Zelepugin S.A., Shkoda O.A., Lepakova O.K., Zelepugin A.S., Kasatskii N.G., Shavnev A.A., Krasnov E.I. Synthesis of the Ti–TiAl3 metallic-intermetallic laminate composite by various methods // Proceedings of VIAM. 2016. No. 11 (47). Ст. 03. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2016-0-11-3-3.

Synthesis of the Ti–TiAl3 metallic-intermetallic laminate composite by various methods

Zelepugin S.A., Shkoda O.A., Lepakova O.K., Zelepugin A.S., Kasatskii N.G., Shavnev A.A., Krasnov E.I.
Abstract

In modern technology, including aircraft manufacturing, the composite materials with higher static and dynamic strength, fracture toughness compared to traditional homogeneous materials are increasingly used. Among the composite materials the laminated composite materials containing alternating layers of metal and intermetallic or ceramic are of great interest. Four methods such as thermal explosion, reactive sintering, reactive pressing and explosive welding+sintering were considered for obtaining the Ti–TiAl3 metallic-intermetallic laminate composite. The microstructure and phase composition of the samples were studied by the X-ray diffraction, local X-ray spectrum and optical microscopy methods. The study shows that the multilayered composite could be obtained by all four methods

Keywords
metallic-intermetallic laminate composite, intermetallide, titanium, aluminum, reactive sintering, pressing, thermal explosion, explosive welding.
Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Istoriya aviacionnogo materialovedeniya. VIAM – 80 let: gody i lyudi / pod obshh. red. E.N. Kablova [History of aviation materials science. VIAM – 80 years: years and people / gen. ed. by E.N. Kablov]. M.: VIAM, 2012. 520 s.
  3. Kablov E.N. Materialy i himicheskie tehnologii dlya aviacionnoj tehniki [Materials and chem-ical technologies for aviation engineering] // Vestnik Rossijskoj akademii nauk. 2012. T. 86. №6. S. 520–530.
  4. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  5. Vecchio K.S. Synthetic multifunctional metallic-intermetallic laminate composites // JOM. 2005. Vol. 57 (3). P. 25–31.
  6. Price R.D., Jiang F., Kulin R.M., Vecchio K.S. Effects of ductile phase volume fraction on the mechanical properties of Ti–TiAl3 metal-intermetallic laminate (MIL) composites // Materials Science and Engineering. 2011. Vol. A 528 (7). P. 3134–3146. DOI:10.1016/j.msea.2010.12.087.
  7. Patselov A., Greenberg B., Gladkovskii S., Lavrikov R., Borodin E. Layered metal-intermetallic composites in Ti–Al system: strength under static and dynamic load // AASRI Procedia. 2012. Vol. 3. P. 107–112. DOI: 10.1016/j.aasri.2012.11.019.
  8. Gurevich L.M., Trykov Yu.P., Pronichev D.V. i dr. Svojstva intermetallidnyh prosloek v sloistyh titano-alyuminievyh kompozitah [Properties of intermetallidny layers in layered titano-aluminum composites] // Izvestiya VolgGTU. 2009. №11 (59). S. 35–40.
  9. Zelepugin S.A., Mali V.I., Zelepugin A.S., Ilina E.V. Failure of metallic-intermetallic laminate composites under dynamic loading // Shock Compression of Condensed Matter. USA, American Institute of Physics. 2012. Vol. 1426. P. 1101–1104. DOI: 10.1063/1.3686471.
  10. Zelepugin S.A., Ilina E.V., Shpakov S.S., Lepakova O.K., Kasackij N.G., Shkoda O.A. Sintez mnogoslojnyh kompozitov i ih razrushenie pri dinamicheskom nagruzhenii [Synthesis of multi-layer composites and their destruction at dynamic loading] // Izvestiya vysshih uchebnyh zavedenij. Fizika. 2010. T. 53. №12–2. C. 161–165.
  11. Zelepugin S.A., Lepakova O.K., Kasackij N.G., Shkoda O.A. Novyj podhod k sintezu mnog-oslojnyh metallo-intermetallidnyh kompozitov [New approach to synthesis of multi-layer metallo-intermetallidny composites] // Izvestiya vysshih uchebnyh zavedenij. Fizika. 2011. T. 54. №10–2. S. 80–83.
  12. Krasnov E.I., Shtejnberg A.S., Shavnev A.A., Serpova V.M., Zhabin A.N. Issledovanie slois-togo metallicheskogo kompozicionnogo materiala sistemy Ti–TiAl3 [Research of layered metal composite material of Ti-TiAl3 system] // Fundamentalnye nauchnye osnovy sovremennyh kompleksnyh metodov issledovanij i ispytanij materialov, a takzhe elementov konstrukcij: sb. mater. molodezhnoj konferencii. M.: VIAM, 2015. S. 11.
  13. Berlin A.A., Shtejnberg A.S., Krasnov E.I., Shavnev A.A., Lomov S.B., Serpova V.M. Eksperimentalnoe issledovanie polucheniya sloistyh kompozicionnyh materialov metodom elektroteplovogo vzryva. Ocenka ostatochnyh napryazhenij [Experimental study of receipt of layer composite materials by the method of electro-thermal explosion. Аssessment of residual stresses] // Aviacionnye materialy i tehnologii. 2014. №S6. S. 5–10. DOI 10.18577/2071-9140-2014-0-s6-5-10.
  14. Krasnov E.I., Shtejnberg A.S., Shavnev A.A., Berezovskij V.V. Issledovanie sloistogo metallicheskogo kompozicionnogo materiala sistemy Ti–TiAl3 [Study of Ti–TiAl3 laminate metal composite material ] // Aviacionnye materialy i tehnologii. 2013. №3. S. 16–19.
  15. Kovtunov A.I., Myamin S.V. Issledovanie tehnologicheskih i mehanicheskih svojstv sloistyh titanoalyuminievyh kompozicionnyh materialov, poluchennyh zhidkofaznym sposobom [Study of the technological and mechanical properties of laminated titano-aluminium composite materials, produced by liquid-phase method] // Aviacionnye materialy i tehnologii. 2013. №1. S. 9–12.
  16. Pacelov A.M., Gladkovskij S.V., Lavrikov R.D., Kamancev I.S. Treshhinostojkost sloistyh kompozitov s cheredovaniem sloev TiAl3–Ti–Al–Al3Ti v usloviyah staticheskogo i ciklicheskogo nagruzheniya [Crack firmness of layered composites with alternation of layers of TiAl3-Ti-Al-Al3Ti in the conditions of static and cyclic loading] // Deformaciya i razrushenie materialov. 2014. №12. S. 7–11.
  17. Lazurenko D.V., Mali V.I., Shevtsova K.E. Structure and properties of Al–Ti multilayered composites with intermetallic layers // Applied Mechanics and Materials. 2014. Vol. 682. P. 132–137. DOI:10.4028/www.scientific.net/AMM.682.132.
  18. Zelepugin S.A., Zelepugin A.S. Failure of multilayer composites under dynamic loading // 11th World Congress on Computational Mechanics (WCCM 2014); 5th European Conference on Computational Mechanics (ECCM 2014); 6th European Conference on Computational Fluid Dynamics (ECCFD 2014). Spain, Barcelona. Int. Center for Numerical Methods in Engineering (CIMNE). 2014. Vol. 4. P. 3926–3933.
  19. Zelepugin S.A., Shpakov S.S. Razrushenie metallo-intermetallidnogo mnogoslojnogo kompozita pri vysokoskorostnom udare [Destruction of metallo-intermetallidny multi-layer composite at high-speed blow] // Mehanika kompozicionnyh materialov i konstrukcij. 2009. T. 15. №3. S. 369–382.
  20. Zelepugin S.A., Shpakov S.S. Razrushenie mnogoslojnyh metallo-intermetallidnyh kompozitov pri dinamicheskom nagruzhenii [Destruction of multi-layer metallo-intermetallidny composites at dynamic loading] // Vestnik Nizhegorodskogo un-ta im. N.I. Lobachevskogo. 2011. №4 (4). S. 1490–1492.
  21. Cao Y., Zhu S., Guo C., Vecchio K.S., Jiang F. Numerical investigation of the ballistic performance of metal-intermetallic laminate composites // Applied Composite Materials. 2015. Vol. 22. P. 437–456. DOI: 10.1007/s10443-014-9416-1.
  22. Zelepugin S.A., Zelepugin A.S. Numerical simulation of multilayer composites failure under dynamic loading // Applied Mechanics and Materials. 2015. Vol. 756. P. 408–413. DOI: 10.4028/www.scientific.net/AMM.756.408.
  23. Deribas A.A. Fizika uprochneniya i svarki vzryvom [Physics of hardening and explosion welding]. Novosibirsk: Nauka, 1972. 188 s.