Petrov A.V., Doriomedov M.S., Skripachyov S.Yu. Recycling technologies of polymer composite materials (review) // Proceedings of VIAM. 2015. No. 8. Ст. 09. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2015-0-8-9-9.

Recycling technologies of polymer composite materials (review)

Petrov A.V., Doriomedov M.S., Skripachyov S.Yu.
Abstract

A review of scientific research dealing with waste recycling of polymer composite materials is presented. A list of the companies involved in recycling is given as well. Advantages and disadvantages of the technologies used are described. Recommendations concerning recycling technologies of fiber reinforced PCM are given. The problems to be solved to implement PCM recycling technologies in Russia are described.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitija materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative development of VIAM Federal State Unitary Enterprise of GNTs Russian Federation on implementation «The strategic directions of development of materials and technologies of their processing for the period till 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] //Vse materialy. Jenciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  3. Kablov E.N., Starcev O.V., Krotov A.S., Kirillov V.N. Klimaticheskoe starenie kompozicionnyh materialov aviacionnogo naznachenija. I. Mehanizmy starenija [Climatic aging of composite materials of aviation assignment. I. Aging mechanisms] //Deformacija i razrushenie materialov. 2010. №11. S. 19–27.
  4. Kirillov V.N., Efimov V.A., Shvedkova A.K., Nikolaev E.V. Issledovanie vlijanija klimaticheskih faktorov i mehanicheskogo nagruzhenija na strukturu i mehanicheskie svojstva PKM [Research of influence of climatic factors and mechanical loading on structure and the PKM mechanical properties] //Aviacionnye materialy i tehnologii. 2011. №4 (21). S. 41–45.
  5. Kirillov V.N., Starcev O.V., Efimov V.A. Klimaticheskaja stojkost' i povrezhdaemost' polimernyh kompozicionnyh materialov, problemy i puti reshenija [Climatic firmness and damageability of polymeric composite materials, problems and solutions] //Aviacionnye materialy i tehnologii. 2012. №S. S. 412–423.
  6. Doneckij K.I., Hrul'kov A.V. Principy «zelenoj himii» v perspektivnyh tehnologijah izgotovlenija izdelij iz PKM [Principles of «green chemistry» in perspective manufacturing techniques of products from PKM] //Aviacionnye materialy i tehnologii. 2014. №S2. S. 24–28.
  7. Vlasenko F.S., Raskutin A.E. Primenenie polimernyh kompozicionnyh materialov v stroitel'nyh konstrukcijah [Application of polymeric composite materials in construction designs] //Trudy VIAM. 2013. №8. St. 03 (viam-works.ru).
  8. Pickering S.J. Recycling technologies for thermoset composite materials – current status //Composites: Part A 37. 2006. Р. 1206–1215.
  9. Borshhevskij A.A., Il'in A.S. Mehanicheskoe oborudovanie dlja proizvodstva stroitel'nyh materialov i izdelij [Mechanical equipment for production of construction materials and products]. M.: Vysshaja shkola. 1987. 366 s.
  10. Howarth J., Sada S.R., Mativenga P.T. Energy intensity and environmental analysis of mechanical recycling of carbon fibre composite //Journal of Cleaner Production. 2014. V. 81. P. 46–50.
  11. Palmer J. Mechanical Recycling of Automotive Composites for Use as Reinforcement in Thermoset Composites //University of Exeter. 2009. https://ore.exeter.ac.uk.
  12. Palmer J., Ghita O.R., Savage L., Evans K.E. Successful closed-loop recycling of thermoset composites //Composites: Part A. 2009. V. 40. P. 490–498.
  13. Keiji Ogi, Takashi Nishikawa, Yasutaka Okano & Ichiro Taketa. Mechanical properties of ABS resin reinforced with recycled CFRP //Advanced Composite Materials. 2007. V. 16. №2. P. 181–194.
  14. Conroy A., Halliwell S., Reynolds T. Composite recycling in the construction industry //Composites. Part A. 2006. V. 37. P. 1216–1222.
  15. Pinero-Hernanz R., Dodds C., Hyde J. et al. Chemical recycling of carbon fibre reinforced composites in nearcritical and supercritical water //Composites: Part A. 2008. V. 39. P. 454–461.
  16. Okajima I. et al. Chemical Recycling of Carbon Fiber Reinforced Plastic with Supercritical Alcohol //Journal of Advanced Research in Physics. 2012. V. 3. №2. P. 1–4.
  17. Pico D., Seide G., Gries T. Thermo chemical processes: potential improvement of the wind blades life cycle //Chemical Engineering Transactions. 2014. V. 36. P. 211–216.
  18. Pinero-Hernanz R., Garcıa-Serna J., Dodds C., Hydec J., Poliakoff M., Jose Cocero M., Kingman S., Pickering S., Lester E. Chemical recycling of carbon fibre composites using alcohols under subcritical and supercritical conditions //J. of Supercritical Fluids. 2008. V. 46. P. 83–92.
  19. Hitachi Chemical Technical Report №56 /Hitachi Chemical Co., Ltd. March. 2014.
  20. Elghazzaoui H., Le Gal La Salle E., Bellettre J. Recycling of aeronautical composites by supercritical solvolysis (http://www.isasf.net).
  21. Final Report Summary – EURECOMP (Recycling Thermoset Composites of the SST) (http://cordis.europa.eu).
  22. Recycling of Composite Materials using Fluidised Bed Processes (http://core.ac.uk).
  23. Recycling Fibres Recovered from Composite Materials using a Fluidised Bed Process (http://eprints.nottingham.ac.uk).
  24. Pimenta S., Pinho S.T. Recycling carbon fibre reinforced polymers for structural applications: technology review and market outlook //Waste Management. 2011. V. 31. №2. P. 378–392.
  25. Meyer L.O., Schulte K., Grove-Nielsen E. CFRP-recycling following a pyrolysis route: process optimization and potentials //Journal of Composite Materials. 2009. V. 43. P. 1121–1132.
  26. Job S. Recycling composites commercially (Part 1) //Reinforced Plastics. 2014. V. 58. №5. P. 32–34.
  27. Job S. Recycling composites commercially (Part 2) //Reinforced Plastics. 2014. V. 58. №5. P. 36–38.
  28. www.carbonxt.de.
  29. http://www.cfk-recycling.com.
  30. http://www.elgcf.com.
  31. http://mitrcf.com.
  32. http://www.emergingmit.com.
  33. http://www.reprocover.com.
  34. http://www.compocycle.com.
  35. http://en.procotex.com.
  36. http://www.refiber.com.
  37. http://extreme-ecosolutions.com.
  38. http://698.jp/cfri.
  39. http://www.ecopolycrete.com.
  40. http://www.hambleside-danelaw.co.uk.
  41. http://www.karborekrcf.it.
  42. Ustanovka dlja piroliza othodov kompozicionnyh materialov [Installation for pyrolysis of waste of composite materials]: pat. 2208203 Ros. Federacija; opubl. 10.07.2003.