Pavlovskaya T.G., Kozlov I.A., Volkov I.A., Zakharov К.Е. Formation of hard wear-resistant anodic oxide coatings on parts made of casting aluminium alloys // Proceedings of VIAM. 2015. No. 8. Ст. 04. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2015-0-8-4-4.

Formation of hard wear-resistant anodic oxide coatings on parts made of casting aluminium alloys

Pavlovskaya T.G., Kozlov I.A., Volkov I.A., Zakharov К.Е.
Abstract

A possibility of formation of hard anodic oxide coatings on parts made of casting alu-minum alloys produced by die casting was investigated. A difference in the process of anodizing of parts made by casting in sand mold, in chill mold and by die casting was revealed. An influence of the chemical composition of metal parts on quality of the formed anodic oxide coating was stated. An influence of the metal structure on the process of solid anodizing was investigated.

Reference list
  1. Tarasov Ju.M., Antipov V.V. Novye materialy VIAM – dlja perspektivnoj aviacionnoj tehniki proizvodstva OAO «OAK» [The VIAM new materials – for perspective aviation engineering of production of JSC «OAK»] //Aviacionnye materialy i tehnologii. 2012. №2. S. 5–6.
  2. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitija materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative development of VIAM Federal State Unitary Enterprise of GNTs Russian Federation on implementation «The strategic directions of development of materials and technologies of their processing for the period till 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  3. Kablov E.N. Korrozija ili zhizn' [Corrosion or life] //Nauka i zhizn'. 2012. №11. S. 16–21.
  4. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] //Vse materialy. Jenciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  5. Tomashov N.D., Tjukina M.N., Zalivalov F.P. Tolstoslojnoe anodirovanie aljuminija i ego splavov [Tolstosloynoye anodizing of aluminum and its alloys]. M.: Mashinostroenie. 1968. 156 s.
  6. Lerner L. Tverdoe anodirovanie aljuminija: istorija i sovremennost' [Firm anodizing of aluminum: history and present] //Cvetnye metally. 2003. №3. S. 84–87.
  7. Goncharenko E.S., Trapeznikov A.V., Ogorodov D.V. Litejnye aljuminievye splavy (k 100-letiju so dnja rozhdenija M.B. Al'tmana) [Cast aluminum alloys (to the 100 anniversary since the birth of M. B. Altman)] //Trudy VIAM. 2014. №4. St. 02 (viam-works.ru).
  8. Fal'ko V.N., Jurkevich S.N., Poljakova T.L., Kunashenko S.V. Opyt nanesenija pokrytij na detali aviacionnoj tehniki [Experience of drawing coverings on detail of aviation engineering] //Metalloobrabotka. 2003. №6. S. 28–30.
  9. Aver'janov E.E. Spravochnik po anodirovaniju [Directory on anodizing]. M.: Mashinostroenie. 1988. 132 s.
  10. Golubev A.I. Anodnoe okislenie aljuminievyh splavov [Anode oxidation of aluminum alloys]. M.: AN SSSR. 1961. 199 s.
  11. Shrejder A.V. Oksidirovanie aljuminija i ego splavov [Oksidirovaniye of aluminum and its alloys]. M.: Metallurgizdat. 1960. 220 s.
  12. Chufistov O.E., Chufistov E.A., Artem'ev V.P. Tehnologii, stroenie i svojstva pokrytij, formiruemyh metodami anodnogo oksidirovanija na aljuminii i ego splavah [Technologies, structure and properties of the coverings created by methods of anodic oxidation on aluminum and its alloy] //Cvetnye metally. 2009. №10. S. 57–61.
  13. Semenova I.V., Florianovich G.M., Horoshilov A.V. Korrozija i zashhita ot korrozii [Corrosion and corrosion protection]: Ucheb. posobie. M.: Fizmatlit. 2010. 416 s.
  14. Korytov V.N., Haljavina M.G., Vishtaljuk A.A., Popova T.P. Tehnologija tverdogo tolstoslojnogo shhavelevosernokislotnogo anodirovanija na detaljah iz aljuminija i ego splavov [Technology of firm tolstosloyny shchavelevosernokislotny anodizing on details from aluminum and its alloys] //Vestnik Rybinskoj gosudarstvennoj aviacionnoj tehnologicheskoj akademii im. P.A. Solov'eva. 2008. №1. S. 143–144.
  15. Karimova S.A., Kutyrev A.E., Pavlovskaja T.G., Zaharov K.E. Nizkotemperaturnoe uplotnenie anodno-oksidnyh pokrytij na detaljah iz aljuminievyh splavov [Low-temperature consolidation of anode oxide coatings on details from aluminum alloys] //Aviacionnye materialy i tehnologii. 2014. №4. S. 9–17.
  16. Bordziłowski J., Królikowska A., Bonora P.L., Maconi I., Sollich A. Underwater EIS measurements //Progress in organic coatings. 2010. V. 67. №4. Р. 414–419.