispytaniya na klimaticheskoj stancii GCKI krupnogabaritnyh konstrukcij iz PKM [The stand for testing for the GTsKI climatic stations of large-size designs from PKM] / V sb. dokl. IX Mezhdunarodnoj nauch. konf. po gidroaviacii «Gidroaviasalon–2012». M. 2012. S. 122–123.
- Erasov V.S., Yakovlev N.O., Gladkih A.V., Goncharov A.A., Skiba O.V., Boyarskih A.V., Podzhivotov N.Yu. Ispytaniya krupnogabaritnyh konstrukcij [Tests of large-size designs ] // Kompozitnyj mir. 2014. №1. S. 72–78.
- Erasov V.S., Yakovlev N.O., Podzhivotov N.Yu., Gladkih A.V., Goncharov A.A., Skiba O.V., Boyarskih A.V. Ispytaniya krupnogabaritnyh konstrukcij iz polimernyh kompozicionnyh materialov na silovom polu GCKI «VIAM» im. G.V. Akimova [Tests of large-size designs from polymeric composite materials on power floor of SCCT «VIAM» of G. V. Akimov] / V sb. dokladov konf. «Fundamental'nye issledovaniya v oblasti zashhity ot korrozii, stareniya, biopovrezhdenij materialov i konstrukcij v razlichnyh klimaticheskih usloviyah i prirodnyh sredah, s cel'yu obespecheniya bezopasnoj jekspluatacii slozhnyh tehnicheskih sistem. M.: VIAM, 2013 (CD-disk).
- Vlasenko F.S., Raskutin A.E. Primenenie polimernyh kompozicionnyh materialov v stroitelnyh konstrukciyah [Applying FRP in building structures] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №8. St. 03. Available at: http://www.viam-works.ru (accessed: September, 03 2015).
- Dimitrienko Yu.I., Sborshhikov S.V., Prozorovskij A.A., Gubareva E.A., Yakovlev N.O., Erasov V.S., Krylov V.D., Grigorev M.M., Fedonyuk N.N. Razrabotka mnogoslojnogo polimernogo kompozicionnogo materiala s diskretnym konstruktivno-ortotropnym zapolnitelem [Development of multi-layer polymeric composite material with discrete constructive and orthotropic filler] // Kompozity i nanostruktury. 2014. T. 6. №1. S. 32–48.
- Yakovlev N.O., Erasov V.S., Popov Yu.O., Kolokoltseva T.V. Razdir po mode III tonkolistovyh polimernyh kompozicionnyh materialov dlya izdelij aviacionnoj tehniki [Tear (mode III) of thin laminate polymer composite materials for aircraft] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №6. St. 12. Available at: http://www.viam-works.ru (accessed: September, 03 2015). DOI: 10.18577/2307-6046-2014-0-6-12-12.
- Dimitrienko Yu.I., Fedonyuk N.N., Gubareva E.A., Sborshhikov S.V., Prozorovskij A.A., Erasov V.S., Yakovlev N.O. Modelirovanie i razrabotka trehslojnyh kompozicionnyh materialov s sotovym zapolnitelem [Modeling and development of three-layered composite materials with cellular filler] // Vestnik MGTU im. N.E. Baumana. Ser. «Estestvennye nauki». 2014. №5 (56). S. 66–81.
- Borshchev A.V., Gusev Yu.A. Polimernye kompozicionnye materialy v avtomobilnoj promyshlennosti [Polymer composite materials in automotive industry] // Aviacionnye materialy i tehnologii. 2014. №S2. S. 34–38.
- Yakovlev N.O., Erasov V.S., Krylov V.D., Popov Yu.A. Metody opredeleniya sdvigovyh harakteristik polimernyh kompozicionnyh materialov [Methods of definition of shift characteristics of polymeric composite materials] // Aviacionnaya promyshlennost. 2014. №1. S. 20–23.
- Yakovlev N.O., Erasov V.S., Kolokoltseva T.V. Osobennosti opredeleniya harakteristik sdviga v ploskosti lista polimernyh kompozicionnyh materialov v razlichnyh standartah [Features of definition of characteristics of shift in the plane of leaf of polymeric composite materials in different standards] // Vse materialy. Enciklopedicheskij spravochnik. 2014. №5. S. 12–16.
- Gulyaev A.I., Tenchurin T.H. Perspektivy primeneniya voloknistyh struktur, poluchennyh sposobom jelektroformovaniya, dlya povysheniya udaro- i treshhinostojkosti polimernyh kompozicionnyh materialov [Perspectives of application of the fibrous structures received in the way of electro formation, for increase udaro-and treshchinostoykost of polymeric composite materials] // Konstrukcii iz kompozicionnyh materialov. 2013. №3. C. 22–26.
- Kablov E.N., Kondrashov S.V., Yurkov G.Yu. Perspektivy ispolzovaniya uglerodsoderzhashhih nanochastic v svyazuyushhih dlya polimernyh kompozicionnyh materialov [Perspectives of use of carbon-containing nanoparticles in binding for polymeric composite materials] // Rossijskie nanotehnologii. 2013. T. 8. №3–4. S. 24–42.
- Yakovlev N.O., Akolzin S.V., Shvec S.M. Opredelenie treshhinostojkosti polimernyh materialov [Definition of crack firmness of polymeric materials] // Novosti materialovedeniya. Nauka i tehnika: elektron. nauch.-tehnich. zhurn. 2014. №4. St. 03. Available at: http://www.materialsnews.ru (accessed: September, 03 2015).
- Gulyaev A.I., Zhuravleva P.L., Filonova E.V., Antyufeeva N.V. Vliyanie otverditelya kataliticheskogo dejstviya na morfologiyu mikrostruktury jepoksidnyh ugleplastikov [Influence of hardener of catalytic action on morphology of microstructure epoxy coal of plastics] // Materialovedenie. 2015. № 5. S. 41–46.
- Ustrojstvo dlya opredeleniya prochnosti kompozicionnogo materiala: pat. 150187 Ros. Federaciya [The device for determination of durability of composite material: pat. 150187 Rus. Federation]; opubl. 18.09.14.
- Yakovlev N.O., Lutsenko A.N., Artemeva I.V. Metody opredeleniya mezhsloevoj treshhinostojkosti sloistyh materialov [Methods of definition of crack firmness between layers in layered materials] // Vse materialy. Enciklopedicheskij spravochnik. 2015. №10. S. 57–62.
- Finogenov G.N., Erasov V.S. Treshhinostojkost polimernyh kompozitov pri mezhslojnyh otryve i sdvige [Crack firmness of polymeric composites at inter laminar separation and shift] // Aviacionnye materialy i tehnologii. 2003. №3. S. 62–67.
- Yakovlev N.O., Erasov V.S., Petrova A.P. Sravnenie normativnyh baz razlichnyh stran po ispytaniyu kleevyh soedinenij materialov [Comparison of regulatory bases of the different countries on testing of glued joints of materials] // Vse materialy. Enciklopedicheskij spravochnik. 2014. №7. S. 2–8.
- Benzeggagh M.L., Kenane M. Measurement of mixed-mode delamination fracture toughness of unidirectional glass/epoxy composites with mixed-mode bending apparatus // Composites Science and Technology. 1996. V. 56. P. 439–449.
- Finogenov G.N. Metody ispytaniya kleevyh soedinenij metallov na treshhinostojkost [Test methods of glued joints of metals on crack firmness] // Klei. Germetiki. Tehnologii. 2007. №5. S. 24–26.
- Krylov V.D., Yakovlev N.O., Kurganova Yu.A., Lashov O.A. Mezhsloevaya treshhinostojkost' konstrukcionnyh polimernyh kompozicionnyh materialov [Interlayer fracture toughness of structural polymer composites] // Aviacionnye materialy i tehnologii. 2016. №1 (40). S. 79–85.
- Sokolov I.I., Raskutin A.E. Ugleplastiki i stekloplastiki novogo pokoleniya [Coalplastics and fiber lasses of new generation] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №4. St. 09. Available at: http://www.viam-works.ru (accessed: September, 03 2015).
- Babin A. N. Svyazujushhie dlya polimernyh kompozicionnyh materialov novogo pokoleniya [Binding for polymeric composite materials of new generation] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №4. St. 11. Available at: http://www.viam-works.ru (accessed: September, 03 2015).
- Panina N.N., Chursova L.V., Babin A.N., Grebeneva T.A., Gurevich Ya.M. Osnovnye sposoby modifikacii epoksidnyh polimernyh materialov v Rossii [The main ways of updating of epoxy polymeric materials in Russia] // Vse materialy. Enciklopedicheskij spravochnik. 2014. №9. S. 10–17.
- Muhametov R.R., Shimkin A.A., Gulyaev A.I., Kucherovskij A.I. Ftalonitrilnoe svyazuyushhee dlya termostojkih kompozitov [Ftalo the nitrile binding for heat-resistant composites] // Materialovedenie. 2015 (v pechati).
- Gulyaev A.I., Zhuravleva P.L. Metodologicheskie voprosy analiza fazovoj morfologii materialov na osnove sinteticheskih smol, modificirovannyh termoplastami (obzor) [Methodological aspects of the phase morphology analysis in materials based on synthetic resins modified by thermoplastics] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №6. St. 09. Available at: http://www.viam-works.ru (accessed: September, 03 2015). DOI: 10/18577-2307-6046-2015-0-6-9-9.
- Deev I.S., Kablov E.N., Kobets L.P., Chursova L.V. Issledovanie metodom skaniruyushhej elektronnoj mikroskopii deformacii mikrofazovoj struktury polimernyh matric pri mehanicheskom nagruzhenii [Research of the scanning electron microscopy method deformation of microphase structure of polymeric matrix at mechanical loading] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №7. St. 06. Available at: http://www.viam-works.ru (accessed: September, 03 2015). DOI: 10/18577-2307-6046-2014-0-7-6-6.
- Gulyaev A.I., Yakovlev N.O., Krylov V.D., Shurtakov S.V. Mikromehanika razrusheniya stekloplastikov pri rassloenii po modam I i II [Microfracture mechanics of fiber glasses at stratification on modes of I and II] // Materialovedenie. 2016. №2. S. 13–22.
- Sham Prasad M.S., Venkatesha C.S., Jayaraju T. Experimental Methods of Determining Fracture Toughness of Fiber Reinforced Polymer Composites under Various Loading Conditions // Journal of Minerals & Materials Characterization & Engineering. 2011. V. 10. №13. P. 1263–1275.