Gayamov A.M., Budinovskiy S.A. Study of an effect of thickness of the barrier coating layer on properties of compositions of high-temperature alloys VZhM1 and ZhS36 with heat-resistant coatings // Proceedings of VIAM. 2014. No. 9. Ст. 03. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2014-0-9-3-3.

Study of an effect of thickness of the barrier coating layer on properties of compositions of high-temperature alloys VZhM1 and ZhS36 with heat-resistant coatings

Gayamov A.M., Budinovskiy S.A.
Abstract

An influence of the thickness of the composite barrier layer [SDP-2+CrC] on heat resistance and kinetics of changes in elemental compositions of VZHM1 and ZHS36 superalloys with heat-resistant coating. Microstructural investigations of «nickel super-alloy–coating» compositions were carried out after the heat resistance test. It has been established that an increase in thickness of the barrier layer reduces significantly diffusion rate of elements across the «nickel superalloy–coating» interface, but the use of barrier layers with the thickness of 20 microns or more leads to a premature detachment of the coating from the substrate. The obtained results allow us to recommend the use of [SDP-2+CrC] barrier layer of 10–15 microns in thickness as a part of the heat-resistant coating.

Reference list
  1. Budinovskij S.A., Mubojadzhjan S.A., Gajamov A.M., Kos'min A.A. Zharostojkie ionno-plazmennye pokrytija dlja lopatok turbin iz nikelevyh splavov, legirovannyh reniem [Heat-resistant ion-plasma coatings for turbine blades of nickel alloys, alloyed with rhenium] //MiTOM. 2008. №6. C. 31–36.
  2. Walston W.S., Schaefer J.C., Murphy W.H. A new type of microstructural instability in superalloys – SRZ /In: Superalloys–1996. The Mineral, Metals & Materials Society. 1996. P. 9–18.
  3. Locci I., MacKay R., Garg A., Ritzert F. Successful surface treatments for reducing instabilities in advanced nickel-base superalloys for turbine blades /In: Technical Memorandum NASA/TM-2004-206622.
  4. Suzuki A., Rae C.M.F., Hobbs R.A., Murakami H. Secondary reaction zone formations in Pt-Aluminised fourth generation Ni-base single crystal superalloys //Advanced Materials Research. 2011. V. 278. P. 78–83.
  5. Budinovskij S.A., Mubojadzhjan S.A., Gajamov A.M., Stepanova S.V. Ionno-plazmennye zharostojkie pokrytija s kompozicionnym bar'ernym sloem dlja zashhity ot okislenija splava ZhS36-VI [Ion-plasma heat-resistant coating with composite barrier layer for protection against oxidation of the alloy ZhS36-VI] //MiTOM. 2011. №1. S. 34–40.
  6. Sposob obrabotki poverhnosti metallicheskogo izdelija [A method of surface treatment of metal products]: pat. 2368701 Ros. Federacija; opubl. 27.09.2009. Bjul. 2009. №27.
  7. Kablov E.N., Petrushin N.V., Vasilenok L.B., Morozova G.I. Renij v zharoprochnyh nikelevyh splavah dlja lopatok gazovyh turbin (Prodolzhenie) [Measurements in high-temperature nickel alloys for gas turbine blades] //Materialovedenie. 2000. №3. S. 38–43.
  8. Kablov E.N. Fiziko-mehanicheskie i tehnologicheskie osobennosti sozdanija zharoprochnyh splavov, soderzhashhih renij [Physical, mechanical and technological features of a high-temperature alloys containing rhenium] //Vestnik Moskovskogo universiteta. Serija 2. «Himija». 2005. T. 46. №3. S. 155–167.
  9. Kablov E.N., Mubojadzhjan S.A. Zharostojkie i teplozashhitnye pokrytija dlja lopatok turbiny vysokogo davlenija perspektivnyh GTD [Heat-resistant and heat-resistant coatings for turbine blades of high pressure promising GTD] //Aviacionnye materialy i tehnologii. 2012. №S. S. 60–70.
  10. Matveev P.V., Budinovskij S.A., Mubojadzhjan S.A., Kos'min A.A. Zashhitnye zharostojkie pokrytija dlja splavov na osnove intermetallidov nikelja [Heat-resistant protective coatings for alloys based on nickel intermetallic] //Aviacionnye materialy i tehnologii. 2013. №2. S. 12–15.
  11. Mubojadzhjan S.A., Budinovskij S.A., Gajamov A.M., Matveev P.V. Vysokotemperaturnye zharostojkie pokrytija i zharostojkie sloi dlja teplozashhitnyh pokrytij [High-temperature heat-resistant coating and heat-resistant layers for thermal barrier coatings] //Aviacionnye materialy i tehnologii. 2013. №1. S. 17–20.
  12. Kablov E.N., Mubojadzhjan S.A. Ionnoe travlenie i modificirovanie poverhnosti otvetstvennyh detalej mashin v vakuumno-dugovoj plazme [Ion etching and surface modification of critical parts of machines in the vacuum arc plasma] //Vestnik MGTU im. N.Je. Baumana. Ser. «Mashinostroenie». 2011. №SP2. S. 149–163.
  13. Kablov E.N., Mubojadzhjan S.A. Teplozashhitnye pokrytija dlja lopatok turbin vysokogo davlenija perspektivnyh GTD [Thermal barrier coatings for turbine blades of the high pressure turbine engine perspective] //Metally. 2012. №1. S. 5–13.
  14. Kablov E.N., Mubojadzhjan S.A., Budinovskij S.A., Lucenko A.N. Ionno-plazmennye zashhitnye pokrytija dlja lopatok gazoturbinnyh dvigatelej [Ion-plasma protective coatings for gas turbine engine blades] //Metally. 2007. № 5. S. 23–34.
  15. Mubojadzhjan S.A., Budinovskij S.A., Gajamov A.M., Smirnov A.A. Poluchenie keramicheskih teplozashhitnyh pokrytij dlja rabochih lopatok turbin aviacionnyh GTD magnetronnym metodom [Preparation of ceramic thermal barrier coatings for turbine blades working GTD magnetron sputtering] //Aviacionnye materialy i tehnologii. 2012. №4. S. 3–8.
  16. Chubarov D.A., Matveev P.V. Novye keramicheskie materialy dlja teplozashhitnyh pokrytij rabochih lopatok GTD [New ceramic materials for thermal barrier coatings operating gas turbine engine blades] //Aviacionnye materialy i tehnologii. 2013. №4.
  17. S. 43–46.
  18. Azarovskij E.N., Mubojadzhjan S.A. Modificirovanie poverhnosti detalej iz konstrukcionnyh stalej v vakuumno-dugovoj plazme titana. Chast' II [Surface modification of parts made of structural steel in the vacuum arc plasma titanium] //Aviacionnye materialy i tehnologii. 2014. №1. S. 3–11.
  19. Gajamov A.M., Budinovskij S.A., Mubojadzhjan S.A., Kos'min A.A. Vybor zharostojkogo pokrytija dlja zharoprochnogo nikelevogo renij-rutenijsoderzhashhego splava marki VZhM4 [The choice of a heat-resistant coatings for heat-resistant nickel-rhenium alloy grade ruthenium VZhM4] //Trudy VIAM. 2014. №1. St. 01 (viam-works.ru).
  20. Galojan A.G., Mubojadzhjan S.A., Egorova L.P., Bulavinceva E.E. Korrozionnostojkoe pokrytie dlja zashhity detalej GTD iz vysokoprochnyh konstrukcionnyh martensitostarejushhih stalej na rabochie temperatury do 450°C [Corrosion-resistant coating for protection GTD parts of high-strength structural steels martensitostareyuschih at operating temperatures up to 450°C] //Trudy VIAM. 2014. №6. St. 03 (viam-works.ru).