Belyaev M.S., Khvatskiy K.K., Gorbovets M.A. Comparative analysis of national standards of RF and the USA on methods of metals fatigue testing // Proceedings of VIAM. 2014. No. 9. Ст. 11. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2014-0-9-11-11.

Comparative analysis of national standards of RF and the USA on methods of metals fatigue testing

Belyaev M.S., Khvatskiy K.K., Gorbovets M.A.
Abstract

A comparative analysis of national standards of RF and the USA on test methods of low-cycle fatigue (LCF) and high-cycle fatigue (HCF) was carried out in this work. The following national standards were considered: RF standard GOST 25.502–79, last revi-sion in 1985, «Strength analysis and testing in machine building. Methods of mechanical testing of metals. Methods of fatigue testing» and two national standards of the USA – ASTM E466–07 «Standard Practice for Conducting Force Controlled Constant Am-plitude Axial Fatigue Tests of Metallic Materials» and ASTM E606–04 «Standard Prac-tice for Strain-Controlled Fatigue Testing». It was shown that there is no noticeable difference between gage sizes of specimens in the standards mentioned above. As compared with GOST, ASTM E standards specify additional high requirements to specimen surfaces and to loading errors. Thus, National standard of RF GOST 25.502–79, last revision in 1985, has to be essentially modified.

Reference list
  1. Raschetnye znachenija harakteristik aviacionnyh metallicheskih konstrukcionnyh materialov [The calculated values of the characteristics of aircraft metallic structural materials]: Spravochnik. M.: OAO «OAK». 2011. 304 s.
  2. Lucenko A.N. Ispytatel'nyj centr FGUP «VIAM»: Osnovnye napravlenija issledovanij i ispytanij, perspektivy razvitija [Testing center of FSUE «VIAM»: Trends of research and testing, development prospects] /V sb. materialov konf. «TestMat–2013». M.: VIAM. 2013 (CD-disk).
  3. Terent'ev V.F., Petuhov A.N. Ustalost' vysokoprochnyh metallicheskih materialov [Tired of high-metallic materials]. M.: IMET RAN – CIAM. 2013. 515 s.
  4. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  5. Erasov V.S., Grinevich A.V., Senik V.Ja., Konovalov V.V., Trunin Ju.P., Nesterenko G.I. Raschetnye znachenija harakteristik prochnosti aviacionnyh materialov [The calculated values of the strength characteristics of aircraft materials] //Aviacionnye materialy i tehnologii. 2012. №2. S. 14–16.
  6. Kablov E.N., Lomberg B.S., Ospennikova O.G. Sozdanie sovremennyh zharoprochnyh materialov i tehnologij ih proizvodstva dlja aviacionnogo dvigatelestroenija [The creation of modern high-temperature materials and manufacturing technologies for aircraft engine] //Kryl'ja Rodiny. 2012. №3–4. S. 34.
  7. Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials – the basis of innovative modernization of Russia] //Metally Evrazii. 2012. №3. S. 10–15.
  8. Erasov V.S., Jakovlev N.O., Nuzhnyj G.A. Kvalifikacionnye ispytanija i issledovanija prochnosti aviacionnyh materialov [Qualification testing and research strength of aircraft materials] //Aviacionnye materialy i tehnologii. 2012. №S. S. 440–448.
  9. Krylov V.D. Metody ispytanij i osobennosti razrushenija tonkolistovyh materialov [Test methods and especially the destruction of thin materials] //Aviacionnye materialy i tehnologii. 2013. №4. S. 54–57.
  10. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace Materials] //Vse materialy. Jenciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  11. Beljaev M.S., Gorbovec M.A., Komarova T.I. Sposob ispytanij i raschetnoe opredelenie predela vynoslivosti dlja gorizontal'nogo uchastka krivoj ustalosti [Test Method and settlement definition of the fatigue limit for the horizontal part of the fatigue curve] //Aviacionnye materialy i tehnologii. 2012. №3. S. 50–55.
  12. Schijve J. Fatigue of structures and materials. Berlin-Heidelberg: Springer-Verlag. 2009. 185 с.
  13. Hvackij K.K., Gorbovec M.A. Sovremennye metody issledovanija vysokotemperaturnoj prochnosti metallicheskih materialov [Modern methods of research of high-strength metallic materials] /V sb. materialov konf. «TestMat–2013». M.: VIAM. 2013 (CD-disk).
  14. Erasov V.S., Nuzhnyj G.A. Zhestkij cikl nagruzhenija pri ustalostnyh ispytanijah [Hard loading cycle fatigue tests at] //Aviacionnye materialy i tehnologii. 2011. №4. S. 35–40.
  15. Wright J.K., Carroll L.J., Simpson J.A. et al. Low Cycle Fatigue of Alloy 617 at 850°C and 950°C //J. of Eng. Mat. and Tech. 2013. V. 135. №7. P. 031005-1–031005-8.
  16. Levkovitch V., Sievert R., Svendsen B. Simulation of deformation and lifetime behavior of a FCC single cristal superalloy at high temperature under low-cycle fatigue loading //Int. J. Fatigue. 2006. V. 28 (12). P. 1791–1802.
  17. Stepnov M.N., Naumkin A.S. Chuvstvitel'nost' konstrukcionnyh materialov k koncentracii naprjazhenij v oblasti mnogociklovoj ustalosti [Sensitivity of structural materials to stress concentration in the high-cycle fatigue] //Vestnik mashinostroenija. 2011. №4. S. 22–25.