Bazyleva O.A., Unchikova M.V., Turenko E.Yu., Bagetov V.V., Shestakov A.V. Study of heat treatment effect on structure, dendritic liquation parameters and time to failure of Ni3Al-based alloy containing Re // Proceedings of VIAM. 2016. No. 10 (46). Ст. 04. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2016-0-10-4-4.

Study of heat treatment effect on structure, dendritic liquation parameters and time to failure of Ni3Al-based alloy containing Re

Bazyleva O.A., Unchikova M.V., Turenko E.Yu., Bagetov V.V., Shestakov A.V.
Abstract

The influence of high temperature annealing on the microstructure, dendritic liquation parameters and time to failure of intermetallic Re-containing alloy VIN1 (VKNA-25) is investigated. It is shown that reduction of liquation due to annealing leads to rise of time to failure of Ni3Al-based intermetallic alloy. By regression analysis the correlation between time to failure and parameters of annealing is fixed. The convergence of the regression model and experimental data is <1,5%.

Keywords
intermetallic, Ni3Al compound, single crystal, long-term strength, microstructure, crystallographic orientation, time to failure, liquation, high temperature annealing.
Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N., Ospennikova O.G., Lomberg B.S. Strategicheskie napravleniya razvitiya konstrukcionnyh materialov i tehnologij ih pererabotki dlya aviacionnyh dvigatelej nastoyashhego i budushhego [The strategic directions of development of constructional materials and technologies of their processing for aircraft engines of the present and the future] // Avtomaticheskaya svarka. 2013. №10. S. 23–32.
  3. Jozwik P., Polkowski W., Bojar Z. Applications of Ni3Al Based Intermetallic Alloys – Current Stage and Potential Perceptivities // Materials. 2015. No. 8. P. 2537–2568.
  4. Nikolaev S.V. Sovmestnoe legirovanie nikelya reniem i perehodnymi metallami V–VI grupp: avtoref. dis. … k.t.n [: thesis Cand. Tech. Sci.]. M., 2014. 24 s.
  5. Bazyleva O.A., Bondarenko Yu.A., Timofeeva O.B., Chabina E.B. Intermetallidnye kompozicii na osnove Ni3Al, legirovannye reniem [Intermetallidnye of composition on the basis of Ni3Al, alloyed by reniye] // Metallurgiya mashinostroeniya. 2011. №4. S. 30–34.
  6. Kablov E.N., Petrushin N.V., Vasilenok L.B., Morozova G.I. Renij v zharoprochnyh nikelevyh splavah [Reny in heat resisting nickel alloys] // Materialovedenie. 2000. №2. S. 23–29.
  7. Bazyleva O.A., Goryunov A.V., Zagvozdkina T.N., Nefedov D.G. Issledovanie likvacionnoj neodnorodnosti splava VKNA-4U MONO i ee vliyaniya na svojstva [Research of segregation heterogenity of alloy VKNA-4U of MONO and its influence on properties] // Metallurgiya mashinostroeniya. 2012. №4. S. 18–21.
  8. Bazyleva O.A., Arginbaeva E.G. Vliyanie termicheskoj obrabotki na strukturu i zharoprochnost' renijsoderzhashhego intermetallidnogo splava na osnove nikelya [Effect of heat treatment on the structure and heat resistance rhenium containing intermetallic nickel-based alloy] // Aviacionnye materialy i tehnologii. 2014. №2. S. 21–26. DOI: 10.18577/2071-9140-2014-0-2-21-26.
  9. Bazyleva O.A., Arginbaeva E.G., Fesenko T.V., Kolodochkina V.G. Issledovanie vliyaniya likvacionnoj neodnorodnosti na strukturu i dolgovechnost' intermetallidnyh splavov na osnove nikelya [Research of influence of segregation heterogenity on structure and durability of intermetallidny alloys on the basis of nickel] // Materialovedenie. 2014. №6. S.7–12.
  10. Jóźwik P., Bojar Z. Influence of Heat Treatment on the Structure and Mechanical Properties of Ni3Al-Based Alloys // Archives of Metallurgy and Materials. 2010. Vol. 55. No. 1. P. 271–279.
  11. Li P., Li S.S., Han Y.F. Influence of solution heat treatment on microstructure and stress rupture properties of a Ni3Al base single crystal superalloy IC6SX // Intermetallics. 2011. Vol. 19. P. 182–186.
  12. Kablov D.E., Sidorov V.V., Min P.G., Puchkov Yu.A. Vliyanie lantana na kachestvo i ekspluatacionnye svojstva monokristallicheskogo zharoprochnogo nikelevogo splava ZhS36-VI [The lanthanum influence on quality and operational properties of single crystal nickel base ZhS36-VI superalloy] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №12. St. 02. Available at: http://www.viam-works.ru (accessed: May 26, 2016). DOI: 10.18577/2307-6046-2015-0-12-2-2.
  13. Rigin V.E., Sidorov V.V., Burcev V.G. Udalenie azota iz slozhnolegirovannyh rasplavov na osnove nikelya v processe ih obezuglerozhivaniya [Nitrogen removal from complex-alloyed melts based on nickel in process of decarburization] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №1. St. 02. Available at: http://www.viam-works.ru (accessed: June 07, 2016). DOI: 10.18577/2307-6046-2016-0-1-2-2.
  14. Echin A.B., Bondarenko Yu.A. Osobennosti vysokogradientnoj napravlennoj kristallizacii i sovremennoe oborudovanie, ispolzuemoe pri proizvodstve lopatok gazoturbinnyh dvigatelej [Modern equipment for turbine blades production designed with a glance of high-gradient directional crystallization process] // Trudy VIAM : electron. nauch.-tenhich. zhurn. 2014. №12. St. 03. Available at: http://viam-works.ru (accessed: June 01, 2016). DOI: 10.18577/2307-6046-2014-0-1-3-3.
  15. Povarova K.B., Drozdov A.A., Bondarenko Yu.A., Bazyleva O.A. i dr. Vliyanie napravlennoj kristallizacii na strukturu i svojstva monokristallov splava na osnove Ni3Al, legirovannogo W, Mo, Cr i RZE [Influence of the directed crystallization on structure and property of monocrystals of alloy on the basis of Ni3Al alloyed by W, Mo, Cr and RZE] // Metally. 2014. №4. S. 35–40.
  16. Novik F.S., Arsov Ya.B. Optimizaciya processov tehnologii metallov metodami planirovaniya eksperimenta [Optimization of processes of technology of metals by methods of planning of experiment]. M.: Mashinostroenie, 1980. 304 s.