Solncev S.St., Shvagireva V.V., Isaeva N.V., Solovyova G.A. High temperature coating for protection of high-strength complex alloyed of nickel alloys of high-temperature gas corrosion // Proceedings of VIAM. 2014. No. 6. Ст. 04. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2014-0-6-4-4.

High temperature coating for protection of high-strength complex alloyed of nickel alloys of high-temperature gas corrosion

Solncev S.St., Shvagireva V.V., Isaeva N.V., Solovyova G.A.
Abstract

Developed coating EVK-104M to ensure the protection of high-strength difficult dope nickel alloy residence VZH159 intended for parts and components of gas turbine engines operating in the specially heat-stressed conditions of high temperature gas corrosion at temperature 1050°C long-and at a temperature of 1200°C briefly.

Keywords
nickel alloys, oxidation, coating, heat resist
Reference list
  1. Kablov E.N. Strategic directions of development of materials and technologies of their processing for the period till 2030 [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviation materials and technologies. 2012. №S. P. 7–17.
  2. Ospennikova O.G. Strategy of development of high-temperature alloys and steels special purpose, protection and thermal barrier coatings [The development strategy of superal-loys and special steel, protective and thermal barrier coatings] //Aviation materials and technologies. 2012. №S. P. 19–36.
  3. Solncev S.S. High-temperature glass-ceramic materials and coatings – a perspective direction of aviation materials [High-temperature glass-ceramic materials and coatings – a promising direction aviation materials] //All materials. Encyclopedic reference. 2009. №1. P. 26–37.
  4. Kablov E.N., Grashenkov D.V., Isaeva N.V., Solncev S.S. Promising high-temperature ceramic composite materials [Promising high-temperature ceramic composites] //Russian chemical journal. 2010. T. LIV. №1. P. 20–24.
  5. Vaganova M.L., Shegoleva N.E., Grashenkov D.V. Prospects of development of high-temperature ceramic composite materials [Prospects for the development of high-temperature ceramic composites] //All materials. Encyclopedic reference. 2013. №5. P. 8–14.
  6. Solncev S.S., Isaeva N.V., Shvagireva V.V., Maksimov V.I. High-temperature coatings for the protection of alloys and carbon-ceramic composite materials from oxidation [High-temperature protective coatings for alloys and composite materials uglerodkeram-icheskih from oxidation] //Conversion in mechanical engineering. 2004. №3. P. 77–81.
  7. Solncev S.S., Isaeva N.V., Shvagireva V.V., Solovyeva G.A. Heat-resistant enamel coating for corrosion protection of steel and superalloys, from the effects of aggressive environments [Heat-resistant enamel coatings for corrosion protection of steel and heat resisting alloys from corrosion] /In: Aviation materials and technologies. 2008. №8. P. 29–31.
  8. Solncev S.S., Isaeva N.V., Shvagireva V.V., Solovyeva G.A. High-temperature heat-resistant enamel coating for protection against corrosive products of combustion of fuel-loaded elements of corrosion-resistant steels and superalloys [High-temperature heat-resistant enamel coatings for protection against corrosion effects of the combustion products of thermally loaded components of corrosion resistant steels and superalloys] /In: Aviation materials and technologies. 2008. №4. P. 16–18.
  9. Kablov E.N., Muboyadjan S.A. Heat-resistant thermal barrier coatings for turbine blades of high pressure promising gas-turbine engines [Heat-resistant heat-resistant coatings for high-pressure turbine blades looking GTE] //Aviation materials and technologies. 2012. №S. P. 60–70.
  10. Muboyadjan S.A., Budinovskiy S.A., Gayamov A.M., Smirnov A.A. Receipt of ceramic thermal barrier coatings for the rotor blades of gas turbine engines magnetron method [Preparation of ceramic thermal barrier coatings for turbine blades of aircraft GTE mag-netron sputtering] //Aviation materials and technologies. 2012. №4. P. 3–8.
  11. Kablov E.N., Ospennikova O.G., Sidorov V.V., Rigin V.E., Kablov D.E. Features of the technology of melting and pouring of modern foundry high-heat-resistant nickel al-loys [Technology features modern smelting and casting casting nickel-base superalloys] //Vestnik MGTU N.E.Baumana. «Engineering». 2011. №SP2. P. 68–78.
  12. Solncev S.S., Shvagireva V.V., Isaeva N.V., Solovyeva G.A. Reinforced heat-resistant glass-enamel for combustion chambers of gas turbine engines [Reinforced heat resistant vitreous for combustors of gas turbine engines] //Aviation materials and technologies. 2010. №1. P. 26–29.
  13. Solncev. S.S, Rozenenkova V.A., Mironova N.A., Gavrilov S.V. Ceramic coatings for protection of high-strength steel heat treatment [The ceramic coating to protect the high-strength steel during heat treatment] //Aviation materials and technologies. 2011. №4. P. 3–8.
  14. Solncev S.S. Technological protection coverage and refractory enamel [Protective technological coatings and refractory enamel]. M.: Engineering. 1984. 255 p.
  15. Chemical technology of glass and glass ceramics [Chemical technology of glass and ceramics] /Еdited by N.M. Pavlushkina. M.: Stroiizdat. 1983. 432 р.
  16. Appen A.A. Temperature-stable inorganic coatings [Thermally stable inorganic coat-ings]. M.-L.: Chemistry. 1976. 107 р.
  17. Solncev S.S., Rozenenkova V.A., Isaeva N.V. The development and use of aerospace technique of glass-ceramic coatings and materials [Development and application in aerospace engineering glass-ceramic coatings and materials] /In: Aviation materials and technologies. Selected works VIAM. 1932–2007. M.: VIAM. 2007. P. 99–107.
  18. Solncev St.S., Rozenenkova V.A., Mironova N.A., Solovyeva G.A. High-temperature coatings for fibrous substrates [High temperature coatings for fibrous substrates] //Works of VIAM. 2013. №10. St. 03 (viam-works.ru).
  19. Rozenenkova V.A., Solncev St.S., Mironova N.A. Complex protection of beryllium alloys and sublimation toxic fumes of beryllium [Comprehensive protection for beryllium alloys from oxidation and sublimation toxic fumes of beryllium] //Works of VIAM. 2013. №5. St. 03 (viam-works.ru).
  20. Kablov E.N., Solncev S.S., Rozenenkova V.A., Mironova N.A. Modern multifunctional high-temperature coatings for nickel alloys, metal sealing of fibrous materials and be-ryllium alloys [Modern polyfunctional high-nickel alloy coatings, sealing materials and fibrous metal beryllium] //News of materials science. Science and technology. 2013. №1 (materialsnews.ru).
  21. Rozenenkova V.A., Solncev St.S., Mironova N.A. Thin film coatings for o-wear materials on the basis of discrete fibers for duct of gas-turbine engine [Thin film coatings for sealing abrasive materials on the basis of discrete fibers to the flow path GTE] //Works of VIAM. 2013. №5. St. 04 (viam-works.ru).