Aleksandrov D.A., Artemenko N.I. Wear-resistant coatings to protect friction parts of modern gas turbine engines // Proceedings of VIAM. 2016. No. 10 (46). Ст. 06. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2016-0-10-6-6.

Wear-resistant coatings to protect friction parts of modern gas turbine engines

Aleksandrov D.A., Artemenko N.I.
Abstract

The article presents perspectives for application of wear-resistant coatings for gas turbine engine friction parts. The main directions of development of wear-resistant coatings abroad, as well as results of work on development of high wear-resistant coatings are adduced. The data on the durability, heat resistance, wear-resistant coatings metallographic studies are presented. The research is executed within the implementation of the complex scientific direction 17.3. «Multi-layer heat-resistant coatings, nanostructured strengthening erosion and corrosion-resistant, wear-resistant, anti-fretting coatings to protect parts of hot section and compressor of turbine engine and gas turbine» («The Strategic directions of development of materials and technologies of their processing for the period till 2030»)

Keywords
wear-resistant coatings, friction parts of GTE, ion-plasma coatings, ceramic coatings.
Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N., Ospennikova O.G., Bazyleva O.A. Materialy dlya vysokonagruzhennyh detalej gazoturbinnyh dvigatelej [Materials for the high-loaded details of gas turbine engines] // Vestnik MGTU im. N.E. Baumana. Ser.: Mashinostroenie. 2011. №SP2. S. 13–19.
  3. Hrushhov M.M., Marchenko E.A., Dubravina A.A., Semenov A.P. Strukturnye osobennosti almazopodobnyh pokrytij s razlichnym mehanizmom legirovaniya i ih tribologicheskie harakteristiki [Structural features of diamondlike coverings with the different mechanism of alloying and their tribological characteristics] // Fizika, himiya i mehanika tribosistem. 2011. №10. S. 147–152.
  4. Kononov D.M., Zhdanov A.A., Morozov V.V. Poluchenie i issledovanie almazopodobnyh PVD-pokrytij [Receiving and research of diamondlike PVD coverings] // Nauchno-tehnicheskij vestnik Povolzhya. 2012. №6. S. 275–278.
  5. Muratore C., Jones D.R., Voevodin A.A. Smart tribological coating with wear sensing capability // Wear. Vol. 265, Issues 5–6, P. 913–920.
  6. Voevodin A.A., Zabinski J.S. Nanocomposite and nanostructured tribological materials for space applications // Composites Science and Technology. 2005. Vol. 55. P. 741–748.
  7. Muboyadzhyan S.A., Budinovskij S.A., Gayamov A.M., Smirnov A.A. Poluchenie keramicheskih teplozashhitnyh pokrytij dlya rabochih lopatok turbin aviacionnyh GTD magnetronnym metodom [Receiving ceramic heat-protective coatings for working blades of turbines of aviation GTD magnetronny method] // Aviacionnye materialy i tehnologii. 2012. №4. S. 3–8
  8. Muboyadzhyan S.A., Pomelov Ya.A. Zashhitnye pokrytiya dlya lopatok kompressora GTD [Protecting covers for GTD compressor blades] // Aviacionnye materialy i tehnologii. M.: VIAM, 2003. Vyp.: Vysokozharoprochnye materialy dlya sovremennyh i perspektivnyh gazoturbinnyh dvigatelej i progressivnye tehnologii ih proizvodstva. S. 116–131.
  9. Kablov E.N., Muboyadzhyan S.A. Ionnoe travlenie i modificirovanie poverhnosti otvetstvennyh detalej mashin v vakuumno-dugovoj plazme [Ion etching and modifying of surface of responsible details of machines in vacuum and arc plasma] // Vestnik MGTU im. N.E. Baumana. Ser.: Mashinostroenie. 2011. №SP2. S. 149–163.
  10. Muboyadzhyan S.A., Lutsenko A.N., Aleksandrov D.A., Gorlov D.S. Issledovanie vozmozhnosti povysheniya sluzhebnyh harakteristik lopatok kompressora GTD metodom ionnogo modificirovaniya poverhnosti [Research of possibility of increase of office characteristics of compressor blades of GTD by method of ionic modifying of surface] // Aviacionnye materialy i tehnologii. M.: VIAM, 2006. №1. S. 42–53.
  11. Muboyadzhyan S.A., Aleksandrov D.A., Gorlov D.S. Ionno-plazmennye nanoslojnye erozionnostojkie pokrytiya na osnove karbidov i nitridov metallov [Ion-plasma nanolayer coverings erosion steady on the basis of carbides and nitrides of metals] // Metally. 2010. №5. S. 39–51.
  12. Muboyadzhyan S.A., Aleksandrov D.A., Gorlov D.S. Nanoslojnye uprochnyayushchie pokrytiya dlya zashhity stalnyh i titanovyh lopatok kompressora GTD [Nanolayer strengthening coverings for protection of steel and titanic compressor blades of GTE] // Aviacionnye materialy i tehnologii. 2011. №3. S. 3–8.
  13. Muboyadzhyan S.A., Lucenko A.N., Aleksandrov D.A., Gorlov D.S., Zhuravleva P.L. Issledovanie svojstv nanoslojnyh erozionnostojkih pokrytij na osnove karbidov i nitridov metallov [Research of properties of nanolayer erosion steady coverings on the basis of carbides and nitrides of metals] // Metally. 2011. №4. S. 91–101.
  14. Aleksandrov D.A., Muboyadzhyan S.A., Gorlov D.S., Konnova V.I. Povyshenie erozionnoj i korrozionnoj stojkosti stalnyh lopatok kompressora GTD s pomoshhyu nanoslojnogo pokrytiya [Increase of erosion and corrosion resistance of steel compressor blades of GTD by means of nanolayer covering] // Problemy chernoj metallurgii i materialovedeniya. 2013. №4. S. 1–7.
  15. Muboyadzhyan S.A., Aleksandrov D.A., Gorlov D.S., Egorova L.P., Bulavinceva E.E. Zashhitnye i uprochnyayushhie ionno-plazmennye pokrytiya dlya lopatok i drugih otvetstvennyh detalej kompressora GTD [Protective and strengthening ion-plasma coverings for blades and other responsible details of the GTE compressor] // Aviacionnye materialy i tehnologii. 2012. №S. S. 71–81.
  16. Belous V.Ya., Varlamova V.E., Muboyadzhyan S.A., Aleksandrov D.A. Ionno-plazmennye pokrytiya dlya zashhity ot korrozii kompressornyh lopatok i drugih detalej GTD, ekspluatiruyushhihsya vo vseklimaticheskih usloviyah [Ионно-плазменные покрытия для защиты от коррозии компрессорных лопаток и других деталей ГТД, эксплуатирующихся во все климатических условиях] // Korroziya: materialy, zashhita. 2012. №1. S. 20–24.
  17. Shchepilov A.V., Muboyadzhyan S.A., Gorlov D.S., Konnova V.I. Issledovanie vliyaniya ionno-plazmennyh pokrytij na dempfiruyushhuyu sposobnost' kompozicii «splav–pokrytie» pri ispytaniyah na vibrodinamicheskom stende [Investigation of the ion-plasma coatings influence on damping capacity of «alloy-coating» composition during testing on vibrodynamic bench] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №4. St. 08. Available at: http://www.viam-works.ru (accessed: May 04, 2016). DOI: 10.18577/2307-6046-2015-0-4-8-8.
  18. Artemenko N.I., Muboyadzhyan S.A. Inzhenernaya metodika ocenki velichiny i haraktera vnutrennih napryazhenij v odnoslojnyh uprochnyayushhih kondensirovannyh pokrytiyah [Engineering method of estimating the magnitude and nature of the internal stresses in the condensed monolayer reinforcing coatings] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №1. St. 04. Available at: http://www.viam-works.ru (accessed: May 04, 2016). DOI: 10.18577/2307-6046-2016-0-1-25-35.
  19. Artemenko N.I., Muboyadzhyan S.A., Simonov V.N., Aleksandrov D.A. Ocenka otnositelnoj iznosostojkosti ionno-plazmennyh kondensirovannyh pokrytij na splavah VT8 i EP742 [Assessment of the relative wear resistance of ion-plasma fused coatings on VT8 and EP742 alloys] // Novosti materialovedeniya. Nauka i tehnika: elektron. nauch.-tehnich. zhurn. 2015. №3. St. 09. Available at: http://www.materialsnews.ru (accessed: May 04, 2016).