Kosmin A.A., Budinovskiy S.A., Matveev P.V., Smirnov A.A. Research of sulfide-oxide corrosion resistance of ZhS36 nickel superalloy with different types of ion-plasma coatings in temperature range 850–900°С // Proceedings of VIAM. 2015. No. 12. Ст. 05. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2015-0-12-5-5.

Research of sulfide-oxide corrosion resistance of ZhS36 nickel superalloy with different types of ion-plasma coatings in temperature range 850–900°С

Kosmin A.A., Budinovskiy S.A., Matveev P.V., Smirnov A.A.
Abstract

Comparative research of sulfide-oxide corrosion resistance of ZhS36 nickel superalloy with different advanced protective ion-plasma coatings is conducted. Results of accelerated comparative research method («salt shell method») tests of ZhS36 nickel superalloy with advanced protective ion-plasma coatings in comparison with standard SDP-6 coating in temperature range 850–900°С are presented.

Keywords
heat-resistant and ion-plasma coatings, ion-plasma technology, heat-resistance, superalloy protection, coatings for turbin blades
Reference list
  1. Inozemtsev A.A., Nihamkin M.A., Sandrackij V.L. Osnovy konstruirovanija aviacionnyh dvigatelej i jenergeticheskih ustanovok [Bases of designing of aircraft engines and energy units]. M.: Mashinostroenie. 2008. T. 2. S. 159–192.
  2. Kablov E.N., Sidorov V.V., Kablov D.E., Rigin V.E., Goryunov A.V. Sovremennye tehnologii polucheniya prutkovyh zagotovok iz litejnyh zharoprochnyh splavov novogo pokoleniya [Modern technologies of receiving the bar stock preparations from foundry heat resisting alloys of new generation] //Aviacionnye materialy i tehnologii. 2012. №S. S. 97–105.
  3. Kablov E.N., Svetlov I.L., Petrushin N.V. Nikelevye zharoprochnye splavy dlja litYa lopatok s napravlennoj i monokristallicheskoj strukturoj. Ch. ΙΙ [Nickel hot strength alloys for molding of blades with the directed and single-crystal structure. P. ΙΙ] //Materialovedenie. 1997. №5. S. 14–16.
  4. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokoleniya [Nickel foundry heat resisting alloys of new generation] //Aviacionnye materialy i tehnologii. 2012. №S. C. 36–52.
  5. Kablov E.N., Svetlov I.L., Petrushin N.V. Nikelevye zharoprochnye splavy dlya litya lopatok s napravlennoj i monokristallicheskoj strukturoj. Ch. Ι [Nickel hot strength alloys for molding of blades with the directed and single-crystal structure. P. Ι] //Materialovedenie. 1997. №4. S. 32–39.
  6. Kablov E.N., Bondarenko Yu.A., Echin A.B., Surova V.A., Kablov D.E. Razvitie processa napravlennoj kristallizatsii lopatok GTD iz zharoprochnyh i intermetallidnyh splavov s monokristallicheskoj strukturoj [Development of process of the directed crystallization of blades of GTE from heat resisting and intermetallic alloys with single-crystal structure] //Vestnik MGTU im. N.E. Baumana. Ser. «Mashinostroenie». 2011. №SP4. S. 20–25.
  7. Zharoprochnyj splav na nikelevoj osnove dlya monokristallicheskogo litya [Heat resisting alloy on nickel basis for single-crystal molding]: pat. 2439184 Ros. Federatsiya; opubl. 05.10.2010.
  8. Kablov E.N., Startsev O.V., Medvedev I.M., Panin S.V. Korrozionnaya agressivnost primorskoj atmosfery. Ch. 1. Faktory vliyaniya (obzor) [Corrosion aggression of the seaside atmosphere. P.1. Factors of influence (overview)] //Korroziya: materialy, zashhita. 2013. №12. S. 6–18.
  9. Kablov E.N., Ospennikova O.G., Bazyleva O.A. Materialy dlya vysokoteplonagruzhennyh detalej gazoturbinnyh dvigatelej [Materials for the high-heatloaded details of gas turbine engines] //Vestnik MGTU im. N.E. Baumana. Ser. «Mashinostroenie». 2011. №SP4. S. 13–19.
  10. Kablov E.N., Muboyadzhyan S.A. Zharostojkie i teplozashhitnye pokrytiya dlya lopatok turbiny vysokogo davleniya perspektivnyh GTD [Heat resisting and heat-protective coverings for turbine blades of high pressure of perspective GTE] //Aviacionnye materialy i tehnologii. 2012. №S. S. 60–70.
  11. Kablov E.N., Muboyadzhyan S.A., Budinovskij S.A., Pomelov Ya.A. Ionno-plazmennye zashhitnye pokrytiya dlya lopatok gazoturbinnyh dvigatelej [Ion-plasma protecting covers for blades of gas turbine engines] //Konversiya v mashinostroenii. 1999. №2. S. 42–47.
  12. Matveev P.V., Budinovskij S.A. Issledovanie svojstv zashhitnyh zharostojkih pokrytij dlya intermetallidnyh nikelevyh splavov tipa VKNA dlya rabochih temperatur do 1300°C [Research of the properties of protective heat-resistant coating for intermetallic nickel alloys operating at temperatures up to 1300°C] //Aviacionnye materialy i tehnologii. 2014. №3. S. 22–26.
  13. Kablov E.N., Muboyadzhyan S.A. Ionnoe travlenie i modificirovanie poverhnosti otvetstvennyh detalej mashin v vakuumno-dugovoj plazme [Ion etching and modifying of surface of responsible details of machines in vacuum and arc plasma] //Vestnik MGTU im. N.E. Baumana. Ser. «Mashinostroenie». 2011. №SP2. S. 149–163.
  14. Kablov E.N., Muboyadzhyan S.A. Heat-resistant coatings for the high-pressure turbine blades of promising GTES //Russian metallurgy (Metally). 2012. V. 2012. №1. P. 1–7.
  15. Matveev P.V., Budinovskij S.A., Muboyadzhyan S.A., Kosmin A.A. Zashhitnye zharostojkie pokrytiya dlya splavov na osnove intermetallidov nikelya [High-temperature coatings for intermetallic nickel-based alloys] //Aviacionnye materialy i tehnologii. 2013. №2. S. 12–15.
  16. Muboyadzhyan S.A., Aleksandrov D.A., Gorlov D.S., Egorova L.P., Bulavinceva E.E. Zashhitnye i uprochnyayushhie ionno-plazmennye pokrytiya dlya lopatok i drugih otvetstvennyh detalej kompressora GTD [Protective and strengthening ion-plasma coverings for blades and other responsible details of the GTE compressor] //Aviacionnye materialy i tehnologii. 2012. №S. S. 71–81.