Sorokin O.Ju., Grachshencov D.V., Solncev S.St., Evdokimov S.A. Ceramic composite materials with high oxidation resistance for the novel aircrafts (review) // Proceedings of VIAM. 2014. No. 6. Ст. 08. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2014-0-6-8-8.

Ceramic composite materials with high oxidation resistance for the novel aircrafts (review)

Sorokin O.Ju., Grachshencov D.V., Solncev S.St., Evdokimov S.A.
Abstract

Future prospect of novel oxidation-resistant materials for aviation purposes was highlighted. The key methods of their processing with ultra-high temperature ceramic matrix (UHTC) were discussed.

Reference list
  1. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Jastin J.F., Jankowiak A. Ultra high temperature ceramics: densification, properties and thermal stability //Aerospace Lab. 2011. №3. P. 1–11.
  3. Matovic B., Yano T. Silicon Carbide and other carbides: from stars to the advanced ceramics /In: Handbook of advanced Ceramics. Chapter 3.1. 2013. P. 225–244.
  4. Dospehi dlja «Burana». Materialy i tehnologii VIAM dlja MKS «Jenergija–Buran» [Armor for the «Buran». Materials and technologies for VIAM ISS «Energia-Buran»] /Pod. red. E.N. Kablova. M.: Fond «Nauka i zhizn'». 2013. 128 s.
  5. Grashhenkov D.V., Chursova L.V. Strategija razvitija kompozicionnyh i funkcional'nyh materialov [Development Strategy composite and functional materials] //Aviacionnye materialy i tehnologii. 2012. №S. S. 231–242.
  6. Opeka M.M., Talmy I.G., Zaykoski J.A. Oxidation-based materials selection for 2000°C+hypersonic aerosurfaces: Theoretical considerations and historical experience //J. Mater. Sci. 2004. V. 39. P. 5887–5904.
  7. Kablov E.N., Grashhenkov D.V., Isaeva N.V., Solncev S.S. Perspektivnye vysokotemperaturnye keramicheskie kompozicionnye materialy [Promising high-temperature ce-ramic composites] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 20–24.
  8. Lebedeva Ju.E., Popovich N.V., Orlova L.A. Zashhitnye vysokotemperaturnye pokrytija dlja kompozicionnyh materialov na osnove SiC [Protective coatings for high-temperature composite materials based on SiC] //Trudy VIAM. 2013. №2. St. 06 (viam-works.ru).
  9. Solncev S.S., Rozenenkova V.A., Mironova N.A., Gavrilov S.V. Keramicheskie pokrytija dlja zashhity vysokoprochnoj stali pri termicheskoj obrabotke [The ceramic coating to protect the high-strength steel during heat treatment] //Aviacionnye materialy i tehnologii. 2011. №4. S. 3–8.
  10. Kablov E.N., Grashhenkov D.V., Isaeva N.V., Solncev S.S., Sevast'janov V.G. Vysokotemperaturnye konstrukcionnye kompozicionnye materialy na osnove stekla i keramiki dlja perspektivnyh izdelij aviacionnoj tehniki [High-temperature structural composite materials based on glass and ceramic products for advanced aircraft] //Steklo i keramika. 2012. №4. S. 7–11.
  11. Simonenko E.P., Simonenko N.P., Sevast'janov V.G., Grashhenkov D.V., Kuznecov N.T., Kablov E.N. Funkcional'no gradientnyj kompozicionnyj material SiC/(ZrO2–HfO2–Y2O3), poluchennyj s primeneniem zol'-gel' metoda [Functionally gradient com-posite material SiC/(ZrO2–HfO2–Y2O3), prepared using a sol-gel method] //Kompozity i nanostruktury. 2011. T. 4. S. 52–64.
  12. Zhu Y., Wang S., Chen H. Effect of copper on microstructure and mechanical properties of Sf/ZrC composites fabricated by low-temperature liquid metal infiltration //Cer. Int. 2014. V. 40. P. 2793–2798.
  13. Bongiorno A., Först C.J., Kalia R.K. A Perspective on Modeling Materials in Extreme Environments: Oxidation of Ultrahigh-Temperature Ceramics //MRS Bulletin. 2006. V. 31. P. 410–418.
  14. Gasch M., Ellerby D., Beckman S. Processing, properties and arc jet oxidation of hafnium diboride/silicon carbide ultrahigh temperature ceramics //J. Mater. Sci. 2004. V. 39. P. 5925–5937.
  15. Eakins E., Jayaseelan D.D., Lee W.E. Toward Oxidation-Resistant ZrB2–SiC Ultra High Temperature Ceramics //Metal. Mater. Trans. A. 2011. V. 42A. P. 878–887.
  16. Ermolenko I.N., Ul'janova T.M., Vitjaz' P.A. Voloknistye vysokotemperaturnye keramicheskie materialy [High temperature ceramic fiber material]. M.: Nauka i tehnika. 1991. 255 s.
  17. Monteverde F., Alfano D., Savino R. Effects of LaB6 addition on arc-jet convectively heated SiC-containing ZrB2-based ultra-high temperature ceramics in high enthalpy supersonic airflows //Corrosion Science. 2013. V. 75. P. 443–453.
  18. Williams P.A., Sakidia R., Perepezko J.H. Oxidation of ZrB2–SiC ultra-high tempera-ture composites over a wide range of SiC content //J. Eur. Cer. Soc. 2012. V. 32. P. 3875–3883.
  19. Magnani G., Antolini F., Beaulardi L. Sintering, high temperature strength and oxidation resistance of liquid-phase-pressureless-sintered SiC–AlN ceramics with addition of rare-earth oxides //J. Eur. Cer. Soc. 2009. V. 29. P. 2411–2417.
  20. Lojanová Š., Dusza J., Šajgalík P. Characterization of rare-earth doped Si3N4/SiC mi-cro/nanocomposites //Proc. and Appl. Of Cer. 2010. V. 4. №1. P. 25–32.
  21. Paul A., Jayaseelan D.D., Venugopal S. UHTC composites for hypersonic applications //Am. Cer. Soc. Bul. 2012. V. 91. №1. P. 22–29.
  22. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemel'nye jelementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare earth elements – materials of current and future high-tech] //Trudy VIAM. 2013. №2. St. 01 (viam-works.ru).
  23. Stackpoole M., Rom G., Whitt J. UHTC composites with nanotube-reinforcement for advanced TPS applications /In: 3-rd Int. Planetary Probe Workshop. Anavyssos, Attiki. 2005.
  24. Gunjaev G.M., Kablov E.N., Aleksashin V.M. Modificirovanie konstrukcionnyh ugleplastikov uglerodnymi nanochasticami [Modification of structural carbon fiber with carbon nanoparticles] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 5–19.