Shcheglova T.M., Nikitina V.J., Lugovoy A.A. An express-method for estimation of heat treatment quality and structure of discrete fibers // Proceedings of VIAM. 2015. No. 8. Ст. 07. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2015-0-8-7-7.

An express-method for estimation of heat treatment quality and structure of discrete fibers

Shcheglova T.M., Nikitina V.J., Lugovoy A.A.
Abstract

An express-method for estimation of heat treatment quality of discrete fibers of 80% Al2O3–20%SiO2 composition and SiO2 dispersion is described in this paper.

Reference list
  1. Shhetanov B.V., Shheglova T.M., Balinova Ju.A. Izgotovlenie, struktura i svojstva polikristallicheskih volokon oksida aljuminija [Manufacturing, structure and properties of polycrystalline fibers of aluminum oxide] /V sb. materialov XXIX ezhegodnoj Mezhdunarodnoj konf. i seminara «Kompozicionnye materialy v promyshlennosti». Jalta. 2009. S. 148–150.
  2. Kablov E.N., Grashhenkov D.V., Isaeva N.V., Solncev S.S. Perspektivnye vysokotemperaturnye keramicheskie kompozicionnye materialy [Perspective high-temperature ceramic composite materials] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 20–24.
  3. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitija materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative development of VIAM Federal State Unitary Enterprise of GNTs Russian Federation on implementation «The strategic directions of development of materials and technologies of their processing for the period till 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  4. Kablov E.N., Shhetanov B.V., Abuzin Ju.A., Ivahnenko Ju.A. Metallicheskie i keramicheskie kompozicionnye materialy [Metal and ceramic composite materials] /V sb. materialov Mezhdunarodnoj nauch.-praktich. konf. «Sovremennye tehnologii – kljuchevoe zveno v vozrozhdenii otechestvennogo aviastroenija». T. 1. Kazan'. 2008. S. 181–188.
  5. Ivahnenko Ju.A., Babashov V.G., Zimichev A.M., Tinjakova E.V. Vysokotemperaturnye tep-loizoljacionnye i teplozashhitnye materialy na osnove volokon tugoplavkih soedinenij [High-temperature heatinsulating and heat-protective materials on the basis of fibers of high-melting connections] //Aviacionnye materialy i tehnologii. 2012. №S. S. 380–386.
  6. Tinjakova E.V., Grashhenkov D.V. Teploizoljacionnyj material na osnove mullito-korundovyh i kvarcevyh volokon [Heatinsulating material on the basis of mullito-korundovy and quartz fibers] //Aviacionnye materialy i tehnologii. 2012. №3. S. 43–46.
  7. Grashhenkov D.V., Balinova Ju.A., Tinjakova E.V. Keramicheskie volokna oksida aljuminija i materialy na ih osnove [Ceramic fibers of aluminum oxide and materials on their basis] //Steklo i keramika. 2012. №4. S. 32–36.
  8. Grashhenkov D.V., Shhetanov B.V., Tinjakova E.V., Shheglova T.M. O vozmozhnosti ispol'zovanija kvarcevogo volokna v kachestve svjazujushhego pri poluchenii legkovesnogo teplozashhitnogo materiala na osnove volokon Al2O3 [About possibility of use of quartz fiber as lightweight heat-protective material binding at receiving on the basis of Al2O3 fibers] //Aviacionnye materialy i tehnologii. 2011. №4. S. 8‒14.
  9. Kablov E.N., Shhetanov B.V., Ivahnenko Ju.A., Balinova Ju.A. Perspektivnye armirujushhie vysokotemperaturnye volokna dlja metallicheskih i keramicheskih kompozicionnyh materialov [Perspective reinforcing high-temperature fibers for metal and ceramic composite materials] //Trudy VIAM. 2013. №2. St. 05 (viam-works.ru)
  10. Shhetanov B.V., Ivahnenko Ju.A., Babashov V.G. Teplozashhitnye materialy [Heat-protective materials] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 12–19.
  11. Babashov V.G., Shhetanov B.V. Gibkij nizkoplotnyj vysokotemperaturnyj material na osnove mullitokorundovogo volokna [Flexible low-density high-temperature material on the basis of mullitokorundovy fiber] //Sovremennye problemy nauki i obrazovanija. 2015. №1 (www.science-education.ru).
  12. Ivahnenko Ju.A., Shheglova T.M., Judin A.V., Pshechenkov P.A. Oksidnye volokna dlja keramicheskih i metallicheskih kompozicionnyh materialov [Oksidnye of fiber for ceramic and metal composite materials] /V sb. statej Mezhdunarodnoj nauch.-tehnich. konf. «Sovremennye materialy i tehnologii–2002». Penza. 2002. S. 41–43.
  13. Shhetanov B.V., Kablov E.N., Shheglova T.M. Mehanizm formirovanija stabilizirovannoj struktury v vysokotermostojkih polikristallicheskih voloknah sistemy Al2O3–SiO2, poluchaemyh po zol'-gel' tehnologii [The mechanism of forming of the stabilized structure in the high-heat-resistant polycrystalline fibers of Al2O3–SiO2 system received on sol-gel of technology] /V sb. materialov XXIV ezhegodnoj Mezhdunarodnoj konf. i vystavki «Kompozicionnye materialy v promyshlennosti». Jalta. 2004. S. 324–326.