Istyagin S.E., Postnov V.I., Veshkin E.A Hydrothermal testing of thermal insulation panels // Proceedings of VIAM. 2015. No. 7. Ст. 12. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2015-0-7-12-12.

Hydrothermal testing of thermal insulation panels

Istyagin S.E., Postnov V.I., Veshkin E.A
Abstract

The results of studies of various thermal insulation panels made of fiberglass to communicate epoxy resin, filled with polyurethane foam (PPU). Test panels climate conducted in accordance with temperature stages. And also tried methods of nondestructive testing continuity foam filling PPU. The possibility of their use in the construction of dryers operating at temperatures up to 100°C.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitija materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative development of VIAM Federal State Unitary Enterprise of GNTs Russian Federation on implementation «The strategic directions of development of materials and technologies of their processing for the period till 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Sokolov I.I., Raskutin A.E. Ugleplastiki i stekloplastiki novogo pokolenija [Ugleplastiki and fibreglasses of new generation] //Trudy VIAM. 2013. №4. St. 09 (viam-works.ru).
  3. Timoshkov P.N., Hrul'kov A.V. Sovremennye tehnologii pererabotki polimernyh kompozicionnyh materialov, poluchaemyh metodom propitki rasplavnym svjazujushhim [Modern refining technologies of the polymeric composite materials received by method of impregnation by the molten binding] //Trudy VIAM. 2014. №8. St. 04 (viam-works.ru).
  4. Kablov E.N. Rossii nuzhny materialy novogo pokolenija [Materials of new generation are necessary to Russia] //Redkie zemli. 2014. №3. S. 8–13.
  5. Kablov E.N. Himija v aviacionnom materialovedenii [Chemistry in aviation materials science] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  6. Murashov V.V., Kosarina E.I., Generalov A.S. Kontrol' kachestva aviacionnyh detalej iz polimernyh kompozicionnyh materialov i mnogoslojnyh kleenyh konstrukcij [Quality control of aviation details from polymeric composite materials and multi-layer kleeny designs] //Aviacionnye materialy i tehnologii. 2013. №3. S. 65–70.
  7. Murashov V.V., Rumjancev A.F., Ivanova G.A., Fajzrahmanov N.G. Diagnostika struktury, sostava i svojstv polimernyh kompozicionnyh materialov [Diagnostics of structure, structure and properties of polymeric composite materials] //Aviacionnye materialy i tehnologii. 2008. №1. S. 17–24.