Postnova M.V., Postnov V.I. Development experience out-of-autoclave methods of formation PCM // Proceedings of VIAM. 2014. No. 4. Ст. 06. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2014-0-4-6-6.

Development experience out-of-autoclave methods of formation PCM

Postnova M.V., Postnov V.I.
Abstract

The basic known technologies out-of-autoclave forming of designs from polymer ma-terials, including their advantages, lacks and scopes are considered. Devices and forms for realizations of the given manufacturing techniques of details from PCM are presented also. Methods UV-solidification are considered at vacuum forming.

Keywords
RFI, RTM
Reference list
  1. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Grashhenkov D.V., Chursova L.V. Strategija razvitija kompozicionnyh i funkcional'nyh materialov [Development Strategy composite and functional materials] //Aviacionnye materialy i tehnologii. 2012. №S. S. 231–242.
  3. Zastrogina O.B., Shvec N.I., Postnov V.I., Serkova E.A. Fenolformal'degidnye svjazujushhie novogo pokolenija dlja materialov inter'era [Phenolformaldehyde binders for a new generation of interior materials] //Aviacionnye materialy i tehnologii. 2012. №S. S. 265–272.
  4. Panina N.N., Kim M.A., Gurevich Ja.M., Grigor'ev M.M., Chursova L.V., Babin A.N. Svjazujushhie dlja bezavtoklavnogo formovanija izdelij iz polimernyh kompozicionnyh materialov [Binders for autoclave-free formation of products from polymeric composite materials] //Klei. Germetiki. Tehnologii. 2013. №10. S. 27–35.
  5. Postnov V.I., Veshkin E.A., Abramov P.A. Puti povyshenija kachestva detalej iz PKM pri vakuumnom formovanii [Ways to improve the quality of parts made in RMB vacuum forming] //Izvestija Samarskogo nauchnogo centra RAN. 2012. T. 14. №4 (3). S. 834–839.
  6. Postnov V.I., Strel'nikov S.V. Vlijanie tehnologii sovmeshhennogo formovanija obshivok i skleivanie ih s sotovym zapolnitelem na tehnologicheskie svojstva paneli [Impact of technology combined molding and gluing their skins with honeycomb panels on the technological properties] //Klei. Germetiki. Tehnologii. 2012. №10. S. 23–29.
  7. Postnov V.I., Strel'nikov S.V., Petuhov V.I., Shvec N.I. Novye reshenija v tehnologii izgotovlenija prepregov dlja panelej inter'era [New solutions in the technology of prepregs for interior panels] //Izvestija Samarskogo nauchnogo centra RAN. 2013. T. 13. №4(2). S. 498–507.
  8. Veselov S.I., Kartashov G.G. Kompozicionnye materialy v aviadvigatelestroenii [Composite materials in aircraft engine]. Kujbyshev: KuAI. 1986. 112 s.
  9. Kshnjakin A.M., Pushkina G.I., Veselov S.I., Kocherzhenko V.A. Informacionnyj listok №459–73. Kujbyshev: CNTI. 1973.
  10. Titov V.V., Kol'cov V.N. Informacionnyj listok №88-001. M.: VIMI. 1988.
  11. Neljub V.A., Grashhenkov D.V., Kogan D.I., Sokolov I.A. Primenenie prjamyh metodov formovanija pri proizvodstve krupnogabaritnyh detalej iz stekloplastikov [Ap-plication of direct methods for molding large parts in the production of fiberglass] //Himicheskaja tehnologija. 2012. №12. S. 735–739.
  12. Chursova L.V., Dushin M.I., Hrul'kov A.V. i dr. Osobennosti tehnologii izgotovlenija detalej iz kompozicionnyh materialov metodom propitki pod davleniem [Features of technology manufacturing parts made of composite materials by pressure impregnation] /V sb. materialov Mezhotraslevoj nauch.-tehnich. konf. «Kompozicionnye materialy v aviakosmicheskom materialovedenii», posvjashhennoj 100-letiju so dnja rozhdenija A.T. Tumanova. 2009. S. 18.
  13. Dzhogan O.M., Kostenko O.P. Metody izgotovlenija detalej iz kompozicionnyh materialov propitkoj v osnastke. Ch. 1. Metody propitki pod davleniem [Methods for the manufacture of parts made of composite materials impregnated in a snap. Part 1. Meth-ods pressure impregnation] /V sb.: «Voprosy proektirovanija i proizvodstva konstrukcij letatel'nyh apparatov». Vyp. 4 (68). Har'kov: HAI. 2011. S. 111–125.
  14. Dzhogan O.M., Kostenko O.P. Metody izgotovlenija detalej iz kompozicionnyh materialov propitkoj v osnastke. Ch. 2. Metody vakuumnoj propitki [Methods for the manufacture of parts made of composite materials impregnated in a snap. Part 2. Vacuum impregnation methods] /V sb.: «Voprosy proektirovanija i proizvodstva konstrukcij letatel'nyh apparatov». Vyp. 1 (69). Har'kov: HAI. 2012. S. 80–92.
  15. Muhametov P.P., Ahmadieva K.R., Kim M.A., Babin A.N. Rasplavnye svjazujushhie dlja perspektivnyh metodov izgotovlenija PKM novogo pokolenija [Melt binders promising methods of manufacturing a new generation of PCM] //Aviacionnye materialy i tehnologii. 2012. №S. S. 260–265.
  16. Hrul'kov A.V., Dushin M.I., Popov Ju.O., Kogan D.I. Issledovanija i razrabotka avtoklavnyh i bezavtoklavnyh tehnologij formovanija PKM [Research and development of the autoclave and non-autoclave molding technologies RMB] //Aviacionnye materialy i tehnologii. 2012. №S. S. 292–301.
  17. Kogan D.I., Chursova L.V., Petrova A.P. Tehnologija izgotovlenija PKM sposobom propitki plenochnym svjazujushhim [Manufacturing technology RMB impregnation method binder film] //Klei. Germetiki. Tehnologii. 2011. №6. S. 25–29.
  18. Kogan D.I., Chursova L.V., Petrova A.P. Polimernye kompozicionnye materialy, poluchennye putem propitki plenochnym svjazujushhim [Polymer composite material obtained by impregnating a film binder] //Kompozicionnye materialy. 2011. №11. S. 2–6.
  19. Postnov V.I., Burhan O.L., Kachura S.M., Rahmatullin A.Je., Samsonov A.V., Jamaev R.R., Shershak P.V. Neprepregovyj avtomatizirovannyj kontrol' massovogo soderzhanija plenochnogo svjazujushhego v prepregah v processe ih izgotovlenija [Non-prepreg automated control of the mass content of the binder film in prepregs during their manufacture] //Izvestija Samarskogo nauchnogo centra RAN. 2012. T. 14. №4 (3). S. 830–833.
  20. Postnov V.I., Senatorova O.B., Zhelezina G.F., Kazakov I.A., Abramov P.A., Gerasimov V.A., Postnova M.V. Opyt primenenija MPKM Alor D16/41 v nosovoj chasti kryla samoleta An-124-100 [Experience of using MPKM Alor D16/41 in the bow wing air-craft An-124-100] //Aviacionnye materialy i tehnologii. 2009. №4. S. 8–17.
  21. Postnov V.I., Ershov V.V., Postnov A.V. Tehnologija processa UF-otverzhdenija panelej iz stekloplastika [Process technology for UV curing fiberglass panels] /V sb. materialov 32 Mezhdunarodnoj konf. «Kompozicionnye materialy v promyshlennosti». Jalta: SLAVPOLIKOM. 2012. S. 416–417.
  22. Dzhogan O.M., Kostenko O.P. Prakticheskaja klassifikacija metodov izgotovlenija detalej iz polimernyh kompozicionnyh materialov propitkoj v osnastke [Practical classification methods of manufacturing parts from polymeric composite materials impregnated in a snap] /V sb.: «Voprosy proektirovanija i proizvodstva konstrukcij letatel'nyh apparatov». Vyp. 1 (73). Har'kov: HAI. 2013. S. 21–32.