Lukin V.I., Rylnikov V.S., Loshinin U.V., Nischev K.N. Low-temperature agglomeration of argentiferous paste at connection silicon with molybdenum // Proceedings of VIAM. 2015. No. 7. Ст. 04. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2015-0-7-4-4.

Low-temperature agglomeration of argentiferous paste at connection silicon with molybdenum

Lukin V.I., Rylnikov V.S., Loshinin U.V., Nischev K.N.
Abstract

The article is about investigating of heat effects taking place while drying and sintering of silver containing paste, used to get low temperature joints in system of «Si on Mo» for semiconductor elements. It was investigated the modifications in form and size of silver particles taking place during drying at different temperatures. The relationship between micro hardness of sintered layers and temperature was investigated.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitija materialov i tehnologij ih pererabotki na period do 2030 go-da» [Innovative development of VIAM Federal State Unitary Enterprise of GNTs Russian Federation on implementation «The strategic directions of development of materials and technologies of their processing for the period till 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokolenija [Nickel foundry hot strength alloys of new generation] //Aviacionnye materialy i tehnologii. 2012. №S. S. 36–51.
  3. Kablov E.N., Antipov V.V., Senatorova O.G., Lukina N.F. Novyj klass sloistyh aljumostekloplastikov na osnove aljuminijlitievogo splava 1441 s ponizhennoj plotnost'ju [New class layered alyumostekloplastikov on basis aluminum-lithium alloy 1441 with lowered density] //Vestnik MGTU im. N.Je. Baumana. 2011. №SP2. S. 174–183.
  4. Kablov E.N., Bondarenko Ju.A., Echin A.B., Surova V.A. Razvitie processa napravlennoj kristallizacii lopatok GTD iz zharoprochnyh splavov s monokristallicheskoj i kompozicionnoj strukturoj [Development of process of the directed crystallization of blades of GTD from hot strength alloys with single-crystal and composition structure] //Aviacionnye materialy i tehnologii. 2012. №1. S. 3‒8.
  5. Bazyleva O.A., Arginbaeva Je.G., Turenko E.Ju. Zharoprochnye litejnye intermetallidnye splavy [Heat resisting cast intermetallidny alloys] //Aviacionnye materialy i tehnologii. 2012. №S. S. 57–60.
  6. Petrova A.P., Lukina N.F. Klei dlja mnogorazovoj kosmicheskoj sistemy [Glues for reusable space system] //Trudy VIAM. 2013. №4. St. 04 (viam-works.ru).
  7. Lukina N.F., Dement'eva L.A., Petrova A.P., Serezhenkov A.A. Konstrukcionnye i termostojkie klei [Constructional and heat-resistant glues] //Aviacionnye materialy i tehnologii. 2012. №S. S. 328–335.
  8. Kucevich K.E., Dement'eva L.A., Lukina N.F., Chursova L.V. Svojstva i naznachenie kleja VK-36RM dlja aviacionnoj tehniki [Properties and glue assignment VK-36RM of aviation engineering] //Klei. Germetiki. Tehnologii. 2013. №8. S. 5–6.
  9. Lukina N.F., Dement’eva L.A., Serezhenkov A.A. et al. Adhesive prepregs and composite matirials on their bases //Russian J. of General Chemistry. 2011. V. 81. №5. P. 1022–1024.
  10. Lukina N.F., Dement'eva L.A., Serezhenkov A.A. i dr. Kleevye prepregi i kompozicionnye materialy na ih osnove [Glue prepregs and composite materials on their basis] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 53–56.
  11. Zhang Zhiye (Zach), Lu Guo-Quan. Pressure-Assisted Low-Temperatuze Sintering of Silver Paste as an Alternative Die-Attach Solution to Soldez Reflow //Trans. Jnd. Applicat. 2002. V. 25. №4. Р. 279–283.
  12. Lukin V.I., Ryl'nikov V.S., Afanas'ev-Hodykin A.N., Kucevich K.E., Nishhev K.N. Metod opredelenija prochnosti sceplenija serebrjanogo pokrytija s kremnievoj podlozhkoj s ispol'zovaniem kleja [Method of determination of durability of coupling of silver covering with silicon substrate with glue use] //Klei. Germetiki. Tehnologii. 2014. №6. S. 34‒36.