Ogorodov D.V., Popov D.A., Trapeznikov A.V. Methods of preparing аluminum-zirconium master alloy (review) // Proceedings of VIAM. 2015. No. 11. Ст. 02. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2015-0-11-2-2.

Methods of preparing аluminum-zirconium master alloy (review)

Ogorodov D.V., Popov D.A., Trapeznikov A.V.
Abstract

The article provides an overview of the main methods of obtaining aluminum-zirconium alloys are marked with their advantages and disadvantages. The equipment and brand materials, which are used in the manufacture of zirconium master alloys, shows the influence of the characteristics of the equipment and the selection of raw materials to the process of obtaining ligatures. The conclusions of the most promising methods of obtaining Al–Zr master alloys.

Reference list
  1. Kablov E.N. Osnovnye itogi i napravleniya razvitiya materialov dlya perspektivnoj aviacionnoj tehniki [The main results and the directions of development of materials for the perspective aircraft equipment] /V kn. 75 let. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2007: Jubilejnyj nauch.-tehnich. sb. M.: VIAM. 2007. S. 20–26.
  2. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative development of FSUE «VIAM» SSC of RF on realization of «Strategic directions of development of materials and technologies of their processing for the period until 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  3. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemelnye elementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare-earth elements – materials for modern and future high technologies] //Trudy VIAM. 2013. №2. St. 01 (viam-works.ru).
  4. Kablov E.N. Materialy dlya izdeliya «Buran» – innovacionnye resheniya formirovaniya shestogo tehnologicheskogo uklada [Materials for «Buran» spaceship – innovative solutions of formation of the sixth technological mode] //Aviacionnye materialy i tehnologii. 2013. №S1. S. 3–9.
  5. Kornysheva I.S., Volkova E.F., Goncharenko E.S., Muhina I.Ju. Perspektivy primenenija magnievyh i litejnyh alyuminievyh splavov [Prospects of application of the magnesian and foundry aluminum] //Aviacionnye materialy i tehnologii. 2012. №S. S. 212–222.
  6. Mironov V.M., Byshkvarko G.S., Kitari G.G. Proizvodstvo ligatur dlya alyuminievyh i magnievyh splavov [Production of ligatures for aluminum and magnesian alloys]. Tula: Glavnaja redakcija cvetnoj metallurgii. 1963. 84 s.
  7. Sposob prigotovleniya ligatury alyuminij–tugoplavkij metal [A way of preparation of a ligature aluminum–refractory metal]: pat. 2232827 Ros. Federacija; opubl. 03.02.2003.
  8. Baranov V.N., Lopatina E.S., Drozdova T.N. i dr. Issledovanie vliyaniya parametrov litya na strukturu splava sistemy Al–Zr [Research of influence of parameters of molding on structure of an alloy of Al–Zr system] //Litejnoe proizvodstvo. 2011. №11. S. 16–18.
  9. Ligatura [Ligature]: pat. 2026935 Ros. Federaciya; opubl. 06.04.1995.
  10. Grigorev V.M. Issledovanie cirkonijsoderzhashhih splavov alyuminiya [Research zirconium containing alloys of aluminum] //Cvetnaya metallurgiya. 2011. №3. S. 30–39.
  11. Jacenko S.P., Skachkov V.M., Varchenja P.A. Poluchenie ligatur na osnove alyuminiya metodom vysokotemperaturnyh obmennyh reakcij v rasplavah solej [Receiving ligatures on the basis of aluminum by method of high-temperature exchange reactions in fusions of salts] //Rasplavy. 2010. №2. S. 89–94.
  12. Moskvitin V.I., Popov D.A., Mahov S.V. Termodinamicheskie osnovy alyuminotermicheskogo vosstanovleniya cirkoniya iz ZrO2 v hloridno-ftoridnyh rasplavah [Thermodynamic basics of aluminothermic zirconium reduction from ZrO2 in chloride-fluoride melts] //Tsvetnye Metally. 2012. №4. S. 43–46.
  13. Mahov S.V., Moskvitin V.I., Popov D.A. Osnovy kinetiki i tehnologii alyuminotermicheskogo polucheniya Al–Zr ligatury iz ZrO2 v hloridno-ftoridnyh solevyh rasplavah [Basis of kinetics and technology of aluminothermic obtaining of AI–Zr ligature from ZrO2 in chloride-fluoride salt melts] // Tsvetnye Metally. 2014. №11. S. 20–25.
  14. Altman M.B. Metallurgiya litejnyh alyuminievyh splavov [Metallurgy of foundry aluminum alloys]. M.: Metallurgiya. 1977. 240 s.
  15. Denisov V.M., Pinigin V.V., Antonova L.T. i dr. Alyuminij i ego splavy v zhidkom sostoyanii [Aluminum and its alloys in a liquid state]. Ekaterinburg: UrO RAN. 2005. 266 s.
  16. Jacenko S.P., Ovsjannikov B.V., Ardashev M.A. Cementacionnoe poluchenie «Master-splava» iz ftoridno-hloridnyh rasplavov [Cementation receiving «Master alloy» from fluoride and chloride fusions] //Rasplavy. 2006. №5. S. 29–36.
  17. Agafonov S.N., Krasikov S.A., Ponomarenko A.A. Fazoobrazovanie pri alyumotermicheskom vosstanovlenii ZrO2 [Phase formation at aluminothermic restoration of ZrO2] //Neorganicheskie materialy. 2012. №8. S. 927.
  18. Belov N.A., Alabin A.N. Perspektivnye splavy s dobavkami cirkoniya i skandiya [Perspective alloys with additives of zirconium and scandium] //Tsvetnye metally. 2007. №2. S. 24–26.
  19. Sposob polucheniya cirkonievoj ligatury [Way of receiving a zirconium ligature]: pat. 2201991 Ros. Federaciya; opubl. 10.04 2003.
  20. Ljakishev N.P., Pliner Ju.L., Ignatenko G.F. Alyuminotermiya [Aluminothermy]. M.: Metallurgiya. 1978. 424 s.
  21. Napalkov V.I., Mahov S.V., Popov D.A. Proizvodstvo ligatur dlya alyuminievyh splavov [Production of ligatures for aluminum alloys] //MiTOM. 2011. №10. S. 26–30.