Kirienko O.A., Shurkova E.N., Volnyj O.S., Barbotko S.L. Assessment of fire safety of PCM at flame distribution on horizontal surface under conditions of heat flow of variable intensity // Proceedings of VIAM. 2015. No. 6. Ст. 11. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2015-0-6-11-11.

Assessment of fire safety of PCM at flame distribution on horizontal surface under conditions of heat flow of variable intensity

Kirienko O.A., Shurkova E.N., Volnyj O.S., Barbotko S.L.
Abstract

Definition of fire safety characteristics of polymer composition materials (PCM) for manufacturing of components of external components of aviation equipment (fuselage, wing, stabilizers, etc.) was carried out under conditions of variable intensity of the heat flow. Samples of glass- and carbon-reinforced polymers were chosen as test subjects. The tests were carried out in CSI-195FAA camera (Custom Scientific Instruments, USA) with the heat radiation panel. The following characteristics of fire safety were defined during the tests: duration of the residual burning, burn-out length, critical heat flow of flame damping, etc. Assessment of fire safety of glass- and carbon-reinforced polymers by the oxygen index method was additionally carried out.

Reference list
  1. Semenov V.N. Jelementy nauchno-tehnicheskogo zadela v mehanike konstrukcij perspektivnyh letatel'nyh apparatov [Elements of scientific and technical backlog in mechanics of designs of perspective flight vehicles] //Vestnik Nizhegorodskogo universiteta im. N.I. Lobachevskogo. 2011. №4 (5). S. 2482–2484.
  2. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitija materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative development of VIAM Federal State Unitary Enterprise of GNTs Russian Federation on implementation «The strategic directions of development of materials and technologies of their processing for the period till 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  3. Kablov E.N. Materialy i himicheskie tehnologii dlja aviacionnoj tehniki [Materials and chemical technologies for aviation engineering] //Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
  4. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki [Strategic directions of development of materials and technologies of their processing] /V kn. Istorija aviacionnogo materialovedenija. VIAM – 80 let: gody i ljudi; Pod obshh. red. E.N. Kablova. M.: VIAM. 2012. S. 505–509.
  5. Garashhenko A.N., Rudzinskij V.P., Kaledin V.O. Obespechenie trebuemyh pokazatelej pozharobezopasnosti konstrukcij iz polimernyh kompozicionnyh materialov s pomoshh'ju ognezashhity [Providing required indicators of fire safety of designs from polymeric composite materials with the help ognezashchity] //Izvestija JuFU. Tehnicheskie nauki. 2013. №8 (145). S. 143–149.
  6. Garashhenko A.N., Garashhenko N.A., Rudzinskij V.P., Suhanov A.V., Marahovskij S.S., Teminovskij I.V. Pozharobezopasnost' stroitel'nyh konstrukcij iz polimernyh kompozicionnyh materialov [Fire safety of construction designs from polymeric composite materials] //Konstrukcii iz kompozicionnyh materialov. 2010. №2. S. 45–59.
  7. Shurkova E.N., Vol'nyj O.S., Izotova T.F., Barbot'ko S.L. Issledovanie vozmozhnosti snizhenija teplovydelenija pri gorenii kompozicionnogo materiala putem izmenenija ego struktury [Research of possibility of decrease in heat release when burning composite material by change of its structure] //Aviacionnye materialy i tehnologii. 2012. №1. S. 27–30.
  8. Barbot'ko S.L., Aseeva R.M., Serkov B.B., Sivenkov A.B., Kruglov E.Ju. Ob opredelenii teplot sgoranija i teplovydelenija pri gorenii polimernyh materialov [About determination of combustion heats and heat release when burning polymeric materials] //Pozharovzryvobezopasnost'. 2012. T. 21. №5. S. 25–32.
  9. Zubkova N.S. Polimernye materialy ponizhennoj pozharnoj opasnosti [Polymeric materials of the lowered fire danger]. M.: MGTU im. A.N. Kosygina. 2004. S. 3–9.
  10. Barbot'ko S.L., Shurkova E.N. O pozharnoj bezopasnosti materialov, ispol'zuemyh dlja izgotovlenija vneshnego kontura samoletov [About fire safety of the materials used for manufacturing of external circuit of airplanes] //Pozharovzryvobezopasnost'. 2011. T. 20. №10. S. 19–24.
  11. Barbot'ko S.L., Barbot'ko M.S., Vol'nyj O.S., Postnov V.I. Vlijanie dlitel'nogo teplovogo vozdejstvija na pozharobezopasnost' polimernyh materialov [Influence of long thermal influence on fire safety of polymeric materials] //Pozharovzryvobezopasnost'. 2014. T. 23. №1. S. 12–20.
  12. Barbot'ko S.L., Shvec N.I., Zastrogina O.B., Izotova T.F. Issledovanie vlijanija tolshhiny stekloplastikov na harakteristiki teplovydelenija pri gorenii [Research of influence of thickness of fibreglasses on heat release characteristics when burning] //Pozharovzryvobezopasnost'. 2013. T. 22. №7. S. 30–36.
  13. Barbot'ko S.L., Shurkova E.N., Vol'nyj O.S., Skryljov N.S. Ocenka pozharnoj bezopasnosti polimernyh kompozicionnyh materialov dlja vneshnego kontura aviacionnoj tehniki [Assessment of fire safety of polymeric composite materials for external circuit of aviation engineering] //Aviacionnye materialy i tehnologii. 2013. №1. S. 56–59.
  14. Kirienko O.A., Shurkova E.N., Vol'nyj O.S., Barbot'ko S.L. Issledovanie vlijanija razlichnyh zashhitnyh pokrytij na harakteristiki pozharnoj bezopasnosti teplovoj akusticheskoj izoljacii fjuzeljazha [Research of influence of different protecting covers on characteristics of fire safety of thermal acoustic insulation of fuselage] //Trudy VIAM. 2014. №10. St. 07 (viam-works.ru).
  15. Skryljov N.S., Vol'nyj O.S., Postnov V.I., Barbot'ko S.L. Issledovanie vlijanija teplovyh faktorov klimata na izmenenie harakteristik pozharobezopasnosti polimernyh kompozicionnyh materialov [Research of influence of thermal factors of climate on change of characteristics of fire safety of polymeric composite materials] //Trudy VIAM. 2013. №9. St. 05 (viam-works.ru).
  16. Barbot'ko S.L., Vol'nyj O.S., Kirienko O.A., Lucenko A.N., Shurkova E.N. Sopostavlenie metodov ocenki pozharnoj opasnosti polimernyh materialov v razlichnyh otrasljah transporta i promyshlennosti [Comparison of methods of assessment of fire danger of polymeric materials in the different industries of transport and the industry] //Vse materialy. Jenciklopedicheskij spravochnik. 2015. №1. S. 2–9.