Kulyushina N.V., Kozlov I.A., Kutyrev A.E., Vagramyan T.A. Adhesive coatings on the basis of trial koxysilanes for aluminum and steel // Proceedings of VIAM. 2015. No. 8. Ст. 05. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2015-0-8-5-5.

Adhesive coatings on the basis of trial koxysilanes for aluminum and steel

Kulyushina N.V., Kozlov I.A., Kutyrev A.E., Vagramyan T.A.
Abstract

A more environment-saving process of formation of adhesive layers on metal surfaces in solutions of organic silicone compounds is offered as an alternative to the processes of phosphating of steels and chromating of aluminum. Trialkoxysilanes-based water compositions were developed and optimum parameters of the process of forming of organic silicone coatings on metallic surfaces were determined on the basis of experimental data. The offered processes of formation of adhesive coatings have a smaller quantity of stages of surface preparation (both aluminum alloys and steels) for the subsequent application of paint coating.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitija materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative development of VIAM Federal State Unitary Enterprise of GNTs Russian Federation on implementation «The strategic directions of development of materials and technologies of their processing for the period till 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Kablov E.N., Starcev O.V., Medvedev I.M. Obzor zarubezhnogo opyta issledovanij korrozii i sredstv zashhity ot korrozii [The overview of foreign experience of researches of corrosion and security features from corrosion] //Aviacionnye materialy i tehnologii. 2015. №2. S. 76–87.
  3. Kablov E.N. Korrozija ili zhizn' [Corrosion or life] //Nauka i zhizn'. 2012. №11. S. 16–21.
  4. Kablov E.N., Starcev O.V., Medvedev I.M., Panin S.V. Korrozionnaja agressivnost' primorskoj at-mosfery. Ch. 1. Faktory vlijanija (obzor) [Corrosion aggression of the seaside atmosphere. P.1. Factors of influence (review)] //Korrozija: materialy, zashhita. 2013. №12. S. 6–18.
  5. Semenova L.V., Malova N.E., Kuznecova V.A., Pozhoga A.A. Lakokrasochnye materialy i po-krytija [Paint and varnish materials and coverings] //Aviacionnye materialy i tehnologii. 2012. №S. S. 315–327.
  6. Karimova S.A., Pavlovskaja T.G. Razrabotka sposobov zashhity ot korrozii konstrukcij, rabotajushhih v uslovijah kosmosa [Development of ways of corrosion protection of the designs working in the conditions of space] //Trudy VIAM. 2013. №4. St. 02 (viam-works.ru).
  7. Kozlova A.A., Kondrashov Je.K. Sistemy lakokrasochnyh pokrytij dlja protivokorrozionnoj zashhity magnievyh splavov [Systems of paint coatings for anticorrosive protection of magnesium alloys] //Aviacionnye materialy i tehnologii. 2014. №2. S. 44–47.
  8. Kuznecova V.A., Kuznecov G.V. Tendencii razvitija v oblasti toplivostojkih lakokrasochnyh pokrytij dlja zashhity toplivnyh kesson-bakov letatel'nyh apparatov (obzor) [Development tendencies in the field of toplivostoyky paint coatings for protection fuel caisson tanks of flight vehicles (review)] //Trudy VIAM. 2014. №11. St.08 (viam-works.ru).
  9. Akimova E.F. Trebovanija k podgotovke poverhnosti chernyh i cvetnyh metallov pered okrashivaniem. Kontrol' kachestva podgotovki poverhnosti [Requirements to surface preparation of black and non-ferrous metals before coloring. Surface preparation quality control] /V sb. nauch. trudov «Pokrytija i obrabotka poverhnosti. Poslednie dostizhenija v tehnologijah, jekologii i oborudovanii». M.: RHTU im. D.I. Mendeleeva. 2015. S. 11–12.
  10. Kuljushina N.V., Akimova E.F., Grigorjan N.S., Vagramjan T.A., Asnis N.A. Podgotovka metallicheskoj poverhnosti s pomoshh'ju kremnijorganicheskih pokrytij [Preparation of metallic surface by means of organic silicon coverings] //Praktika protivo-korrozionnoj zashhity. 2011. №4 (62). S. 6–11.
  11. Gerald L. Witucki //Journal of coatings technology. 1993. V. 65. №822. Р. 57–60.
  12. Men'shikov V.V., Kalinkina A.A., Mazurova D.V., Akimova E.F., Vagramjan T.A. Primenenie vodnyh rastvorov na osnove silanov dlja podgotovki poverhnosti pered naneseniem lakokrasochnyh pokrytij (Obzor literaturnyh dannyh) [Application of aqueous solutions on the basis of silons for surface preparation before drawing paint coatings (The review of literary data)] //Korrozija: materialy, zashhita. 2010. №4. S. 30–37.