Chaynikova A.S., Vaganova M.L., Shchegoleva N.E., Lebedeva Yu.E. Technological aspects of fabrication of radiotransparent glass-ceramic materials based on high-temperature aluminosilicate systems (review) // Proceedings of VIAM. 2015. No. 11. Ст. 04. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2015-0-11-4-4.

Technological aspects of fabrication of radiotransparent glass-ceramic materials based on high-temperature aluminosilicate systems (review)

Chaynikova A.S., Vaganova M.L., Shchegoleva N.E., Lebedeva Yu.E.
Abstract

An analysis of state-of-art technology solutions in the area of radiotransparent glass-ceramic materials based on aluminosilicate systems was made. The development of glass-ceramic materials fabrication methods was overviewed from glass to ceramic technology. It was shown that direct controlled crystallisation performance provides fabrication of materials with unique combination of physical-mechanical, thermophysical and functional properties. The examples of sol-gel fabrication of aluminosilicate ceramics were given. Advantages and disadvantages of different technological methods used for radiotransparent pyrocerams fabrication were discussed. Technological problems of creating complex constructions made of radiotransparent pyrocerams were overviewed.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Kablov E.N., Grashhenkov D.V., Isaeva N.V., Solncev S.S. Perspektivnye vysokotemperaturnye keramicheskie kompozicionnye materialy [Perspective high-temperature ceramic composite materials] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 20–24.
  3. Kablov E.N., Shhetanov B.V., Ivahnenko Ju.A., Balinova Ju.A. Perspektivnye armirujushhie vysokotemperaturnye volokna dlya metallicheskih i keramicheskih kompozicionnyh materialov [The perspective reinforcing high-temperature fibers for metal and ceramic composite materials] //Trudy VIAM. 2013. №2. St. 05 (viam-works.ru).
  4. Kablov E.N., Gerasimov V.V., Visik E.M., Demonis I.M. Rol napravlennoj kristallizacii v resursosberegajushhej tehnologii proizvodstva detalej GTD [Role of the directed crystallization in the resource-saving production technology of details of GTE] //Trudy VIAM. 2013. №3. St. 01 (viam-works.ru).
  5. Uvarova N.E., Grashhenkov D.V., Isaeva N.V., Orlova L.A., Sarkisov P.D. Vysokotemperaturnye radioprozrachnye materialy: segodnya i zavtra [High-temperature radiotransparent materials: today and tomorrow] //Aviacionnye materialy i tehnologii. 2010. №1. S. 16–21.
  6. Kablov E.N., Grashhenkov D.V., Isaeva N.V., Solncev S.S., Sevastyanov V.G. Vysokotemperaturnye konstrukcionnye kompozicionnye materialy na osnove stekla i keramiki dlya perspektivnyh izdelij aviacionnoj tehniki [High-temperature constructional composite materials on the basis of glass and ceramics for perspective products of the aircraft equipment] //Steklo i keramika. 2012. №4. S. 7–11.
  7. Corning U.S., Zanotto E.D. A Bright future for glass-ceramics //American ceramic society bulletin. 2010. V. 89. №8. P. 19–27.
  8. Suzdaltsev E.I. Radio transparent, heat-resistant materials for the 21th century //Refractories and Industrial Ceramics. 2002. V. 43. №3–4. Р. 103–110.
  9. Radioprozrachnyj steklokristallicheskij material dlya aviacionnoj tehniki [Radiotransparent glass crystal material for the aircraft equipment]: pat. 2440936 Ros. Federaciya; opubl. 27.01.2012.
  10. Method of making ceramics and product thereof: pat. 2920971 US; publ. 12.01.1960.
  11. Sposob izgotovleniya antennogo obtekatelya iz steklokeramiki lithium aluminiumo silicat sostava [Way of production of an antenna fairing from glass ceramics of lithium aluminosilicate structure]: pat. 2326094 Ros. Federaciya; opubl. 10.06.2008.
  12. Refractory glass ceramics: pat. 7867932 US; publ. 05.03.2009.
  13. Suzdaltsev E.I., Zaichuk N.V., Rozhkova T.I. The Waste Used in the Production of Glass Ceramics of Lithium Alumina-silicate Composition //Refractories and Industrial Ceramics. 2003. V. 44. №4. P. 273–276.
  14. Suzdaltsev E.I., Kharitonov D.V. Intensified Sintering of Lithium Aluminosilicate Ceramics //Refractories and Industrial Ceramics. 2004. V. 45. №2. P. 88–90.
  15. Solovev V.I., Ahlestin E.S., Sysoev E.R., Tryapkin A.A. Perspektivy razvitiya poroshkovoj tehnologii sitallov [Prospects of development of powder technology of sitall] //Steklo i keramika. 1992. №3. S. 12–14.
  16. Sintered cordierite glass-ceramic bodies: pat. 8394732 US; pabl. 12.03.2013.
  17. Suzdalcev E.I., Haritonov D.V., Dmitriev A.V. Sostojanie rabot v oblasti sinteza radioprozrachnyh materialov i perspektivy sozdanija novyh kompozicij s uluchshennymi radiotehnicheskimi harakteristikami [Condition of works in the field of synthesis of radiotransparent materials and prospect of creation of new compositions with the improved radio engineering characteristics] //Konstrukcii iz kompozicionnyh materialov. 2008. №2. S. 45–54.
  18. Sarkisov P.D., Grashhenkov D.V., Orlova L.A., Uvarova N.E., Popovich N.V. Sovremennye dostizheniya v oblasti sozdaniya vysokotemperaturnyh radioprozrachnyh materialov [Modern achievements in the field of creation of high-temperature radiotransparent materials] //Tehnika i tehnologiya silikatov. 2009. T. 16. №1. S. 2–10.
  19. Chanikova A.S., Voropaeva M.V., Alekseeva L.A., Orlova L.A., Samsonov V.I. Sovremennoe sostoyanie razrabotok v oblasti radioprozrachnyh kordieritovyh sitallov (obzor) [Current state of developments in the field of radio transparent cordierite glass-ceramic (review)] //Aviacionnye materialy i tehnologii. 2014. №S6. S. 45–51.
  20. Keramicheskij material [Ceramic material]: pat. 540844 Ros. Federaciya; opubl. 30.12.1976.
  21. Sposob polucheniya keramiki iz kvarcevogo stekla [Way of receiving ceramics from quartz glass]: pat. 614073 SSSR; opubl. 05.07.1978.
  22. Suzdaltsev E.I. Glass Ceramics of β-Spodumene Composition with Controlled Dielectric Constant //Refractories and Industrial Ceramics. 2002. V. 43. №5–6. Р. 176–178.
  23. Suzdaltsev E.I., Rozhkova T.I. Materials with Controlled Dielectric Constants Based on a Glass Ceramic of Lithium Alumina-silicate Composition //Refractories and Industrial Ceramics. 2003. V. 44. №4. P. 260–262.
  24. Shamsudin Z., Hodzic A., Soutis C., Hand R.J., Hayes S.A., Bond I.P. Characterization of Thermo-mechanical Properties of MgO–Al2O3–SiO2 Glass Ceramic with Different Heat Treatment Temperatures //Journal of Materials Science. 2011. V. 46. №17. P. 5822–5829.
  25. Patzig C., Höche T., Hu Y., Ikeno H., Krause M., Dittmer M., Gawronski A., Rüssel C., Tanaka I., Henderson G.S. Zr coordination change during crystallization of MgO–Al2O3–SiO2–ZrO2 glass ceramics //Journal of Non-Crystalline Solids. 2014. №384. Р. 47–54.
  26. Fernandes H.R., Tulyaganov D.U., Ferreira J.M.F. The role of P2O5, TiO2 and ZrO2 as nucleating agents on microstructure and crystallization behavior of lithium disilicate-based glass //Journal of materials science. 2013. №48. Р. 765–773.
  27. Yun Mo Sung, Jong-Sub Lee, Kee-Chun Shin. The role of precursor nuclei in the crystallization of aluminosilicate glasses //Journal of materials science letters. 2000. V. 19. P. 675–677.
  28. Shabanova G.N., Taranenkova V.V., Korogodskaya A.N., Khristich E.V. Structure of the
  29. BaO–Al2O3–SiO2 system (review) //Glass and Ceramics. 2003. V. 60. №1–2. P. 43–46.
  30. Orlova L.A., Popovich N.V., Uvarova N.E., Poleari A., Sarkisov P.D. High-temperature Resistant Glass-ceramics Based on Sr-anorthite and Tialite Phases //Ceramics International. 2012. V. 38. №8. P. 6629–6634.
  31. Sigaev V.N. Kafedre himicheskoj tehnologii stekla i sitallov 80 let: yunost umeet – zrelost mozhet [To chair of chemical technology of glass and sitall of 80 years: youth is able – the maturity can] //Steklo i keramika. 2013. №4. S. 6–13.
  32. Sarkisov P.D., Orlova L.A., Popovich N.V., Brunch R., Chajnikova A.S., Klinkmyuller K., Shchegoleva N.E. Processy spekaniya i kristallizacii pri poluchenii stronciyanortitovoj steklokeramiki [Processes of agglomeration and crystallization when receiving strontianite glass ceramics] //Steklo i keramika. 2012. №8. S. 14–16.
  33. Ceramic material: pat. 5642868 US; publ. 01.07.1997.
  34. Bansal N.P., Hyatt M.J. Crystallization and Properties of Sr–Ba Aluminosilicate Glass-Ceramic Matrices /In: NASA Technical memorandum 10764 Prepared for the 15th Annual Conference on Composites and Advanced Ceramics sponsored by the American Ceramiс Society. Cocoa Beach, Florida. 1991.
  35. Yun Mo Sung, Woo Chul Kwak. Influence of Various Heating Procedures on the Sintered Density of Sr-celsian Glass-ceramic //Journal of Materials Science Letters. 2002. V. 21. №11. P. 841–843.
  36. Yun Mo Sung. Monocelsian formation in the SrO–Al2O3–2SiO2 glass //Journal of Materials Science Letters. 2000. V. 19. P. 453–454.
  37. Yun Mo Sung. Crystallization characteristics of SrO–Al2O3–SiO2–B2O3 glass //Journal of materials science letters. 2001. V. 20. P. 2235–2237.
  38. Yun Mo Sung. Phase formation kinetics in SrO–Al2O3–SiO2–B2O3 glass //Journal of materials science. 2002. V. 37. P. 699–703.
  39. Yun Mo Sung, Sungtae Kim. Sintering and crystallization of off-stoichiometric SrO–Al2O3–2SiO2 glasses //Journal of materials science. 2000. V. 35. P. 4293–4299.
  40. Yun Mo Sung. Crystallization of celsian glasses of (SrO–Al2O3–2SiO2)–(Al2O3) pseudobinary compositions //Journal of materials science letters. 2001. V. 20. P. 839–840.
  41. Yun Mo Sung. Mechanical properties of off-stoichiometric celsian glass-ceramics //Journal of materials science letters.1999. V. 18. P. 1229–1232.
  42. Uvarova N.E., Orlova L.A., Lebedeva Ju.E., Grashhenkov D.V. Primenenie metoda elektronnogo paramagnitnogo rezonansa dlya izucheniya strukturnyh izmenenij v processe geleobrazovaniya pri poluchenii keramiki i steklokeramiki zol-gel metodom [Application of a method of an electronic paramagnetic resonance for studying of structural changes in process of jellification when receiving ceramics and glass ceramics sol-gel by method] //Aviacionnye materialy i tehnologii. 2011. №3. S. 26–30.
  43. Grashhenkov D.V., Solncev S.St., Shhegoleva N.E., Naumova A.S., Gaponov B.N. Steklokeramicheskij kompozicionnyj material [Glass-ceramic composite material] //Aviacionnye materialy i tehnologii. 2012. №S. S. 368–372.
  44. Shhegoleva N.E., Grashhenkov D.V., Vaganova M.L., Solncev S.S. Perspektivnyj steklokeramicheskij kompozicionnyj material [Perspective glass-ceramic composite material] //Tehnika i tehnologija silikatov. 2014. T. 21. №1. S. 6–11.
  45. Shhegoleva N.E., Vaganova M.L., Grashhenkov D.V. Primenenie rentgenofazovogo analiza dlja izuchenija processa kristallizacii pri poluchenii kalcijaljumosilikatnoj keramiki zol-gel metodom [Application of the X-ray phase analysis for studying of process of crystallization when receiving calcium aluminosilicate ceramics sol-gel by method] //Perspektivnye materialy. 2014. №5. S. 16–21.
  46. Orlova L.A., Chajnikova A.S., Popovich N.V., Lebedeva Ju.E. Kompozity na osnove ayumosilikatnoj steklokeramiki s diskretnymi napolnitelyami [Composites on the basis of aluminosilicate glass ceramics with discrete fillers] //Steklo i keramika. 2013. №4. S. 41–46.
  47. Lebedeva Ju.E., Grashhenkov D.V., Popovich N.V., Orlova L.A., Chajnikova A.S. Razrabotka i issledovanie termostabilnyh pokrytij, poluchennyh zol-gel metodom v sisteme Y2O3–Al2O3–SiO2, dlja SiC-soderzhashhih materialov [Development and research of thermostable coating received by sol-gel method in Y2O3–Al2O3–SiO2 system for SiC-based matireals] //Trudy VIAM. 2013. №12. St. 03 (viam-works.ru).
  48. Solncev St.S., Rozenenkova V.A., Mironova N.A., Soloveva G.A. Vysokotemperaturnye pokrytiya na osnove sol-gel tehnologii [High-temperature coatings on basis of sol-gel technology] //Trudy VIAM. 2014. №1. St. 03 (viam-works.ru).
  49. Lebedeva Ju.E., Popovich N.V., Orlova L.A. Zashhitnye vysokotemperaturnye pokrytiya dlya kompozicionnyh materialov na osnove SiC [Protective high-temperature coverings for composite materials on the basis of SiC] //Trudy VIAM. 2013. №2. St. 06 (viam-works.ru).
  50. Kablov E.N., Grashhenkov D.V., Uvarova N.E. Issledovaniya metodom infrakrasnoj spektroskopii strukturnyh izmenenij gelej v processe termicheskoj obrabotki pri poluchenii vysokotemperaturnyh steklokeramicheskih materialov po zol-gel tehnologii [Researches by method of infrared spectroscopy of structural changes of gels in the course of heat treatment when receiving high-temperature glass-ceramic materials on technology sol-gel] //Aviacionnye materialy i tehnologii. 2011. №2. S. 22–25.
  51. Romashin A.G., Rusin M.Yu., Borodai F.Ya. Structural Ceramic and Fibrous Materials Based on Quartz Glass //Refractories and Industrial Ceramics. 2004. V. 45. №6. P. 387–391.
  52. Xian Xin Li, Ying Sun, Jia Lu Li, Ming Ma. Research Progress of SiO2 Matrix Composites Materials for Radomes //Advanced Materials Research. 2012. V. 430–432. P. 1119–1122.