Postnov V.I., Burkhan O.L. Development of a set of alternative methods of express laboratory and process non-destructive control of properties of semi-finished and structures of the PCM on main stages of their production // Proceedings of VIAM. 2015. No. 10. Ст. 11. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2015-0-10-11-11.

Development of a set of alternative methods of express laboratory and process non-destructive control of properties of semi-finished and structures of the PCM on main stages of their production

Postnov V.I., Burkhan O.L.
Abstract

The article is devoted to the actual problem of development and implementation in the aviation enterprises the complex of alternative to existing and complementing them methods and means of nondestructive express-control of properties of polymeric composite materials (PCM) in the manufacture of prepregs, structures and components of the FRP at key stages of their production to improve their reliability and increase lifetime. It is paid much attention to the problem of modern automation technology and laboratory express-control of properties of the PCM. Automation of control process at all stages will allow to manage timely the process parameters as during the semi-finished products manufacture, so at the stage of forming structures of the PCM. Control procedures of the dynamic properties of PCM at key stages throughout the production chain of manufacturing structures of the PCM are summarized. The basic principles for the development of controls are given. The theoretical foundations o

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitija materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative development of VIAM Federal State Unitary Enterprise of GNTs Russian Federation on implementation «The strategic directions of development of materials and technologies of their processing for the period till 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Kablov E.N. Materialy dlja izdelija «Buran» – innovacionnye reshenija formirovanija shestogo tehnologicheskogo uklada [Materials for the product «Buran» – innovative solutions of forming of the sixth technological way] //Aviacionnye materialy i tehnologii. 2013. №S1. S. 3–9.
  3. Kablov E.N., Kondrashov S.V., Jurkov G.Ju. Perspektivy ispol'zovanija uglerodsoderzhashhih nanochastic v svjazujushhih dlja polimernyh kompozicionnyh materialov [Perspectives of use of carbon-containing nanoparticles in binding for polymeric composite materials] //Rossijskie nanotehnologii. 2013. T. 8. №3–4. S. 24–42.
  4. Rumjancev S.V., Kulish E.E., Borisov O.I. Istochniki nizkojenergeticheskogo izluchenija v nerazrushajushhem kontrole [Sources of low-energy emission in non-destructive testing]. M.: Atomizdat. 1976. 128 s.
  5. Nikitin K.E., Postnov V.I., Kachura S.M., Rahmatullin A.Je., Burhan O.L. Komp'juternaja ustanovka ISS 1003M dlja nepreryvnogo monitoringa soderzhanija svjazujushhego v prepregah v processe propitki [The ISS 1003М computer installation for continuous monitoring of the contents binding in prepregs in the course of impregnation] //Aviacionnye materialy i tehnologii 2009. №4. S. 21–23.
  6. Postnov V.I., Burhan O.L., Petuhov V.I. Avtomatizirovannyj metod izmerenija i upravlenija tehnologicheskimi parametrami formovanija izdelij iz PKM [The automated method of measurement and management of technological parameters of formation of products from PKM] /V sb. statej «Innovacii v mashinostroenii». Penza. 2007. S. 202–204.
  7. Postnov V.I., Nikitin K.E., Burhan O.L., Petuhov V.I., Orzaev V.G. Issledovanie ul'trazvukovym metodom strukturnyh izmenenij v PKM v processe formovanija polimernyh kompozicionnyh materialov [Research by ultrasonic method of structural changes in PKM in the course of formation of polymeric composite materials] //Aviacionnye materialy i tehnologii. 2009. №3. S. 25–29.
  8. Nikitin K.E., Burhan O.L., Postnov V.I., Petuhov V.I. Laboratornaja ustanovka dlja issledovanija i otrabotki rezhimov formovanija IPF2003 polimernyh kompozicionnyh materialov ul'trazvukovym metodom [Laboratory installation for research and working off of modes of formation ИПФ2003 of polymeric composite materials by ultrasonic method] //Zavodskaja laboratorija. 2008. №4. S. 38–40.
  9. Postnov V.I., Burhan O.L., Rahmatullin A.Je., Kachura S.M., Nikitin E.K. Metodika nerazrushajushhego kontrolja temperatury steklovanija v izdelijah iz PKM [Technique of non-destructive testing of glass transition temperature in products from PKM] /V sb. trudov III Mezhdunarodnoj nauch.-praktich. konf. «Sistemy upravlenija zhiznennym ciklom izdelij aviacionnoj tehniki». Ul'janovsk. 2012. S. 181.