Abstract

The physical, mechanical and thermo-physical properties of the domestic foamed elastic VPP-1 and rigid plate-type VPP-5 polymer materials produced to substitute the foreign foamed elastic «Solimide» (USA) and rigid plate-type «Rohacell» (Germany) polyimide materials are described in the article. Properties of the domestic foamed VPP-1 and VPP-5 polyimide materials are compared with foreign foamed polyimide analogue materials. The description of the manufacturing method for the foamed polyimide test specimens on the foamed polymeric materials mechanical treatment equipment developed in VIAM is provided. The recommendations on application of the domestic foamed polyimide materials VPP-1 and VPP-5 are given as well.

Reference list
  1. Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials – basis of innovative modernization of Russia] //Metally Evrazii. 2012. №3. S. 10–15.
  2. Kablov E.N. Himija v aviacionnom materialovedenii [Chemistry in aviation materials science] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  3. Kablov E.N. Razrabotki VIAM dlja gazoturbinnyh dvigatelej i ustanovok [Development of VIAM for gas turbine engines and installations] //Kryl'ja Rodiny. 2010. №4. S. 31–33.
  4. Bejder Je.Ja., Petrova G.N., Izotova T.F., Barbot'ko S.L. Stekloplastiki na termoplastichnoj matrice [Fibreglasses on thermoflexible matrix] //Trudy VIAM. 2013. №7. St. 03 (viam-works.ru).
  5. Stoljankov Ju.V., Ishodzhanova I.V., Antjufeeva N.V. K voprosu o defektah obrazcov dlja ispytanij ugleplastikov [To question of defects of test pieces ugleplastikov] //Trudy VIAM. 2014. №10. St. 10 (viam-works.ru).
  6. Doroshenko N.I., Chursova L.V. Jevoljucija materialov dlja lopastej vertoletov [Evolution of materials for blades of helicopters] //Aviacionnye materialy i tehnologii. 2012. №2. S. 16–18.
  7. Petrova G.N., Rumjanceva T.V., Bejder Je.Ja. Vlijanie modificirujushhih dobavok na pozharobezopasnye svojstva i tehnologichnost' polikarbonata [Influence of modifying additives on fireproof properties and technological effectiveness of polycarbonate] //Trudy VIAM. 2013 №6. St. 06 (viam-works.ru).
  8. Dobrohotova M.L. i dr. Poliimidy [Polyimide]: Spravochnik po plasticheskim massam. M.: Himija. 1969. S. 317–325.
  9. PMI – peny s iskljuchitel'nymi harakteristikami [PMI – foams with exclusive characteristics] //Plastiks. 2007. №10. S. 1–2.
  10. Krut'ko Je.T., Prokopchuk N.R. Perspektivnye puti sozdanija novyh termostojkih materia-lov na osnove poliimidov [Perspective ways of creation of new heat-resistant materials on the basis of polyimide] //Trudy BGTU. 2013. №4. Himija, tehnologija organicheskih veshhestv i biotehnologii. S. 145–149.
  11. Mihajlin Ju.A. Termoustojchivye polimery i polimernye materialy [Thermosteady polymers and polymeric materials]. SPb.: Professija. 2006. 623 s.
  12. Kornienko P.V., Shirshin K.V. i dr. Poluchenie vspenennyh poliimidnyh materialov na osnove akrilonitrila i metakrilovoj kisloty [Receiving frothed polyimide materials on basis akrilonitrila and methacrylic acid] //Plasticheskie massy. 2013. №6. S. 4–17.
  13. Berlin A.A., Shutov F.A. Himija i tehnologija gazonapolnennyh vysokopolimerov [Chemistry and technology of gas-filled high polymers]. M.: Nauka. 1980. 504 s.
  14. Bejder Je.Ja., Gureeva E.V., Petrova G.N. Penopoliimidy [Penopoliimidy] //Vse materialy. Jenciklopediche-skij spravochnik. 2012. №6. S. 2–8.
  15. Bejder Je.Ja., Petrova G.N., Izotova T.F., Gureeva E.V. Kompozicionnye termoplastichnye materialy i penopoliimidy [Composite thermoflexible materials and penopoliimidy] //Trudy VIAM. 2013. №11. St. 01 (viam-works.ru).
  16. Stoljankov Ju.V., Bejder Je.Ja., Platonov M.M., Petrova G.N. Ustrojstvo dlja mehanicheskoj obrabotki vspenennyh polimernyh materialov [The device for machining of frothed polymeric materials] //Trudy VIAM. 2015 (v pechati).
  17. Ustrojstvo dlja mehanicheskoj obrabotki vspenennyh polimernyh materialov [The device for machining of frothed polymeric materials]: pat. №145916. Ros. Federacija; opubl. 27.09.2014.