Ivanov M.S., Kuleznev V.N. Method of mechanical spectroscopy of pipe grades of polyethylene // Proceedings of VIAM. 2016. No. 11 (47). Ст. 09. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2016-0-11-9-9.

Method of mechanical spectroscopy of pipe grades of polyethylene

Ivanov M.S., Kuleznev V.N.
Abstract

The method of research of creep at step loading is offered and the device of automatic registration of deformation is developed. This method consists in uniaxial step stretching of polymer sample in isothermal conditions at temperature of 100°C when mobility of supermolecular structures of polymer is facilitated. As a result the dependence of relative deformation on time is having the step appearance . The constant deformation, i.e. equilibrium deformation of certain structural elements remains on each step of this curve. The curve consists of three sites: on the first the Hooke law is carried out; the second is responsible for step creep; on the third is developed the general plastic strain and sample passes to neck. Sample reduction to the initial sizes is also revealed at loading reduction after step loading. It is supposed that driving force of process of retardation are relaxation processes. The method of step loading is peculiar «mechanical spectroscopy» of supermolecular structu

Keywords
method of step loading, polyethylene pipe grades, tie molecule.
Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Grashhenkov D.V., Chursova L.V. Strategiya razvitiya kompozicionnyh i funkcionalnyh materialov [Strategy of development of composite and functional materials] // Aviacionnye materialy i tehnologii. 2012. №S. S. 231–242.
  3. Larionov S.A., Deev I.S., Petrova G.N., Bejder E.Ya. Vliyanie uglerodnyh napolnitelej na elektrofizicheskie, mehanicheskie i reologicheskie svojstva polietilena [Effect of carbon fillers on the electrical, mechanical and rheological properties of polyethylene] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №9. St. 04. Available at: http://www.viam-works.ru (accessed: April 20, 2016).
  4. Shurajc A.L., Kargin V.Yu., Volnov Yu.N. Gazoprovody iz polimernyh materialov: posobie po proektirovaniyu, stroitelstvu i ekspluatacii [Gas pipelines from polymeric materials: grant on design, construction and operation]. Saratov: Volga – HHI vek, 2007. S. 30–46.
  5. Cheng Joy J. Mechanical and Chemical Properties of High Density Polyethylene: Effects of Microstructure on Creep Characteristics: PHD thesis. Waterloo. Ontario. Canada. 2008. P. 9–10.
  6. Marihin V.A., Myasnikova L.P. Nadmolekulyarnaya struktura polimerov [Supramolecular structure of polymers]. L.: Himiya, 1977. C. 42–49.
  7. Uajt Dzh.L., Choj D.D. Polietilen, polipropilen i drugie poliolefiny: per. s angl [Polyethylene, polypropylene and other polyolefins: tans. from English]. SPb.: Professiya, 2006. S. 97–100.
  8. Kuleznev V.N., Shershnev V.A. Himiya i fizika polimerov. 2-e izd. [Chemistry and physics of polymers. 2nd ed.]. M.: Koloss, 2007. S. 118–121.
  9. Petrova G.N., Perfilova D.N., Gryaznov V.I., Bejder E.Ya. Termoplastichnye elastomery dlya zameny rezin [Thermoflexible elastomer for replacement of rubbers] // Aviacionnye materialy i tehnologii. 2012. №S. S. 302–308.
  10. Petrova G.N., Rumyantseva T.V., Perfilova D.N., Bejder E.Ya., Gryaznov V.I. Termoelastoplasty – novyj klass polimernyh materialov [Thermoelastoplastics – new class of polymeric materials] // Aviacionnye materialy i tehnologii. 2010. №4. S. 20–25.
  11. Tkachuk A.I., Grebeneva T.A., Chursova L.V., Panina N.N. Termoplastichnye svyazuyushhie. Nastoyashhee i budushhee [Thermoplastic binders. The present and the future] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №11. St. 07. Available at: http://www.viam-works.ru (accessed: April 20, 2016).
  12. Kablov E.N. Korroziya ili zhizn [Corrosion or life] // Nauka i zhizn. 2012. №11. S. 16–21.
  13. Deev I.S., Kablov E.N., Kobets L.P., Chursova L.V. Issledovanie metodom skaniruyushhej elektronnoj mikroskopii deformacii mikrofazovoj struktury polimernyh matric pri mehanicheskom nagruzhenii [Research of the scanning electron microscopy method deformation of microphase structure of polymeric matrix at mechanical loading] // Trudy VIAM: elektron. nauch-tehnich. zhurn. 2014. №7. St. 06. Available at: http://www.viam-works.ru (accessed: April 20, 2016). DOI: 10.18577/2307-6046-2014-0-7-6-6.
  14. Kuleznev V.N., Ivanov M.S. Stupenchataya polzuchest polietilenov trubnyh marok v temperaturnom rezhime predplavleniya [Step creep of polyethylene of pipe brands in temperature mode of premelting] // Vysokomolekulyarnye soedineniya. 2016. Ser.: A. T. 58. №4. S. 1–8.
  15. Pemberton S., Chrystle-Lowe D., Rafiq S., Modelska K., Ingham E. Development of slow crack growth resistance (strain hardering) test for assessment of ageing PE pipeline materials // 17th Plastic Pipes Conference. September 22–24, 2014. Chicago. Illinoys, USA.
  16. Deblieck Rudy A.C., D.J.M. van Beek, Remerie K., Ward Ian M. Failure mechanisms in polyolefines: The role of crazing, shear yielding and the entanglement network // Polymer. 2011. V. 52. P. 2979–2990.
  17. McCarthy M., Deblieck R., Mindermann P., Kloth R., Kurelec L., Martens H. New accelerated method to determine slow crack growth behavior of polyethylene pipe materials // 14th Plastic Pipes Conference. 2008.
  18. Kurelec L., Teeuwenb M., Schoffeleersb H., Deblieck R. Strain hardening modulus as a measure of environmental stress crack resistance of high density polyethylene // Polymer. 2005. V. 46. P. 6369–6379.
  19. E. van der Stok, Scholten F. Strain hardering tests on PE pipe materials // Plastic Pipes XVI Conference. September 24–26, 2012. Barcelona, Spain.
  20. Alwis K.G.N.C., Burgoyne C.J. Accelerated creep testing for aramid fibres using the stepped isothermal method // J. Mater. Sci. 2008. V. 43. P. 4789–4800.
  21. Achereiner F., Engelsing K., Bastian M., Heidemeyer P. Accelerated creep testing of polymers using the stepped isothermal method // Polymer Testing. 2013. V. 32. P. 447–454.
  22. Hadid M., Guerira B., Bahri M., Zouani A. Assessment of the stepped isostress method in the prediction of long term creep of thermoplastics // Polymer Testing. 2014. V. 34. P. 113–119.