Mitin A.O., Sentiourin E.G., Mekalina I.V., Bogatov V.A. Protective shock-resistant and vandal-proof materials and laminated glass composition // Proceedings of VIAM. 2016. No. 12 (48). Ст. 06. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2016-0-12-6-6.

Protective shock-resistant and vandal-proof materials and laminated glass composition

Mitin A.O., Sentiourin E.G., Mekalina I.V., Bogatov V.A.
Abstract

Overview of the results of patent research in the field of development of materials and multilayered vandal-proof glazing compositions, nonshatterable, safety technical means of protection, designed for open installation in public places is presented. The main world trends are identified in the field of development of vandal-proof transparent composite materials provided reducing weight of products, improvement in performance and giving variable functional properties to the material . Work is executed in the framework of the integrated scientific direction 15.4. «Optical materials and glazing materials» («Strategic directions of development of materials and technologies for processing them for the period up to 2030»)

Keywords
polymethylmethacrylate, polycarbonate, impact-resistance, armor protection, glass ceramic, abrasion resistance.
Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. GOST R 51136–2008. Stekla zashhitnye mnogoslojnye. Obshhie tehnicheskie usloviya [GOST P 51136-2008. Glasses the protective multi-layer. General specifications]. M., 2008. 24 s.
  3. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  4. Kablov E.N. Konstrukcionnye i funkcionalnye materialy – osnova ekonomicheskogo i nauchno-tehnicheskogo razvitiya Rossii [Constructional and functional materials – basis of economic and scientific and technical development of Russia] // Voprosy materialovedeniya. 2006. №1. S. 64–67.
  5. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] // Vse materialy. Enciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  6. Sposob formovaniya izdelij iz organicheskogo stekla: pat. 2203804 Ros. Federaciya [Way of formation of products from organic glass: pat. 2203804 Rus. Federation]; zayavl. 19.12. 00; opubl.10.05.03.
  7. Mekalina I.V., Trigub T.S., Bogatov V.A., Sentyurin E.G. Novoe vysokoteplostojkoe orientirovannoe orgsteklo marki VOS-2AO [The new high-heatresistant oriented organic glass of the VOS-2AO brand] // Aviacionnye materialy i tehnologii. 2010. №3. S. 14–19.
  8. Mekalina I.V., Sentyurin E.G., Klimova S.F., Bogatov V.A. Novye «serebrostojkie» organicheskie stekla [New «silver resistant» organic glasses] // Aviacionnye materialy i tehnologii. 2012. №4. S. 45–48.
  9. Petrov A.A., Mekalina I.V., Sentyurin E.G., Bogatov V.A. Issledovanie osobennostej izgotovleniya detalej ostekleniya iz chastichno sshityh organicheskih stekol [Features of manufacture of glazing parts from partially cross-linked organic glasses] // Aviacionnye materialy i tehnologii. 2013. №2. S. 32–34.
  10. Mnogoslojnaya steklopolimernaya kompoziciya: pat. 2184093 Ros. Federaciya [The multi-layer glass polymeric composition: pat. 2184093 Rus. Federation]; zayavl. 20.06.20; opubl. 27.06.02.
  11. Sposob izgotovleniya mnogoslojnogo stekla: pat. 2223240 Ros. Federaciya [Way of manufacturing of multi-layer glass: pat. 2223240 Rus. Federation]; zayavl. 26.12.01; opubl.10.02.04.
  12. Sposob izgotovleniya mnogoslojnogo stekla: pat. 2228851 Ros. Federaciya [Way of manufacturing of multi-layer glass: pat. 2228851 Rus. Federation]; zayavl. 16.03.01; opubl. 20.05.04.
  13. Prozrachnoe mnogoslojnoe stroitelnoe osteklenie: pat. 2396224 Ros. Federaciya [Transparent multi-layer construction glazing: pat. 2396224 Rus. Federation]; zayavl. 01.04.09; opubl. 10.08.10.
  14. Krynin A.G., Hohlov Yu.A., Bogatov V.A., Kislyakov P.P. Prozrachnye interferencionnye pokrytiya dlya funkcionalnyh materialov ostekleniya [Transparent interferential coatings for functional materials of glazing] // Trudy VIAM : elektron. nauch.-tenhich. zhurn. 2013. №11. St. 05. Available at: http://viam-works.ru (accessed at: February, 24 2015).
  15. Struktura udaroprochnogo ostekleniya: pat. 4312903 SShA [Structure of shock-resistant glazing: pat. 4312903 USA]; zayavl. 05.03.80; opubl. 26.01.82.
  16. Sposob izgotovleniya mnogoslojnyh bezoskolochnyh stekol: pat. 81028318 Germaniya [Way of manufacturing of multi-layer shatter-proof glasses: stalemate. 81028318 Germany]; zayavl. 13.06.08; opubl. 17.12.09.
  17. Mnogoslojnaya steklopolimernaya kompoziciya: pat. 2184093 Ros. Federaciya [Multi-layer glass polymer composition: pat. 2184093 Dews. Federation]; zayavl. 20.06.00; opubl. 27.06.02.
  18. Struktura udaroprochnogo ostekleniya: pat. 4312903 SShA [Structure of shock-resistant glazing: pat. 4312903 USA]; zayavl. 05.03.80; opubl. 26.01.82.
  19. Sposob laminirovaniya listov stekla s ispolzovaniem mikrovolnovogo izlucheniya: pat. 7063760 SShA [Way of lamination of sheets of glass with use of microwave radiation: pat. 7063760 USA]; zayavl. 13.01.04; opubl. 20.06.06.
  20. Sposob laminirovaniya stekla s ispolzovaniem korotkovolnovoj radiacii: pat. 7063760 SShA [Way of lamination of glass with use of short-wave radiation: pat. 7063760 USA]; zayavl. 13.01.2004; opubl. 20.06.06.
  21. Sposob laminirovaniya listov stekla s ispolzovaniem korotkovolnovogo izlucheniya: pat. 7344613 SShA [Way of lamination of sheets of glass with short wave radiation use: pat. 7344613 USA]; zayavl. 09.01.06; opubl. 18.03.08.
  22. Prozrachnoe osteklenie s pokrytiem. Sposob izgotovleniya: pat. 4710433 SShA [Transparent glazing with covering. Way of manufacturing: pat. 4710433 USA]; zayavl. 09.07.86; opubl. 01.12.87.
  23. Mnogoslojnoe osteklenie s zashhitoj ot elektromagnitnogo izlucheniya: pat. 2793106 Franciya [Multi-layer glazing with protection against electromagnetic radiation: pat. 2793106 France]; zayavl. 28.04.99; opubl. 03.11.00.
  24. Prozrachnoe abrazivostojkoe osteklenie. Sposob izgotovleniya: pat. 4272587 SShA [Transparent abrasive resistant glazing. Way of manufacturing: pat. 4272587 USA]; zayavl. 17.12.79; opubl. 09.06.81.