Veshkin E.A Features of out-of-autoclave forming of poor-porous PCM // Proceedings of VIAM. 2016. No. 2 (38). Ст. 07. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2016-0-2-7-7.

Features of out-of-autoclave forming of poor-porous PCM

Veshkin E.A
Abstract

Methods of decrease in porosity in PCM manufactured by vacuum molding are considered. Technological properties of epoxy binder and prepreg on its basis are studied with the use of instruments of Brookfield Cap 2000+, DSC 204F1 and IAP 2003. On the basis of these studies parameters of technological mode of curing of PCM are selected. The study of the mechanical properties of fiberglass is carried out on testing machine Zwick/Roell Z050.

Keywords
epoxy binder, prepreg of fiberglass, control techniques of technological properties, fiberglass, thermal analysis.
Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Prognozy razvitiya mirovogo rynka grazhdanskoj aviacii [Forecasts of development of the world market of civil aviation] // TI CAGI. 2003. №3–4. S. 6.
  3. Available at: http://www.airbus.com (accessed: March 18, 2015).
  4. Available at: http://www.compositesworld.com (accessed: March 18, 2015).
  5. Veshkin E.A., Postnov V.I., Zastrogina O.B., Satdinov R.A. Tehnologiya uskorennogo formovaniya trehslojnyh sotovyh panelej interera samoleta [Technology of the accelerated formation of three-layered cellular panels of interior of airplane] // Izvestiya Samarskogo nauchnogo centra RAN. 2013. T. 15. №4 (4). S. 799–805.
  6. Kogan D.I., Dushin M.I., Borshhev A.N., Veshkin E.A., Abramov P.A., Makrushin K.V Svojstva konstrukcionnyh ugleplastikov, izgotovlennyh propitkoj pod vakuumom [Properties constructional coal of the plastics made by impregnation under vacuum] // Izvestiya Samarskogo nauchnogo centra RAN. 2012. T. 14. №4 (2). S. 762–766.
  7. Postnov V.I., Veshkin E.A., Abramov P.A. Osobennosti podgotovki polimernogo svyazuyushhego dlya snizheniya poristosti stekloplastikov, poluchaemyh metodom vakuumnogo formovaniya [Features of preparation polymeric binding for decrease in porosity of the fibreglasses received by method of vacuum formation] // Izvestija Samarskogo nauchnogo centra RAN. 2011. T. 13. №4 (2). S. 462–468.
  8. Kablov E.N., Startsev O.V., Krotov A.S., Kirillov V.N. Klimaticheskoe starenie kompozicionnyh materialov aviacionnogo naznacheniya. III. Znachimye faktory starenya [Climatic aging of composite materials of aviation assignment. III. Significant factors of aging] // Deformaciya i razrushenie materialov. 2011. №1. S. 34–40.
  9. Gecha E.Ya., Nesterenko V.A. K voprosu ob opredelenii kojefficienta diffuzii vody v polimernyh materialah po krivym pogloshheniya [To question of determination of diffusion factor of water in polymeric materials on absorption curves] // Plasticheskie massy. 2005. №5. S. 46–49.
  10. Kablov E.N., Startsev O.V., Krotov A.S., Kirilov V.N. Klimaticheskoe starenie kompozicionnyh materialov aviacionnogo naznacheniya. I. Mehanizmy stareniya [Climatic aging of composite materials of aviation assignment. I. Aging mechanisms] // Deformaciyaa i razrushenie materialov. 2010. №11. S. 19–26.
  11. Available at: http://www.gurit.com (accessed: March 18, 2015).
  12. Available at: http://www.cytec.com (accessed: March 18, 2015).
  13. Deraster R.L. Deracure curing agent DR. Product Datasheet, Finnester coating Oy. 3.11.2011.
  14. Muhametov R.R., Ahmadieva K.R., Kim M.A., Babin A.N. Rasplavnye svyazujushhie dlya perspektivnyh metodov izgotovleniya PKM novogo pokoleniya [Melt binding for perspective methods of production of PCM of new generation] // Aviacionnye materialy i tehnologii. 2012. №S. S. 260–265.
  15. Panina N.N., Kim M.A., Gurevich Ya.M., Grigorev M.M., Chursova L.V., Babin A.N. Svyazujushhie dlya formovaniya izdelij iz polimernyh kompozicionnyh materialov [Binding for formation of products from polymeric composite materials] // Klei. Germetiki. Tehnologii. 2013. №10. S. 27–35.
  16. Anjali, Sanjay Choudhry, Vijay Kumar. Effect of porosity on themechanical strength of composite materials // International Journal of Mechanical and Industrial Engineering. 2012. V. 2. №3. P. 82–84.
  17. Dushin M.I., Kogan D.I., Khrulkov A.V., Gusev Yu.A. Prichiny obrazovanija poristosti v izdeliyah iz polimernyh kompozicionnyh materialov (obzor) [The reasons of formation of porosity in products from polymeric composite materials (overview)] // Kompozity i nanostruktury. 2013. №3. S. 60–68.
  18. Postnov V.I., Veshkin E.A., Abramov P.A. Puti povyshenija kachestva detalej iz PKM pri vakuumnom formovanii [Ways of improvement of quality of details from PKM at vacuum formation] // Izvestiya Samarskogo nauchnogo centra RAN. 2012. T. 14. №4 (3). S. 834–839.
  19. Veshkin E.A., Abramov P.A., Postnov V.I., Strel'nikov S.V. Vlijanie tehnologii podgotovki preprega na svojstva PKM [Influence of technology of preparation of prepreg on PKM properties] // Vse materialy. Enciklopedicheskij spravochnik. 2013. №9. S. 8–14.
  20. Kablov E.N. Himiya v aviacionnom materialovedenii [Chemistry in aviation materials science] // Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  21. Antyufeeva N.V., Komarova O.A., Pavlovskij K.A., Aleksashin V.M. Opyt primeneniya kalorimetricheskogo kontrolya reakcionnoj sposobnosti preprega KMU-11tr [Practice of the calorimetric control reactionary ability prepreg KMU-11tr] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №2. St. 06. URL: http://www.viam-works.ru (accessed: March 18, 2015). DOI: 10.18577/2307-6046-2014-0-2-6-6.
  22. Malysheva G.V., Ahmetova E.Sh., Shimina Yu.Yu. Ocenka temperatur fazovyh perehodov polimernyh svyazuyushhih metodom differencialno-skanirujushhej kalorimetrii [Assessment of temperatures of phase transitions polymeric binding method differential scanning calorimetry] // Klei. Germetiki. Tehnologii. 2014. №6. S. 29–33.
  23. Postnov V.I., Nikitin K.E., Burhan O.L., Petuhov V.I., Orzaev V.G. Issledovanie ultrazvukovym metodom strukturnyh izmenenij v PKM v processe formovaniya polimernyh kompozicionnyh materialov [Research by ultrasonic method of structural changes in PKM in the course of formation of polymeric composite materials] // Aviacionnye materialy i tehnologii. 2009. №3. S. 25–29.
  24. Nikitin K.E., Burhan O.L., Postnov V.I., Petuhov V.I. Laboratornaja ustanovka dlya issledovaniya i otrabotki processov formovaniya IPF 2003 polimernyh kompozicionnyh materialov ultrazvukovym metodom [Laboratory installation for research and working off of processes of formation of IPF of 2003 polymeric composite materials by ultrasonic method] // Zavodskaja laboratorija. Diagnostika materialov. 2008. №4. S. 38–41.