Nesterova T.A., Platonov M.M., Nazarov I.A., Barbotko S.L. Researches on development new material for ballonet of pneumatic emergency slide of helicopter // Proceedings of VIAM. 2016. No. 12 (48). Ст. 07. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2016-0-12-7-7.

Researches on development new material for ballonet of pneumatic emergency slide of helicopter

Nesterova T.A., Platonov M.M., Nazarov I.A., Barbotko S.L.
Abstract

Research on development of film-fabric material intended for manufacturing ballonets, survival equipment of helicopter crew are conducted. Frictioned fabric applied now for manufacturing ballonets has an insufficient bonding strength of coating with fabric and as a result short service life of ballonets. For carrying out research materials have been made of synthetic polyamide or polyester fabrics with double-sided polymer coating on the basis of polyurethane rubbers of brands SKU-8A and SKU-8TB, mix of ethylene-propylene rubber of SKEPT-40 brand with butyl rubber of BK-1675N brand and siloxane rubber of SKT brand. Their physical, physicomechanical and special properties are studied. It is shown that film-fabric material made on the basis of polyester fabric аrt. 208 and polyurethane SKU-8TB rubber is the most conformed to the requirements.

Keywords
multi-layer material, ballonet, gas permeability, polymer coating, technical fabrics.
Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33
  2. Kablov E.N. Materialy i himicheskie tehnologii dlya aviacionnoj tehniki [Materials and chemical technologies for aviation engineering] // Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
  3. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] // Vse materialy. Enciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  4. Savenkova A.V., Chursova L.V., Eliseev O.A., Glazov P.A. Germetiki aviacionnogo naznacheniya [Hermetics of aviation assignment] // Aviacionnye materialy i tehnologii. 2012. №3. S. 40–43.
  5. Kablov E.N. Rossii nuzhny materialy novogo pokoleniya [Materials of new generation are necessary to Russia] // Redkie zemli. 2014. №3. S. 8–13.
  6. TSO-C69с. Technical Standard Orbler: publ. 18.08.1999. Р. 1–20.
  7. Normy letnoj godnosti samoletov transportnoj kategori: AP-25; 3-e izd., s popravkami 1–7: utv. Postanovleniem 28-j sessii Soveta po aviacii i ispolzovaniyu vozdushnogo prostranstva 11.12.2008 [Standards of the flight validity of airplanes of transport category: AP-25; 3rd ed., with corrections 1–7: are approved as the Resolution of the 28th session of Council for aircraft and use of air space November 12, 2008]. M.: Aviaizdat, 2014. 278 s.
  8. Barbotko S.L. Pozharobezopasnost aviacionnyh materialov [Fire safety of aviation materials] // Aviacionnye materialy i tehnologii. 2012. №S. S. 431–439.
  9. Nesterova T.A., Barbotko S.L., Nikolaeva M.F., Gerter Yu.A. Mnogoslojnyj zashhitno-dekorativnyj material dlya dekorirovaniya detalej v salonah samoletov i vertoletov [Multi-layer protective and decorative material for decorating details in the cabin of aircraft and helicopters] // Trudy VIAM: elektron. nauch.-tehni. zhurn. 2013. №8. St. 04. Available at: http://www.viam-works.ru (accessed: June 11, 2016).
  10. Sytyj Yu.V., Sagomonova V.A., Kislyakova V.I., Bolshakov V.A. Vibropogloshhayushhie materialy na osnove termojelastoplastov [Vibro absorbing materials on the basis of thermoelastoplastics] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №3. St. 06. Available at: http://viam-works.ru (accessed: June 11, 2016).
  11. Platonov M.M., Nesterova T.A., Nazarov I.A., Bejder E.Ya. Pozharobezopasnyj material na tekstilnoj osnove s poliuretanovym pokrytiem dlya naduvnoj obolochki spasatelnogo trapa [Fabric-based fireproof material with polyurethane coating for inflatable shell of rescue ladder] // Aviacionnye materialy i tehnologii. 2013. №2. S. 50–54.
  12. Platonov M.M., Shuldeshov E.M., Nesterova T.A., Sagomonova V.A. Akusticheskie polimernye materialy novogo pokoleniya (obzor) [Acoustic polymeric materials of new generation (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №4. St. 09. Available at: http://viam-works.ru (accessed: 30.06.2016). DOI: 10.18577/2307-6046-2016-0-4-9-9.
  13. 13 Kukin G.N., Solov'eva A.N. Tekstilnoe materialovedenie [Textile materials science]. M.: Lenprombytizdat, 1985. S. 163–202.
  14. 14 Reznichenko S.V. Bolshoj spravochnik rezinshhika [The large references book for specialist in rubbers]. M.: MAI, 2012. Ch. 1: Kauchuki i ingredienty. S. 340–346.
  15. Alifanov E.V., Chaykun A.М., Venediktova M.A., Naumov I.S. Osobennosti receptur rezin na osnove etilenpropilenovyh kauchukov i ih primenenie v izdeliyah specialnogo naznacheniya (obzor) [Specialties of rubber compounds recipes based on ethylene-propylene rubbers and their application in the articles for special purpose (review)] // Aviacionnye materialy i tehnologii. 2015. №2 (35). S. 51–55. DOI: 10.18577/2071-9140-2015-0-2-51-55.
  16. Venediktova M.A., Naumov I.S., Chajkun A.M., Eliseev O.A. Sovremennye tendencii v oblasti ftorsiloksanovyh i siloksanovyh kauchukov i rezin na ih osnove (obzor) [Investigation of properties changing of serial rubber compounds on the base of different rubbers in standardized working fluids] // Aviacionnye materialy i tehnologii. 2014. №S3. S. 17–24. DOI: 10.18577/2071-9140-2014-0-S3-17-24.
  17. Andrianova G.P. Himiya i tehnologiya polimernyh plenochnyh materialov i iskusstvennoj kozhi [Chemistry and technology of polymeric film materials and imitation leather]. M.: Legkaya i pishhevaya promyshlennost, 1981. Ch. 2: Tehnologicheskie processy proizvodstva polimernyh plenochnyh materialov i iskusstvennoj kozhi. S. 160–211.