Kucheryaev V.V., Mironova N.A., Shishkov S.U. Research of technological features of Ni–Al–Co system ingots deformation // Proceedings of VIAM. 2016. No. 3 (39). Ст. 01. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2016-0-3-1-1.
Research of technological features of Ni–Al–Co system ingots deformation
Abstract
The results of studies of the structure and rheological properties of the experimental alloy based on ternary Ni–Al–Co system for development gas turbine disk technology are presented. Application specifics of protective coatings technology (РСТ) based on vitreous during isothermal forging of the experimental alloy ingots based on ternary Ni–Al–Co on the air are considered. The effectiveness of PCT in the deformation process is experimentally demonstrated.
Reference list
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
- Kablov E.N., Lomberg B.S., Ospennikova O.G. Sozdanie sovremennyh zharoprochnyh materialov i tehnologij ih proizvodstva dlya aviacionnogo dvigatelestroeniya [Creation of modern heat resisting materials and technologies of their production for aviation engine building] // Krylya Rodiny. 2012. №3–4. S. 34–38.
- Lomberg B.S., Ovsepyan S.V., Bakradze M.M., Mazalov I.S. Vysokotemperaturnye zharo-prochnye nikelevye splavy dlya detalej gazoturbinnyh dvigatelej [High-temperature heat resisting nickel alloys for details of gas turbine engines] //Aviacionnye materialy i tehnologii. 2012. №S. S. 52–57.
- Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokoleniya [Nickel foundry heat resisting alloys of new generation] // Aviacionnye materialy i tehnologii. 2012. №S. C. 36–52.
- Lomberg B.S., Ovsepjan S.V., Bakradze M.M. Osobennosti legirovanija i termicheskoj obrabotki zharoprochnyh nikelevyh splavov dlja diskov gazoturbinnyh dvigatelej no-vogo pokolenija [Features of alloying and thermal processing of heat resisting nickel alloys for disks of gas turbine engines of new generation] // Aviacionnye materialy i tehnologii. 2010. №2. S. 3–8.
- Kablov E.N., Petrushin N.V., Elyutin E.S. Monokristallicheskie zharoprochnye splavy dlya gazoturbinnyh dvigatelej [Single-crystal hot strength alloys for gas turbine engines] // Vestnik MGTU im. N.E. Baumana. Ser. «Mashinostroenie». 2011. №SP2. S. 38–52.
- High temperature resistant cobalt base superalloy: pat. 2010/0061883 US; publ. 11.03.10.
- Cobalt base alloy with high heat resistance and high strength and process for producing the same: pat. 2008/0185078 Japan; publ. 07.08.08.
- Ternary nickel eutectic alloy: pat. 2009/0136381 UK; publ. 28.05.08.
- Irridium-based alloy with high heat resistance and high strength and process for producing the same: pat. 2008/0206090 Japan; publ. 28.08.08.
- Bazyleva O.A., Arginbaeva E.G., Turenko E.Yu. Zharoprochnye litejnye intermetallidnye splavy [Heat resisting cast intermetallic alloys] //Aviacionnye materialy i tehnologii. 2012. №S. S. 57–60.
- Kablov E.N., Ospennikova O.G., Bazyleva O.A. Materialy dlya vysokoteplonagruzhennyh detalej gazoturbinnyh dvigatelej [Materials for the high-heatloaded details of gas turbine engines] // Vestnik MGTU im. N.E. Baumana. Ser. «Mashinostroenie». 2011. №SP4. S. 13–19.
- Letnikov M.N., Lomberg B.S., Ovsepyan S.V. Issledovanie kompozicij sistemy Ni–Al–Co pri razrabotke novogo zharoprochnogo deformiruemogo intermetallidnogo splava [Investigation experimental alloys based on Ni–Al–Co ternary system for development a new high-temperature intermetallic alloy for disk application] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. № 10. St. 01. Available at: http://www.viam-works.ru (accessed: May 21, 2015).
- Ponomarenko D.A., Rozenenkova V.A., Skugorev A.V., Shishkov S.Yu. Effektivnoe ispolzovanie zashhitnyh tehnologicheskih pokrytij pri izotermicheskoj shtampovki na vozduhe slozhnoprofilnyh detalej iz titanovyh splavov [Effective use of protective technological coverings at isothermal punching on air of difficult profile details from titanium alloys] // Kuznechno-shtampovochnoe proizvodstvo. Obrabotka materialov davleniem. 2014. №9. S. 44–48.
- Ponomarenko D.A., Moiseev N.V., Skugorev A.V. Effektivnaya tehnologiya izgotovleniya diskov GTD iz zharoprochnyh nikelevyh splavov [Effective manufacturing techniques of disks GTD from heat resisting nickel alloys] // Kuznechno-shtampovochnoe proizvodstvo. Obrabotka metallov davleniem. 2013. №10. S. 13–17.