Bazyleva O.A., Arginbaeva E.G., Shestakov A.V., Koljadov E.V. Micro-structural parameters and mechanical properties of intermetallic nickel alloy cast by directional solidification // Proceedings of VIAM. 2015. No. 12. Ст. 01. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2015-0-12-1-1.

Micro-structural parameters and mechanical properties of intermetallic nickel alloy cast by directional solidification

Bazyleva O.A., Arginbaeva E.G., Shestakov A.V., Koljadov E.V.
Abstract

The investigations of directional solidification parameters (rate and temperature gradient of crystallization) on microstructure, structural and phase parameters (lattices parameters of γꞌ- and γ-phases, misfit) and mechanical properties of intermetallic VIN alloys based on nickel were considered.

Keywords
intermetallic Ni3Al, directional solidification, a single crystal, the temperature gradient crystallization, rate of crystallization, the structure, lattice parameter, lattice misfit, temperature strength.
Reference list
  1. Stroganov G.B., Logunov A.V., Gerasimov V.V. i dr. Vysokoskorostnaya napravlennaya kristallizatsiya [The high-speed directed crystallization] //Litejnoe proizvodstvo. 1983. №12. S. 20–22.
  2. Gerasimov V.V., Visik E.M. Tehnologicheskie aspekty litya detalej goryachego trakta GTD iz intermetallidnyh nikelevyh splavov tipa VKNA s monokristallicheskoj strukturoj [Technological aspects of molding of details of hot path of GTE from intermetallic nickel alloys of VKNA type with single-crystal structure] //Litejshhik Rossii. 2012. №2. S. 19–23.
  3. Kablov E.N., Gerasimov V.V., Visik E.M., Demonis I.M. Rol napravlennoj kristallizatsii v resursosberegayushchej tehnologii proizvodstva detalej GTD [Role of the directed crystallization in the resource-saving production technology of details of GTE] //Trudy VIAM. 2013. №3. St. 01 (viam-works.ru).
  4. Kablov E.N., Bondarenko Yu.A., Echin A.B., Surova V.A. Razvitie protsessa napravlennoj kristallizacii lopatok GTD iz zharoprochnyh splavov s monokristallicheskoj i kompozicionnoj strukturoj [Development of process of the directed crystallization of blades of GTE from hot strength alloys with single-crystal and composition structure] //Aviacionnye materialy i tehnologii. 2012. №1. S. 3–8.
  5. Echin A.B., Bondarenko Yu.A. Novaya promyshlennaya vysokogradientnaya ustanovka UVNS-6 dlya polucheniya lopatok i drugih detalej GTD iz litejnyh zharoprochnyh i intermetallidnyh splavov s monokristallicheskoj strukturoj [New industrial high-gradient UVNS-6 for manufacture of GTE blades and other parts from casting heat-resistant and intermetallic alloys with single-crystal structure] //Aviacionnye materialy i tehnologii. 2014. №4. S. 31–36.
  6. Petrushin N.V., Ignatova I.A., Logunov A.V., Samojlov A.I., Razumovskij I.M. Issledovanie vliyaniya razmernogo nesootvetstviya periodov reshetok γ- i γʹ-faz na harakteristiki zharoprochnosti dispersionno-tverdejushhih nikelevyh splavov [Research of influence of dimensional discrepancy of the periods of grids γ- and γʹ-phases on characteristics of thermal stability of age-hardening nickel alloys] //Metally. 1981. №6. S. 153–159.
  7. Nazarkin R.M. Rentgenovskij analiz splavov na osnove intermetallida Ni3Al [The x-ray analysis of alloys on the basis of Ni3Al intermetallic compound] /V sb. dokladov VI Vserossijskoj ezhegodnoj konf. molodyh nauch. sotrudnikov i aspirantov. M.: IMET RAN. 2009. S. 59–62.
  8. Bazyleva O.A., Arginbaeva E.G., Turenko E.Yu. Zharoprochnye litejnye intermetallidnye splavy [Heat resisting cast intermetallic alloys] //Aviacionnye materialy i tehnologii. 2012. №S. S. 57–60.
  9. Povarova K.B., Bazyleva O.A., Drozdov A.A., Kazanskaya N.K., Morozov A.E. Samsonova M.A. Konstrukcionnye zharoprochnye splavy na osnove Ni3Al: poluchenie, struktura i svojstva [Constructional hot strength alloys on the basis of Ni3Al: receiving, structure and properties] //Materialovedenie. 2011. №4. S. 39–48.
  10. Povarova K.B., Drozdov A.A., Bondarenko Yu.A., Bazyleva O.A., Bulahtina M.A., Morozov A.E., Antonova A.V. Vliyanie napravlennoj kristallizacii na strukturu i svojstva monokristallov splava na osnove Ni3Al, legirovannogo W, Mo, Cr i RZE [Influence of the directed crystallization on structure and property of monocrystals of alloy on the basis of Ni3Al alloyed by W, Mo, Cr and REE] //Metally. 2014. №4. S. 35–41.
  11. Kablov E.N., Buntushkin V.P., Povarova K.B., Bazyleva O.A., Morozova G.I., Kazanskaya N.K. Malolegirovannye legkie zharoprochnye vysokotemperaturnye materialy na osnove intermetallida Ni3Al [The low-alloyed easy heat resisting high-temperature materials on the basis of Ni3Al intermetallic compound] //Metally. 1999. №1. S. 58–65.
  12. Buntushkin V.P., Kablov E.N., Bazyleva O.A., Morozova G.I. Splavy na osnove alyuminidov nikelya [Alloys on the basis of nickel aluminides] //MiTOM. 1999. №1. S. 32–34.
  13. Goryunov A.V., Rigin V.E. Sovremennaya tehnologiya polucheniya litejnyh zharoprochnyh nikelevyh splavov [The modern technology of cast nickel base superalloys production] //Aviacionnye materialy i tehnologii. 2014. №2. S. 3–7.
  14. Kablov E.N., Sidorov V.V., Kablov D.E., Rigin V.E., Goryunov A.V. Sovremennye tehnologii polucheniya prutkovyh zagotovok iz litejnyh zharoprochnyh splavov novogo pokoleniya [Modern technologies of receiving the bar stock preparations from foundry heat resisting alloys of new generation] //Aviacionnye materialy i tehnologii. 2012. №S. S. 97–105.
  15. Samojlov A.I., Nazarkin R.M., Moiseeva N.S. Opredelenie misfita vo fragmentirovannyh monokristallah nikelevyh zharoprochnyh splavov [Definition miss-fit in fragmented mono-crystals of nickel hot strength alloys] //Trudy VIAM. 2013. №5. St. 02 (viam-works.ru).
  16. Samojlov A.I., Kablov E.N., Petrushin N.V. i dr. Razmernoe nesootvetstvie kristallicheskih reshetok γ i γʹ-faz v nikelevyh renijsoderzhashhih zharoprochnyh splavah [Dimensional discrepancy of crystal lattices γ- and γʹ-phases in nickel reny containing hot strength alloys] /V sb. Aviacionnye materialy i tehnologii. Vyp. «Vysokorenievye zharoprochnye splavy, tehnologija i oborudovanie dlja proizvodstva splavov i lit'ja monokristallicheskih turbinnyh lopatok GTD». M.: VIAM. 2004. S. 48–57.
  17. Litye lopatki gazoturbinnyh dvigatelej: splavy, tehnologii, pokrytiya [Cast blades of gas turbine engines: alloys, technologies, coverings] /Pod obshh. red. E.N. Kablova. 2-e izd. M.: Nauka. 2006. 632 s.
  18. Grankin S.S., Sverdlov V.Ya. Issledovanie gradienta temperatury na fronte kristallizatsii monokristallicheskih Ni–W-splavov [Temperature gradient research at the front crystallization of single-crystal Ni – W-alloys] //Voprosy atomnoj nauki i tehniki. Ser. Vakuum, chistye materialy, sverhprovodniki. 2008. T. 17. №1. S. 162–165.