Vinogradov S.S., Terkulova Y.A., Kurdyukova E.A., Nikiforov A.A. Wear-proof, antifriction and fretting-resistant coating based on Ni–B // Proceedings of VIAM. 2015. No. 1. Ст. 02. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2015-0-1-2-2.

Wear-proof, antifriction and fretting-resistant coating based on Ni–B

Vinogradov S.S., Terkulova Y.A., Kurdyukova E.A., Nikiforov A.A.
Abstract

The developed Ni–B coating impregnated with VAP-5 suspension ensures a low fric-tion factor, high wear- and fretting resistance for friction parts from steels. The coating is workable in air within -80÷+250°C temperature range under specific loadings up to 50 MPa.

Reference list
  1. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and processing technologies for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Chichinadze A.V., Braun Je.D., Bushe N.A. i dr. Osnovy tribologii (trenie, iznos, smazka) [Fundamentals of Tribology (friction, wear, lubrication)]. 2-e izd., pererabot. i dop. M.: Mashinostroenie. 2001. 664 s.
  3. Tribotehnika (iznos i bezyznosnost') [Tribotechnics (wear and bezyznosnogo)]: Uchebnik /Pod red. D.N. Garkunova. 4-e izd., pererabot. i dop. M.: Izd-vo MSHA. 2001. 616 s.
  4. Tribologija. Issledovanija i prilozhenija: opyt SShA i stran SNG [Tribology. Research and applications: the US experience and CIS] /Pod red. A.V. Belogo, K. Ludemy, N.K. Myshkina. M.: Mashinostroenie; N'ju-Jork: Allerton Press. 1993. 454 s.
  5. Kablov E.N. Materialy dlja izdelija «Buran» – innovacionnye reshenija formirovanija shestogo tehnologicheskogo uklada [Materials for the product «Buran» – innovative solutions forming the sixth technological order] //Aviacionnye materialy i tehnologii. 2013. №S1. S. 3–9.
  6. Erasov V.S., Kotova E.A. Jerozionnaja stojkost' aviacionnyh materialov k vozdejstviju tverdyh (pylevyh) chastic [Erosion resistance to the effects of aircraft materials solid (dust) particles] //Aviacionnye materialy i tehnologii. 2011. №3. S. 30–36.
  7. Gura G.S. Kachenie tel s treniem. Fretting [Rolling bodies with friction. Fretting]. Sochi: OOO «Poligraficheskij centr „Dorija”». 2009. 295 s.
  8. Uoterhauz R.B. Fretting-korrozija [Fretting corrosion]. L.: Mashinostroenie. 1976. 272 s.
  9. Elagina O.Ju. Tehnologicheskie metody povyshenija iznosostojkosti detalej mashin [Technological methods to improve the wear resistance of machine parts]: Ucheb. posobie. M.: Logos. 2009. 488 s.
  10. Garkunov D.N. Povyshenie iznosostojkosti detalej samoletov [Wear resistance aircraft parts]. M.: Oborongiz. 1960. 142 s.
  11. Tonysheva O.A., Voznesenskaja N.M., Shal'kevich A.B., Petrakov A.F. Issledovanie vlijanija vysokotemperaturnoj termomehanicheskoj obrabotki na strukturu, tehnologicheskie, mehanicheskie i korrozionnye svojstva vysokoprochnoj korrozionnostojkoj stali perehodnogo klassa s povyshennym soderzhaniem azota [Investigation of the effect of high-temperature thermomechanical treatment on the structure, process, mechanical and corrosion properties of high-strength stainless steel transition class with a high content of nitrogen] //Aviacionnye materialy i tehnologii. 2012. №3. S. 31–36.
  12. Tonysheva O.A., Voznesenskaja N.M., Eliseev Je.A., Shal'kevich A.B. Novaja vysokoprochnaja jekonomnolegirovannaja azotsoderzhashhaja stal' povyshennoj nadezhnosti [New high sparingly nitrogen-containing steel of high reliability] //Aviacionnye materialy i tehnologii. 2012. №S. S. 84–88.
  13. Gromov V.I., Kurpjakova N.A., Sedov O.V., Korobova E.N. Vakuumnaja i ionno-plazmennaja himiko-termicheskaja obrabotka otvetstvennyh detalej gazoturbinnyh dvigatelej [Vacuum and ion-plasma chemical-thermal processing of critical parts of gas turbine engines] //Aviacionnye materialy i tehnologii. 2012. №S. S. 147–156.
  14. Ovsepjan S.V., Lukina E.A., Filonova E.V., Mazalov I.S. Formirovanie uprochnjajushhej fazy v processe vysokotemperaturnogo azotirovanija svarivaemogo zharoprochnogo deformiruemogo splava na osnove sistemy Ni‒Co‒Cr [Formation of the reinforcing phase in the high-temperature nitriding process weldable superalloy based wrought alloy of Ni–Co–Cr] //Aviacionnye materialy i tehnologii. 2013. №1. S. 3–8.
  15. Rjabov D.K., Kolobnev N.I., Samohvalov S.V., Mahsidov V.V. Vlijanie predvaritel'nogo estestvennogo starenija na svojstva splava 1913 v iskusstvenno sostarennom sostojanii [Effect of prior natural aging on the properties of the alloy 1913 in the artificially aged condition] //Aviacionnye materialy i tehnologii. 2013. №2. S. 8–11.
  16. Azarovskij E.N., Mubojadzhjan S.A. Modificirovanie poverhnosti detalej iz konstrukcionnyh stalej v vakuumno-dugovoj plazme titana [Surface modification of parts made of structural steel in the vacuum arc plasma titanium] //Aviacionnye materialy i tehnologii. 2013. №3. S. 20–25.
  17. Rjabov D.K., Kolobnev N.I. Izmenenie mehanicheskih svojstv splava 1913 pri dvuhstupenchatom iskusstvennom starenii [Changes in mechanical properties of the alloy 1913 in the two-stage artificial aging] //Aviacionnye materialy i tehnologii. 2013. №4. S. 3–7.
  18. Solncev St.S. Jerozionnostojkie vlagozashhitnye termoregulirujushhie pokrytija mnogo-razovoj teplozashhity orbital'nogo korablja «Buran» [Erosion-resistant waterproof thermal control coating reusable thermal protection orbiter «Buran»] //Aviacionnye materialy i tehnologii. 2013. №S1. S. 94–124.
  19. Ivanov E.V. Sozdanie iznosostojkih i antifrikcionnyh materialov i pokrytij dlja kosmicheskogo korablja «Buran» [Creating a wear-resistant and anti-friction materials and coatings for spacecraft «Buran»] //Aviacionnye materialy i tehnologii. 2013. №S1.
  20. S. 142–151.
  21. Azarovskij E.N., Mubojadzhjan S.A. Modificirovanie poverhnosti detalej iz konstrukcionnyh stalej v vakuumno-dugovoj plazme titana. Chast' II [Surface modification of parts made of structural steel in the vacuum arc plasma titanium. Part II] //Aviacionnye materialy i tehnologii. 2014. №1. S. 3–11.
  22. Razuvaev E.I., Kapitanenko D.V. Vlijanie termomehanicheskoj obrabotki na strukturu i svojstva austenitnyh stalej [Effect of thermomechanical treatment on the structure and properties of austenitic steels] //Trudy VIAM. 2013. №5. St. 01 (viam-works.ru).
  23. Rozenenkova V.A., Solncev St.S., Mironova N.A. Tonkoplenochnye pokrytija dlja uplotnitel'nyh istiraemyh materialov na osnove diskretnyh volokon dlja protochnogo trakta GTD [Thin film coatings for sealing abrasive materials on the basis of discrete fibers to the flow path GTE] //Trudy VIAM. 2013. №5. St. 04 (viam-works.ru).
  24. Markova E.S., Jakusheva N.A., Pokrovskaja N.G., Shal'kevich A.B. Tehnologicheskie oso-bennosti proizvodstva martensitostarejushhej stali VKS-180 [Technological features of steel production martensitostareyuschey VKS-180] //Trudy VIAM. 2013. №7. St. 01 (viam-works.ru).
  25. Kablov E.N., Lomberg B.S., Ospennikova O.G. Sozdanie sovremennyh zharoprochnyh materialov i tehnologij ih proizvodstva dlja aviacionnogo dvigatelestroenija [The creation of modern high-temperature materials and production technologies for aviation engine] //Kryl'ja Rodiny. 2012. №3–4. S. 34–38.
  26. Bakradze M.M., Ovsepjan S.V., Shugaev S.A., Letnikov M.N. Vlijanie rezhimov zakalki na strukturu i svojstva shtampovok diskov iz zharoprochnogo nikelevogo splava JeK151-ID [Effect of tempering on the structure and properties of the disk forgings of heat-resistant nickel alloy EK151-ID] //Trudy VIAM. 2013. №9. St. 01 (viam-works.ru).
  27. Baldaev L.H. Renovacija i uprochnenie detalej mashin metodami gazotermicheskogo napylenija [Renovation and strengthening of machine parts methods of thermal spraying]. M.: Izd-vo KHT. 2004. 134 s.
  28. Petrov G.L., Burov N.G. Tehnologija i oborudovanie gazoplamennoj obrabotki metallov [Technology and equipment flame treatment of metals]. M.: Mashinostroenie. 1969. 288 s.
  29. Mazalov I.S., Filonova E.V., Lomberg B.S. Formirovanie struktury pri deformacii i termicheskoj obrabotke zagotovok detalej iz nikelevogo vysokoprochnogo svarivaemogo splava VZh172 [Structure formation during the deformation and heat treatment blanks welded high-strength nickel alloy VZH172] //Trudy VIAM. 2013. №12. St. 01 (viam-works.ru).
  30. Kablov E.N., Mubojadzhjan S.A. Ionnoe travlenie i modificirovanie poverhnosti otvetstvennyh detalej mashin v vakuumno-dugovoj plazme [Ion etching and surface modification of critical parts in machines vacuum arc plasma] //Vestnik MGTU im. N.Je. Baumana. Ser. «Mashinostroenie». 2011. №SP2. S. 149–163.
  31. Kablov E.N., Starcev O.V., Krotov A.S., Kirillov V.N. Klimaticheskoe starenie kompozicionnyh materialov aviacionnogo naznachenija. III. Znachimye faktory starenija [Climatic aging of composite materials aviation applications. III. Significant factors of aging] //Deformacija i razrushenie materialov. 2011. №1. S. 34–40.
  32. Bogorad L.Ja. Hromirovanie [Chromium-plating]. L.: Mashinostroenie. 1984. 97 s.
  33. Solodkova L.N., Kudrjavcev V.N. Jelektroliticheskoe hromirovanie [Electrolytic chrome]. M.: Globus. 2007. 191 s.
  34. Beljaev P.P., Zil'berfarb M.I., Garetovskaja M.P. Metallicheskie pokrytija v himicheskom mashinostroenii [Metal coatings in chemical engineering]. Sb. II. M.: Mashgiz. 1951. 144 s.
  35. Borisov V.S., Kasparova E.V. Himicheskoe nikelirovanie [Chemical nickel plating]. Sb. 2. M.: MDNTP im. F.Je. Dzerzhinskogo. 1958.
  36. Vishenkov S.A., Kasparova E.V. Povyshenie iznosostojkosti i zashhita ot korrozii deta-lej iz chernyh i cvetnyh metallov himicheskim nikelirovaniem [Wear resistance and corrosion protection of ferrous and non-ferrous metal chemical nickel plating] //Bjulleten' obmena proizvodstvenno-tehnicheskim opytom. 1958. №6. 208 s.
  37. Gorbunova K.M., Nikiforova A.A. Fiziko-himicheskie osnovy processa himicheskogo nikelirovanija [Physico-chemical foundations of electroless nickel plating]. M.: AN SSSR. 1960. 448 s.
  38. Rjabchenkov A.V., Velemicina V.I. Himicheskoe nikelirovanie kak sredstvo zashhity per-litnyh stalej ot vysokotemperaturnoj gazovoj korrozii. Vnutrennie naprjazhenija ni-kel'-fosfornyh pokrytij i ih vlijanie na ustalostnuju prochnost' stali [Chemical nickel plating as a means of protection pearlite steels from high-temperature gas corrosion. Internal voltage nickel-phosphorus coatings and their influence on the fatigue strength of steel] /Trudy CNIITMASh. 1961. №22. 37 s.
  39. Vishenkov S.A., Kasparova E.V. Povyshenie nadezhnosti i dolgovechnosti detalej mashin himicheskim nikelirovaniem [Improving the reliability and durability of machine parts electroless nickel plating]. M.: Mashgiz. 1963. 208 s.
  40. Vansovskaja K.M. Metallicheskie pokrytija, nanesennye himicheskim sposobom [Metal coatings deposited by chemical means]. L.: Mashinostroenie. 1985. 103 s.